# US 2001/0024880 A1 · Methods and apparatuses for monitoring and controlling mechanical or chemical-mechanical planarization of microelectronic substrate assemblies

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024880 A1
- Document ID: US20010024880A1
- Status: Published application
- Kind: A1
- Application number: 09/862,396
- Filed: 2001-05-21
- Published: 2001-09-27
- Earliest claimed: 1999-08-31
- Assignees: Micron Technology, Inc.
- Inventors: Jim Hofmann; Gundu M. Sabde; Stephen J. Kramer; Scott E. Moore
- Web page: https://patentgrep.com/patent/US20010024880A1

## CPC

- B24B 37/013: Devices or means for detecting lapping completion
- B24B 21/04: for grinding plane surfaces
- B24B 37/042: {operating processes therefor}
- B24B 49/16: taking regard of the load
- H10P 74/238: {comprising acting in response to an ongoing measurement without interruption of processing, e.g. endpoint detection or in-situ thickness measurement}
- H10P 95/062: {involving a dielectric removal step}
- B24B: MACHINES, DEVICES, OR PROCESSES FOR GRINDING OR POLISHING (grinding of gear teeth B23F, of screw-threads B23G1/36; by electro-erosion B23H; abrasive or related blasting B24C; tools for grinding, buffing or sharpening B24D; polishing compositions C09G1/00; abrasives C09K3/14; electrolytic etching or polishing C25F3/00; grinding arrangements for use on assembled railway tracks E01B31/17); DRESSING OR CONDITIONING OF ABRADING SURFACES; FEEDING OF GRINDING, POLISHING, OR LAPPING AGENTS
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

Methods and devices for mechanical and/or chemical-mechanical planarization of semiconductor wafers, field emission displays and other microelectronic substrate assemblies. One method of planarizing a microelectronic substrate assembly in accordance with the invention includes pressing a substrate assembly against a planarizing surface of a polishing pad at a pad/substrate interface defined by a surface area of the substrate assembly contacting the planarizing surface. The method continues by moving the substrate assembly and/or the polishing pad with respect to the other to rub at least one of the substrate assembly and the planarizing surface against the other at a relative velocity. As the substrate assembly and polishing pad rub against each other, a parameter indicative of drag force between the substrate assembly and the polishing pad is measured or sensed at periodic intervals. The drag force parameter, for example, can be lateral displacement or lateral forces between a first component coupled to one of the substrate assembly or the polishing pad and a second component in either a carrier assembly holding the substrate assembly or a table supporting the polishing pad. The drag force parameter can be measured along a lateral axis to produce a waveform having minimum and maximum peaks relative to minimum and maximum peak drag forces between the substrate assembly and the polishing pad along the axis. The maximum peak drag forces or the difference of the minimum and maximum peak drag forces are processed to generate a force-time relationship. The status of a parameter, such as the onset of planarity or the endpoint of the process, is then estimated by analyzing the force-time relationship.

## Claims

### Claim 1

A method for diagnosing mechanical or chemical-mechanical planarization processing of microelectronic-device substrate assemblies, comprising:
sensing peak drag forces between a microelectronic substrate assembly and a polishing pad along a first lateral axis;
processing the sensed peak drag forces to generate a force-time relationship between the peak drag forces and time; and
estimating the status of a parameter of the planarizing process by analyzing changes in the force-time relationship.

### Claim 2 (depends on 1)

The method of claim 1 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an endpoint layer over the substrate, and a cover layer over the endpoint layer that fills the trenches; and
estimating the status of a parameter of the planarizing process comprises assessing an endpoint at the endpoint layer by performing a first regression on a downward slope in the force-time relationship to determine a first line, performing a second regression on a relatively flat slope in the force-time relationship to determine a second line, assessing a reference time at an intersection of the first and second lines, and terminating removal of material from the substrate assembly at an endpoint time equal to the reference time plus a predetermined over-polish time.

### Claim 3 (depends on 1)

The method of claim 1 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an silicon nitride endpoint layer over the substrate, and a silicon dioxide cover layer over the endpoint layer that fills the trenches; and
estimating the status of a parameter of the planarizing process comprises assessing an endpoint at the endpoint layer by performing a first regression on a downward slope in the force-time relationship to determine a first line, performing a second regression on a relatively flat slope in the force-time relationship to determine a second line, assessing an exposure time at an intersection of the first and second lines, and terminating removal of material from the substrate assembly at an endpoint time equal to the exposure time plus a predetermined over-polish time.

