# US 2001/0025010 A1 · Hydrocarbon-based fuel reforming catalyst and production method therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0025010 A1
- Document ID: US20010025010A1
- Status: Published application
- Kind: A1
- Application number: 09/780,442
- Filed: 2001-02-12
- Published: 2001-09-27
- Earliest claimed: 2000-03-21
- Assignees: Toyota Jidosha Kabushiki Kaisha
- Inventors: Takeshi Hirabayashi
- Web page: https://patentgrep.com/patent/US20010025010A1

## CPC

- C01B 3/326: characterised by the catalysts
- B01J 23/8892: {Manganese}
- C01B 2203/1076: Copper or zinc-based catalysts
- Y02P 20/52: using catalysts, e.g. selective catalysts
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A hydrocarbon-based fuel reforming catalyst that suffers less capability deterioration and has excellent heat resistance and excellent durability is disclosed. The reforming catalyst includes CuOx/ZnO/ZrO2/MnOx or CuOx/ZnO/ZrO2/Y2O3 formed by adding manganese or yttrium to a reforming catalyst composed of copper, zinc and zirconium. If manganese is added, the ratio of manganese to the sum of manganese and zirconium (n/(Mn+Zr)) is from about 0.1 to about 0.62 and, preferably, about 0.17 to about 0.5, and the ratio of copper to the sum of copper and zinc (Cu/(Cu+Zn)) is from about 0.2 to about 0.6 and, preferably, about 0.3 to about 0.48. The reforming catalyst exhibits less capability deterioration and good durability in the steam reforming reaction of methanol.

## Claims

### Claim 1

A reforming catalyst for use in a steam reforming reaction of a hydrocarbon-based fuel, comprising:
a compound containing copper, zinc and zirconium as main components; and
manganese.

### Claim 2 (depends on 1)

The reforming catalyst according to claim 1, wherein a ratio of a mole number of manganese to a mole number of a sum of manganese and zirconium is within a range of about 0.1 to about 0.62.

### Claim 3 (depends on 1)

The reforming catalyst according to claim 1, wherein a ratio of a mole number of manganese to a mole number of a sum of manganese and zirconium is within a range of about 0.17 to about 0.5.

### Claim 4 (depends on 1)

The reforming catalyst according to claim 1, wherein a ratio of a mole number of copper to a mole number of a sum of copper and zinc is within a range of about 0.2 to about 0.6.

### Claim 5 (depends on 1)

The reforming catalyst according to claim 1, wherein a mole ratio of copper to a mole number of a sum of copper and zinc is within a range of about 0.3 to about 0.48.

### Claim 6 (depends on 1)

A monolithic catalyst comprising a reforming catalyst for a hydrocarbon-based fuel according to claim 1 coated on a surface of a monolithic honeycomb.

### Claim 7 (depends on 2)

A monolithic catalyst comprising a reforming catalyst for a hydrocarbon-based fuel according to claim 2 coated on a surface of a monolithic honeycomb.

### Claim 8 (depends on 4)

A monolithic catalyst comprising a reforming catalyst for a hydrocarbon-based fuel according to claim 4 coated on a surface of a monolithic honeycomb.

### Claim 9

A reforming catalyst for use in a steam reforming reaction of a hydrocarbon-based fuel, comprising:
a compound containing copper, zinc and zirconium as main components; and
yttrium.

### Claim 10 (depends on 9)

A monolithic catalyst comprising a reforming catalyst for a hydrocarbon-based fuel according to claim 9 coated on a surface of a monolithic honeycomb.

### Claim 11

A production method for a reforming catalyst for a hydrocarbon-based fuel, comprising:
forming an oxide of copper, an oxide of zinc, an oxide of zirconium, and an oxide of manganese; and
mixing the oxide of copper, the oxide of zinc, the oxide of zirconium, and the oxide of manganese to obtain a mixed oxide.

### Claim 12 (depends on 11)

The production method according to claim 11, further comprising baking the mixed oxide at a temperature of about 200 to about 700° C.

### Claim 13 (depends on 12)

The production method according to claim 12, wherein the mixed oxide is baked for about 1 to about 3 hours.

### Claim 14 (depends on 12)

The production method according to claim 12, further comprising:
washing and filtering the mixed oxide by maintaining the mixed oxide at a temperature of about 70 to about 90° C. for about 20 to about 60 minutes;
repeating the washing filtering;
then baking the mixed oxide; and
drying the mixed oxide material obtained by the washing and filtering by maintaining the mixed oxide at a temperature of from about 100 to about 150° C.

### Claim 15 (depends on 12)

The production method according to claim 12, further comprising hydrogen-reducing the mixed oxide material after baking at a temperature of about 200 to about 400° C.

### Claim 16

A production method for a reforming catalyst for a hydrocarbon-based fuel, comprising:
forming an oxide of copper, an oxide of zinc, an oxide of zirconium, and an oxide of yttrium; and
mixing the oxide of copper, the oxide of zinc, the oxide of zirconium, and the oxide of yttrium to obtain a mixed oxide.

### Claim 17 (depends on 16)

The production method according to claim 16, further comprising baking the mixed oxide at a temperature of about 200 to about 700° C.

### Claim 18 (depends on 17)

The production method according to claim 17, wherein the mixed oxide material is baked for about 1 to about 3 hours.

### Claim 19 (depends on 17)

The production method according to claim 17, further comprising:
washing and filtering the mixed oxide by maintaining the mixed oxide at a temperature of about 70 to about 90° C. for about 20 to about 60 minutes;
repeating the washing and filtering;
then baking the mixed oxide; and
drying the mixed oxide obtained by the washing and filtering by maintaining the mixed oxide at a temperature of about 100 to about 150° C.

### Claim 20 (depends on 17)

The production method according to claim 17, further comprising hydrogen-reducing the mixed oxide after baking at a temperature of about 200 to about 400° C.