# US 2001/0024875 A1 · Method for patterning semiconductor devices on a silicon substrate using oxynitride film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024875 A1
- Document ID: US20010024875A1
- Status: Published application
- Kind: A1
- Application number: 09/867,377
- Filed: 2001-05-30
- Published: 2001-09-27
- Earliest claimed: 1999-07-16
- Assignees: Vanguard International Semiconductor Corporation
- Inventors: Liang-Gi Yao; Pin-Ting Wang
- Web page: https://patentgrep.com/patent/US20010024875A1

## CPC

- H10P 14/6316: {Formation by nitridation, e.g. nitridation of the substrate}
- G03F 7/091: {characterised by antireflection means or light filtering or absorbing means, e.g. anti-halation, contrast enhancement}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10P 14/6927: {the material being a silicon oxynitride, e.g. SiON or SiON:H}
- H10P 50/73: {using masks for insulating materials}
- G03F 1/26: Phase shift masks [PSM]; PSM blanks; Preparation thereof
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A method for fabricating and patterning semiconductor devices with a resolution down to 0.12 μm on a substrate structure. The method begins by providing a substrate structure comprising various layers of oxide and/or nitride formed over either monocrystalline silicon or polycrystalline silicon. A silicon oxynitride layer is formed on the substrate structure. Key characteristics of the oxynitride layer include: a refractive index of between about 1.85 and 2.35 at a wavelength of 248 nm, an extinction coefficient of between 0.45 and 0.75 at a wavelength of 248 nm, and a thickness of between about 130 Angstroms and 850 Angstroms. A photoresist layer is formed over the silicon oxynitride layer and exposed at a wavelength of between about 245 nm and 250 nm; whereby during exposure at a wavelength of between 245 nm 250 nm, the silicon oxynitride layer provides a phase-cancel effect.

## Claims

### Claim 1

A method of patterning semiconductor devices with a resolution down to 0.12 μm on a substrate structure comprising the steps of:
a. forming an oxide layer over a monocrystalline silicon substrate structure;
b. forming a nitride layer on said oxide layer; said nitride layer having a refractive index of between 2.28 and 2.32 at a wavelength of 248 nm;
c. forming a silicon oxynitride layer on said nitride layer; said silicon oxynitride layer having a refractive index of between about 1.85 and 2.35 at a wavelength of 248 nm, an extinction coefficient of between 0.45 and 0.75 at a wavelength of 248 nm, and a thickness of between about 130 angstroms and 850 angstroms;
d. forming a photoresist layer over said silicon oxynitride layer; and
e. exposing said photoresist at a wavelength of between about 245 nm and 250 nm; whereby during exposure at a wavelength of between 245 nm 250 nm, said silicon oxynitride layer provides a phase-cancel effect.

### Claim 2 (depends on 1)

The method of claim 1 wherein said nitride layer has a thickness of between about 1000 Angstroms and 2500 Angstroms and said oxide layer has a thickness of between about 50 Angstroms and 300 Angstroms.

### Claim 3 (depends on 1)

The method of claim 1 which further includes etching said oxynitride layer, said nitride layer and said oxide layer to form a contact opening.

### Claim 4 (depends on 1)

The method of claim 1 wherein said photoresist layer has a thickness of between about 3000 Angstroms and 8000 Angstroms.

### Claim 5 (depends on 1)

The method of claim 1 wherein said oxide layer is formed using a LPCVD process; said nitride layer is formed using LPCVD; and said silicon oxynitride layer is formed by reacting silane, nitric oxide and helium in a plasma at temperatures between about 200° C. and 550° C., at a pressure of between about 3 torr and 8 torr, and at a power of between about 120 watts and 200 watts.