### Claim 4 (depends on 1)

The method of claim 1 wherein estimating the status of a parameter of the planarizing process comprises assessing an onset of planarity of the substrate assembly by monitoring a change from a decreasing slope in the force-time relationship to an increasing slope.

### Claim 5 (depends on 1)

The method of claim 1 wherein estimating the status of a parameter of the planarizing process comprises assessing an onset of planarity of the substrate assembly by monitoring a change from an increasing slope in the force-time relationship to a decreasing slope.

### Claim 6 (depends on 1)

The method of claim 1 wherein estimating the status of a parameter of the planarizing process comprises assessing an onset of planarity of the substrate assembly by monitoring a change from a decreasing slope in the force-time relationship to a relatively flat slope.

### Claim 7 (depends on 1)

The method of claim 1 wherein estimating the status of a parameter of the planarizing process comprises assessing an onset of planarity of the substrate assembly by monitoring a change from an increasing slope in the force-time relationship to a relatively flat slope.

### Claim 8 (depends on 1)

The method of claim 1 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the status of a parameter of the planarizing process comprises assessing exposure of the endpoint layer by monitoring a change from a decreasing slope of the force-time relationship to an increasing slope.

### Claim 9 (depends on 1)

The method of claim 1 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the status of a parameter of the planarizing process comprises assessing exposure of the endpoint layer by monitoring a change from an increasing slope of the force-time relationship to a decreasing slope.

### Claim 10 (depends on 1)

The method of claim 1 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the status of a parameter of the planarizing process comprises assessing exposure of the endpoint layer by monitoring a change from a decreasing slope of the force-time relationship to a relatively flat slope.

### Claim 11 (depends on 1)

The method of claim 1 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the status of a parameter of the planarizing process comprises assessing exposure of the endpoint layer by monitoring a change from an increasing slope of the force-time relationship to a relatively flat slope.

### Claim 12 (depends on 1)

The method of claim 1 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the status of a parameter of the planarizing process comprises assessing exposure of the endpoint layer by monitoring a change from a relatively flat slope of the force-time relationship to a decreasing slope.

### Claim 13 (depends on 1)

The method of claim 1 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the status of a parameter of the planarizing process comprises assessing exposure of the endpoint layer by monitoring a change from a relatively flat slope of the force-time relationship to an increasing slope.

### Claim 14

A method of mechanical or chemical-mechanical planarization of microelectronic substrate assemblies, comprising:
measuring lateral displacement or lateral forces between a first component coupled to one of the substrate assembly or the polishing pad and a second component in either a carrier assembly holding the substrate assembly or a table supporting the polishing pad, the lateral displacement or lateral forces between the first and second components being proportionate to lateral drag forces between the substrate assembly and the polishing pad;
processing the measured lateral displacement or lateral forces between the first and second components to generate a force-time relationship between the lateral drag forces and time; and
estimating the status of a parameter of the planarizing process by analyzing changes in the force-time relationship.

### Claim 15 (depends on 14)

The method of claim 14 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an endpoint layer over the substrate, and a cover layer over the endpoint layer that fills the trenches; and
estimating the status of a parameter of the planarizing process comprises assessing an endpoint at the endpoint layer by performing a first regression on a downward slope in the force-time relationship to determine a first line, performing a second regression on a relatively flat slope in the force-time relationship to determine a second line, assessing a reference time at an intersection of the first and second lines, and terminating removal of material from the substrate assembly at an endpoint time equal to the reference time plus a predetermined over-polish time.

### Claim 16 (depends on 14)

The method of claim 14 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an silicon nitride endpoint layer over the substrate, and a silicon dioxide cover layer over the endpoint layer that fills the trenches; and
estimating the status of a parameter of the planarizing process comprises assessing an endpoint at the endpoint layer by performing a first regression on a downward slope in the force-time relationship to determine a first line, performing a second regression on a relatively flat slope in the force-time relationship to determine a second line, assessing an exposure time at an intersection of the first and second lines, and terminating removal of material from the substrate assembly at an endpoint time equal to the exposure time plus a predetermined over-polish time.

### Claim 17 (depends on 1)

The method of claim 1 wherein estimating the status of a parameter of the planarizing process comprises assessing an onset of planarity of the substrate assembly by monitoring a change from a decreasing slope in the force-time relationship to an increasing slope.

