# US 2001/0025009 A1 · Process for producing a catalyst body

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0025009 A1
- Document ID: US20010025009A1
- Status: Published application
- Kind: A1
- Application number: 09/822,038
- Filed: 2001-03-29
- Published: 2001-09-27
- Earliest claimed: 1998-09-29
- Assignees: Siemens Aktiengesellschaft
- Inventors: Stefan Fischer; Ronald Neufert; Gunther Pajonk; Frank Witzel
- Web page: https://patentgrep.com/patent/US20010025009A1

## CPC

- B01D 53/9418: {for removing nitrogen oxides by selective catalytic reduction [SCR] using a reducing agent in a lean exhaust gas}
- B01J 23/22: Vanadium
- B01J 23/30: Tungsten
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01D 2255/20715: Zirconium
- B01D 2255/20723: Vanadium
- B01D 2255/20776: Tungsten
- B01D 2255/2092: Aluminium
- B01D 2255/30: Silica
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

A process for producing a catalyst body includes providing titanium dioxide, tungsten trioxide, vanadium pentoxide, aluminum oxide, and/or silicon oxide for the catalyst body. A kneadable and/or shapable compound is processed to form a shaped body by extrusion or by coating of a support body. The shaped body is dried and is calcined to form an active compound. The calcined shaped body is artificially aged by a final heat treatment at a temperature higher than the calcination temperature to produce a catalyst body having a high resistance to deactivation at high temperatures. The starting materials include from 65 to 95% by weight of titanium dioxide, 2 to 30% by weight of tungsten trioxide, 0 to 2% by weight of vanadium pentoxide, preferably, less than 1.5%, 0.1 to 10% by weight of aluminum oxide, and 0.1 to 10% by weight of silicon dioxide. The final heat treatment is done is at 660 to 700° C., drying is at 20 to 100° C. prior to calcination, and calcination is at 400° C. to less than 700° C.

## Claims

### Claim 1

A process for producing a catalyst body, which comprises:
producing a compound from starting materials including tungsten trioxide, vanadium pentoxide, titanium dioxide, aluminum oxide, and silicon oxide;
processing the compound into a shaped body by one of extrusion and coating of a support body;
forming an active compound from the compound by calcinating the shaped body at a calcination temperature; and
artificially aging the calcined shaped body by a final heat treatment at a temperature, higher than the calcination temperature, of from 620 to 720° C. for a total duration of from 20 to 80 hours.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the compound is kneadable.

### Claim 3 (depends on 1)

The process according to claim 1, wherein the compound is shapable.

### Claim 4 (depends on 1)

The process according to claim 1, which further comprises carrying out the aging step by performing the final heat treatment at a temperature of from 660 to 700° C.

### Claim 5 (depends on 1)

The process according to claim 1, which further comprises drying the shaped body at a temperature of from 20 to 100° C. prior to the calcination.

### Claim 6 (depends on 1)

The process according to claim 1, which further comprises carrying out the forming step by calcinating the shaped body at a temperature of from 400° C. to less than 700° C.

### Claim 7 (depends on 1)

The process according to claim 1, which further comprises carrying out the producing step by providing starting materials including from 65 to 95% by weight of titanium dioxide, 2 to 30% by weight of tungsten trioxide, 0 to 2% by weight of vanadium pentoxide, 0.1 to 10% by weight of aluminum oxide, and 0.1 to 10% by weight of silicon dioxide.

### Claim 8 (depends on 7)

The process according to claim 7, which further comprises carrying out the producing step by providing starting materials including less than 1.5% by weight of vanadium pentoxide.

### Claim 9 (depends on 1)

The process according to claim 1, which further comprises selecting the starting materials to produce the shaped body having from 65 to 95% by weight of titanium dioxide, 2 to 30% by weight of tungsten trioxide, 0 to 2% by weight of vanadium pentoxide, 0.1 to 10% by weight of aluminum oxide, and 0.1 to 10% by weight of silicon dioxide.

### Claim 10 (depends on 9)

The process according to claim 9, which further comprises selecting the starting materials to produce the shaped body having less than 1.5% by weight vanadium pentoxide.