# US 2001/0024870 A1 · Fabrication process of a semiconductor integrated circuit device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024870 A1
- Document ID: US20010024870A1
- Status: Published application
- Kind: A1
- Application number: 09/773,000
- Filed: 2001-01-31
- Published: 2001-09-27
- Earliest claimed: 1997-05-30
- Assignees: Hitachi, Ltd.
- Inventors: Yoshikazu Tanabe; Isamu Asano; Makoto Yoshida; Naoki Yamamoto; Masayoshi Saito; Nobuyoshi Natsuaki
- Web page: https://patentgrep.com/patent/US20010024870A1

## CPC

- H10D 64/01354: {passivation or protection of the electrode, e.g. using re-oxidation}
- H10D 64/01312: {the additional layer comprising a metal or metal silicide formed by deposition, i.e. without a silicidation reaction, e.g. sputter deposition}
- H10D 64/01338: {with a treatment, e.g. annealing, after the formation of the conductor}
- H10D 64/664: {the additional layers comprising a barrier layer between the layer of silicon and an upper metal or metal silicide layer}
- H10D 84/0135: {Manufacturing their gate conductors}
- H10D 84/0147: {Manufacturing their gate sidewall spacers}
- H10D 84/0172: {Manufacturing their gate conductors}
- H10D 84/0181: {Manufacturing their gate insulating layers}
- H10D 84/038: {using silicon technology, e.g. SiGe}
- H10P 14/6308: {of Group IV semiconductors}
- H10B 12/05: {Making the transistor}
- H10B 12/09: {with simultaneous manufacture of the peripheral circuit region and memory cells}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

With a view to preventing the oxidation of a metal film at the time of light oxidation treatment after gate patterning and at the same time to making it possible to control the reproducibility of oxide film formation and homogeneity of oxide film thickness at gate side-wall end portions, in a gate processing step using a poly-metal, a gate electrode is formed by patterning a gate electrode material which has been deposited over a semiconductor wafer 1A having a gate oxide film formed thereon and has a poly-metal structure and then, the principal surface of the semiconductor wafer 1A heated to a predetermined temperature or vicinity thereof is supplied with a hydrogen gas which contains water at a low concentration, the water having been formed from hydrogen and oxygen by a catalytic action, to selectively oxidize the principal surface of the semiconductor wafer 1A, whereby the profile of the side-wall end portions of the gate electrode is improved.

## Claims

### Claim 1

A process for the fabrication of a semiconductor integrated circuit device, comprising the steps of:
(a) forming a silicon film over a silicon-oxide-film-containing gate insulation film which has been formed over a silicon surface of a wafer;
(b) forming a refractory metal film of tungsten or molybdenum over said silicon film through a medium of a barrier layer of a nitride of tungsten;
(c) forming a gate electrode by patterning said silicon film and said refractory metal film; and
(d) after said step (c), thermally oxidizing the silicon film without oxidizing said refractory metal film, under a gas ambient containing (1) hydrogen, and (2) water vapor synthesized from a mixed gas of oxygen and hydrogen gases by a catalyst, and containing substantially no hydrogen radicals, the partial pressure of the water vapor being lower than that of the hydrogen in the gas ambient.

### Claim 2 (depends on 1)

A process according to claim 1, wherein said gas ambient does not contain nitrogen gas.

### Claim 3 (depends on 1)

A process according to claim 1, wherein in the step (d), said wafer is heated to a temperature in a range of 800 to 900° C.

### Claim 4

A process for the fabrication of a semiconductor integrated circuit device, comprising the steps of:
(a) forming a silicon film over a silicon-oxide-film-containing gate insulation film, the gate insulation film having a thickness of not more than 5 nm and being formed over a silicon surface of a major surface of a wafer;
(b) forming a refractory metal film over said silicon film;
(c) forming a gate electrode by patterning said silicon film and said refractory metal film, a gate length of the gate electrode being not more than 0.25 μm; and
(d) after said step (c), thermally oxidizing the silicon film without oxidizing said refractory metal film, under a hydrogen gas ambient containing water vapor synthesized from a mixed gas of oxygen and hydrogen gases by a catalyst, the partial pressure of the water vapor being lower than that of the hydrogen in the hydrogen gas ambient, the upper limit of total oxide film thickness grown by said thermally oxidizing being about one and a half of the thickness of the gate insulation film.

### Claim 5 (depends on 4)

A process according to claim 4, wherein said hydrogen gas ambient does not contain nitrogen.

### Claim 6 (depends on 4)

A process according to claim 4, wherein in step (d), said wafer is heated to a temperature in a range of 800 to 900° C.

### Claim 7

A process for the fabrication of a semiconductor integrated circuit device, comprising the steps of:
(a) forming a first film of silicon over a silicon-oxide-film-containing gate insulation film which has been formed over a silicon surface of a major surface of a wafer;
(b) forming a refractory metal film of tungsten or molybdenum over said first film;
(c) forming a gate electrode by patterning said first film and said refractory metal film; and
(d) after said step (c), thermally oxidizing the first film without oxidizing said refractory metal film, under a hydrogen gas ambient, substantially without nitrogen gas, the hydrogen gas ambient containing water vapor synthesized from a mixed gas of oxygen and hydrogen gases by a catalyst, the partial pressure of the water vapor being lower than that of hydrogen gas in the hydrogen gas ambient.