### Claim 18 (depends on 1)

The method of claim 1 wherein estimating the status of a parameter of the planarizing process comprises assessing an onset of planarity of the substrate assembly by monitoring a change from an increasing slope in the force-time relationship to a decreasing slope.

### Claim 19 (depends on 1)

The method of claim 1 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the status of a parameter of the planarizing process comprises assessing exposure of the endpoint layer by monitoring a change from a decreasing slope of the force-time relationship to a relatively flat slope.

### Claim 20 (depends on 1)

The method of claim 1 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the status of a parameter of the planarizing process comprises assessing exposure of the endpoint layer by monitoring a change from an increasing slope of the force-time relationship to a relatively flat slope.

### Claim 21

A method of mechanical or chemical-mechanical planarization of microelectronic substrate assemblies, comprising:
removing material from a substrate assembly using a polishing pad by pressing the substrate assembly against the polishing pad at a pad/substrate interface and moving at least one of the substrate assembly and the pad relative to the other in a planarizing plane;
generating a drag force-waveform by sensing drag forces between the substrate assembly and the polishing pad along a single lateral axis generally parallel with the planarizing plane;
creating a force-time relationship by correlating peak amplitudes of the sensed drag forces with time; and
terminating planarization of the substrate assembly at an estimated endpoint time defined by a time relative to a change in the measured peak amplitudes of the waveform.

### Claim 22 (depends on 21)

The method of claim 21 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an endpoint layer over the substrate, and a cover layer over the endpoint layer that fills the trenches; and
terminating planarization comprises determining the estimated endpoint time by performing a first regression on a downward slope in the force-time relationship to determine a first line, performing a second regression on a relatively flat slope in the force-time relationship to determine a second line, assessing a reference time at an intersection of the first and second lines, and adding a predetermined over-polish time to the reference time.

### Claim 23 (depends on 21)

The method of claim 21 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an silicon nitride endpoint layer over the substrate, and a silicon dioxide cover layer over the endpoint layer that fills the trenches; and
terminating planarization comprises determining the estimated endpoint time by performing a first regression on a downward slope in the force-time relationship to determine a first line, performing a second regression on a relatively flat slope in the force-time relationship to determine a second line, assessing an exposure time at an intersection of the first and second lines, and adding a predetermined over-polish time to the exposure time.

### Claim 24 (depends on 21)

The method of claim 21 wherein terminating planarization comprises assessing an onset of planarity of the substrate assembly by monitoring a change from a decreasing slope in the force-time relationship to an increasing slope.

### Claim 25 (depends on 21)

The method of claim 21 wherein terminating planarization comprises assessing an onset of planarity of the substrate assembly by monitoring a change from an increasing slope in the force-time relationship to a decreasing slope.

### Claim 26 (depends on 21)

The method of claim 21 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
terminating planarization comprises assessing exposure of the endpoint layer by monitoring a change from a decreasing slope of the force-time relationship to a relatively flat slope.

### Claim 27 (depends on 21)

The method of claim 21 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
terminating planarization comprises assessing exposure of the endpoint layer by monitoring a change from an increasing slope of the force-time relationship to a relatively flat slope.

### Claim 28

A method of mechanical or chemical-mechanical planarization of microelectronic substrate assemblies, comprising:
removing material from a substrate assembly using a polishing pad by pressing the substrate assembly against the polishing pad and moving at least one of the substrate assembly and the pad relative to the other in a planarizing plane;
measuring lateral displacement or lateral forces between a first component coupled to one of the substrate assembly or the polishing pad and a second component in either a carrier assembly holding the substrate assembly or a table supporting the polishing pad, the lateral displacement or lateral forces between the first and second components being proportionate to lateral drag forces between the substrate assembly and the polishing pad;
processing the measured lateral displacement or lateral forces between the first and second components to generate a force-time relationship between the lateral drag forces and time; and
estimating an endpoint time of the substrate assembly using a change in the force-time relationship.

### Claim 29 (depends on 28)

The method of claim 28 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an endpoint layer over the substrate, and a cover layer over the endpoint layer that fills the trenches; and
estimating the endpoint time of the substrate assembly comprises performing a first regression on a downward slope in the force-time relationship to determine a first line, performing a second regression on a relatively flat slope in the force-time relationship to determine a second line, assessing an exposure time at an intersection of the first and second lines, and adding a predetermined over-polish time to the exposure time.