### Claim 6

A method of patterning semiconductor devices with a resolution down to 0.12 μm on a substrate structure comprising the steps of:
a. forming an oxide layer on a silicon layer overlying a substrate structure; said oxide layer being composed of silicon glass;
b. forming a silicon oxynitride layer on said oxide layer; said silicon oxynitride layer having a refractive index of between about 1.85 and 2.35 at a wavelength of 248 nm, an extinction coefficient of between 0.45 and 0.75 at a wavelength of 248 nm, and a thickness of between about 130 Angstroms and 850 Angstroms;
c. forming a photoresist layer over said silicon oxynitride layer; and
d. exposing said photoresist layer at a wavelength of between about 245 nm and 250 nm; whereby during exposure at a wavelength of between 245 nm and 250 nm, said silicon oxynitride layer provides a phase-cancel effect.

### Claim 7 (depends on 6)

The method of claim 6 wherein said oxide layer is composed of undoped silicon glass, has a thickness of between about 1000 Angstroms and 5000 Angstroms, has a refractive index of between about 1.4 and 1.65, and is formed using an O3— TEOS process.

### Claim 8 (depends on 6)

The method of claim 6 wherein said oxide layer is composed of boron doped silicon glass and has a thickness of between about 1000 Angstroms and 5000 Angstroms, has a refractive index of between about 1.4 and 1.65, and is formed using an O3— TEOS process.

### Claim 9 (depends on 6)

The method of claim 6 wherein said oxide layer is composed of boron and phosphorous doped silicon glass and has a thickness of between about 1000 Angstroms and 5000 Angstroms, has a refractive index of between about 1.4 and 1.65, and is formed using an O3— TEOS process.

### Claim 10 (depends on 6)

The method of claim 6 which further includes etching said oxynitride layer and said oxide layer to form a contact opening and removing said photoresist layer.

### Claim 11 (depends on 6)

The method of claim 6 wherein said photoresist layer has a thickness of between about 3000 Angstroms and 8000 Angstroms.

### Claim 12 (depends on 6)

The method of claim 6 wherein said silicon oxynitride layer is formed by reacting silane, nitric oxide and helium in a plasma at temperatures between about 200° C. and 550° C., at a pressure of between about 3 torr and 8 torr, and at a power of between about 120 watts and 200 watts.

### Claim 13

A method of patterning semiconductor devices with a resolution down to 0.12 μm on a substrate structure comprising the steps of:
a. forming a nitride layer on a silicon layer of a substrate structure; said nitride layer having a refractive index of between 2.28 and 2.32 at a wavelength of 248;
b. forming a silicon oxynitride layer on said nitride layer; said silicon oxynitride layer having a refractive index of between about 1.85 and 2.35 at a wavelength of 248 nm, an extinction coefficient of between 0.45 and 0.75 at a wavelength of 248 nm, and a thickness of between about 130 Angstroms and 850 Angstroms;
c. forming a photoresist layer over said silicon oxynitride layer; and
d. exposing said photoresist at a wavelength of between about 245 nm and 250 nm; whereby during exposure at a wavelength of between 245 nm and 250 nm, said silicon oxynitride layer provides a phase-cancel effect.

### Claim 14 (depends on 13)

The method of claim 13 wherein said nitride layer has a thickness of between about 1000 Angstroms and 2500 Angstroms.

### Claim 15 (depends on 13)

The method of claim 13 which further includes forming a dielectric layer over said silicon oxynitride layer and planarizing said dielectric layer prior to forming said photoresist layer; and etching said dielectric layer, said oxynitride layer and said nitride layer to form a contact opening after exposing said photoresist layer.

### Claim 16 (depends on 13)

The method of claim 13 wherein said photoresist layer has a thickness of between about 3000 Angstroms and 8000 Angstroms.

### Claim 17 (depends on 13)

The method of claim 13 wherein said nitride layer is formed using a LPCVD process and said silicon oxynitride layer is formed by reacting silane, nitric oxide and helium in a plasma at temperatures between about 200° C. and 550° C., at a pressure of between about 3 torr and 8 torr, and at a power of between about 120 watts and 200 watts.