### Claim 30 (depends on 28)

The method of claim 28 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an silicon nitride endpoint layer over the substrate, and a silicon dioxide cover layer over the endpoint layer that fills the trenches; and
estimating the endpoint time of the substrate assembly comprises performing a first regression on a downward slope in the force-time relationship to determine a first line, performing a second regression on a relatively flat slope in the force-time relationship to determine a second line, assessing an exposure time at an intersection of the first and second lines, and adding a predetermined over-polish time to the exposure time.

### Claim 31 (depends on 28)

The method of claim 28 wherein estimating the endpoint time comprises assessing an onset of planarity of the substrate assembly by monitoring a change from a decreasing slope in the force-time relationship to an increasing slope.

### Claim 32 (depends on 28)

The method of claim 28 wherein estimating the endpoint time comprises assessing an onset of planarity of the substrate assembly by monitoring a change from an increasing slope in the force-time relationship to a decreasing slope.

### Claim 33 (depends on 28)

The method of claim 28 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the endpoint time comprises assessing exposure of the endpoint layer by monitoring a change from a decreasing slope of the force-time relationship to a relatively flat slope.

### Claim 34 (depends on 28)

The method of claim 28 wherein:
the substrate assembly includes a substrate, an endpoint layer over the substrate and a cover layer over the endpoint layer; and
estimating the endpoint time comprises assessing exposure of the endpoint layer by monitoring a change from an increasing slope of the force-time relationship to a relatively flat slope.

### Claim 35

A method of mechanical or chemical-mechanical planarization of microelectronic substrate assemblies, comprising:
removing material from a substrate assembly using a polishing pad by pressing the substrate assembly against the polishing pad and moving at least one of the substrate assembly and the pad relative to the other in a planarizing plane;
generating a drag force waveform by sensing drag forces between the microelectronic substrate assembly and the polishing pad along at least a first lateral axis extending generally parallel to the planarizing plane;
processing the waveform to plot peak amplitudes of the waveform over time, the plot having a first section and a second section;
performing a first regression on the first section to define a first line and a second regression on the second section to define a second line;
determining an intersection time corresponding to an intersection between the first and second lines;
estimating an endpoint time of the substrate assembly by adding a predetermined over-polish time to the intersection time; and
terminating removal of material from the substrate assembly at the estimated endpoint time.

### Claim 36 (depends on 34)

The method of claim 34 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an silicon nitride endpoint layer over the substrate, and a silicon dioxide cover layer over the endpoint layer that fills the trenches; and
determining the intersection time comprises performing the first regression on a downward slope of the first section in the force-time relationship to determine the first line, performing the second regression on a relatively flat slope of the second section in the force-time relationship to determine the second line, and locating the intersection of the first and second lines to identify when the silicon nitride endpoint layer is exposed.

### Claim 37

A method of mechanical or chemical-mechanical planarization of microelectronic substrate assemblies, comprising:
providing a substrate assembly having a substrate, an endpoint layer having lands at a desired endpoint elevation in the substrate assembly, and a cover layer over the endpoint layer;
removing material from the cover layer of the substrate assembly using a polishing pad by pressing the substrate assembly against the polishing pad and moving at least one of the substrate assembly and the pad relative to the other in a planarizing plane;
measuring lateral displacement or lateral forces between a first component coupled to one of the substrate assembly or the polishing pad and a second component in either a carrier assembly holding the substrate assembly or a table supporting the polishing pad, the lateral displacement or lateral forces between the first and second components being proportionate to lateral drag forces between the substrate assembly and the polishing pad;
processing the measured lateral displacement or lateral forces between the first and second components to generate a force-time relationship between the lateral drag forces and time; and
performing a first regression on a downwardly sloping section of the force-time relationship to define a first line and a second regression on a relative flat section of the force-time relationship occurring after the downwardly sloping section to define a second line;
determining an exposure time of the endpoint layer by assessing an intersection between the first and second lines;
estimating an endpoint time of the substrate assembly by adding a predetermined over-polish time to the exposure time; and
terminating removal of material from the substrate assembly at the estimated endpoint time.

### Claim 38 (depends on 37)

The method of claim 37 wherein:
the substrate assembly comprises a shallow-trench-isolation structure including a substrate having trenches, an silicon nitride endpoint layer over the substrate, and a silicon dioxide cover layer over the endpoint layer that fills the trenches; and
determining the intersection time comprises performing the first regression on a downward slope of the first section in the force-time relationship to determine the first line, performing the second regression on a relatively flat slope of the second section in the force-time relationship to determine the second line, and locating the intersection of the first and second lines to identify when the silicon nitride endpoint layer is exposed.