### Claim 8

A process for the fabrication of a semiconductor integrated circuit device, comprising the steps of:
(a) forming an isolation groove in a silicon surface of a major surface of a wafer;
(b) embedding an insulating material in said groove;
(c) after the step (b), planarizing the major surface of said wafer by chemical mechanical polishing;
(d) forming a silicon film over a gate insulation film containing a silicon oxide film having a thickness not more than 5 nm, said silicon oxide film being a principal portion of the entire thickness of the gate insulation film, the silicon oxide film having been formed over the silicon surface of said wafer by thermally oxidizing the silicon surface;
(e) forming a refractory metal film over said silicon film;
(f) forming a gate electrode by patterning said silicon film and said refractory metal film, the gate length of said gate electrode being not more than 0.25 μm; and
(g) after said step (f), thermally oxidizing the silicon film without oxidizing said refractory metal film, under a hydrogen gas ambient containing water vapor, the partial pressure of the water vapor being lower than that of the hydrogen in the hydrogen gas ambient.

### Claim 9 (depends on 8)

A process according to claim 8, wherein said hydrogen gas ambient does not contain nitrogen gas.

### Claim 10 (depends on 8)

A process according to claim 8, wherein in step (g), said wafer is heated to a temperature in a range of 800 to 900° C.

### Claim 11

A process for the fabrication of a semiconductor integrated circuit device, comprising the steps of:
(a) forming a silicon film over a silicon-oxide-film-containing gate insulation film, the gate insulation film having a thickness not more than 5 nm and formed over a silicon surface of a major surface of a wafer;
(b) forming a refractory metal film of tungsten over said silicon film;
(c) forming a gate electrode by patterning said silicon film and said refractory metal film, the gate length of said gate electrode being not more than 0.25 μm; and
(d) after said step (c), thermally oxidizing the silicon film without oxidizing said refractory metal film, under a gas ambient containing hydrogen and water vapor, and containing substantially no hydrogen radicals, the partial pressure of the water vapor being lower than that of the hydrogen in the gas ambient.

### Claim 12

A process for the fabrication of a semiconductor integrated circuit device, comprising the steps of:
(a) forming a refractory metal film of tungsten of molybdenum over a silicon-oxide-film-containing gate insulation film, the gate insulation film having a thickness not more than 5 nm and having been formed over a silicon surface of a major surface of a wafer;
(b) forming a gate electrode by patterning said refractory metal film, the gate length of said gate electrode being not longer than 0.25 μm; and
(c) after said step (b), thermally oxidizing the silicon surface without oxidizing said refractory metal film, under a hydrogen gas ambient containing water vapor synthesized from a mixed gas of oxygen and hydrogen gases by a catalyst, and containing substantially no hydrogen radicals, the partial pressure of the water vapor being lower than that of the hydrogen in the hydrogen gas ambient.

### Claim 13

A process for the fabrication of a semiconductor integrated circuit device, comprising the steps of:
(a) forming a refractory metal film of tungsten or molybdenum over a silicon-oxide-film-containing gate insulation film, the gate insulation film having a thickness not more than 5 nm and having been formed over a silicon surface of a major surface of a wafer;
(b) forming a gate electrode by patterning said refractory metal film, the gate length of said gate electrode being not longer than 0.25 μm; and
(c) after said step (b), thermally oxidizing the silicon surface without oxidizing said refractory metal film, under a hydrogen gas ambient, substantially without nitrogen gas, the hydrogen gas ambient containing water vapor synthesized from a mixed gas of oxygen and hydrogen gases by a catalyst, and containing substantially no hydrogen radicals, the partial pressure of the water vapor being lower than that of the hydrogen in the hydrogen gas ambient, the thermal oxidation of the silicon surface being performed at a temperature such that, in the hydrogen gas ambient, titanium nitride would be oxidized and a nitride of tungsten would not be oxidized.

### Claim 14 (depends on 13)

A process according to claim 13, wherein in step (c), the wafer is heated to a temperature in a range of 800 to 900° C.

### Claim 15

A process for the fabrication of a semiconductor integrated circuit device, comprising the steps of:
(a) forming an isolation groove in a silicon surface of a major surface of a wafer;
(b) embedding an insulating material in said groove;
(c) after said step (b), planarizing said major surface of said wafer by chemical mechanical polishing;
(d) forming a refractory metal film over a gate insulation film containing a silicon oxide film, having a thickness not more than 5 nm, as a principal portion of the entire thickness of the gate insulation film, said silicon oxide film having been formed over the silicon surface of said wafer by thermally oxidizing the silicon surface;
(e) forming a gate electrode by patterning said refractory metal film, the gate length of said gate electrode being not longer than 0.25 μm; and
(f) after said step (e), thermally oxidizing the silicon surface without oxidizing said refractory metal film, under a hydrogen gas ambient containing water vapor, the partial pressure of the water vapor being lower than that of the hydrogen in the hydrogen gas ambient.

### Claim 16 (depends on 15)

A process according to claim 15, wherein said hydrogen gas ambient does not contain nitrogen gas.

### Claim 17 (depends on 15)

A process according to claim 15, wherein in the step (f), said wafer is heated to a temperature in a range of 800 to 900° C.

### Claim 18

A process for the fabrication of a semiconductor integrated circuit device, the semiconductor integrated circuit device comprising:
(a) a gate insulating film over a silicon-base surface region;
(b) a gate electrode having:
(i) a lower polysilicon film constituting a silicon-base region together with the silicon-base surface region, said silicon-base region including silicon as its principal component; and
(ii) an upper refractory metal film including a refractory metal as its principal component,
wherein the upper refractory metal film constitutes a refractory metal region including a refractory metal as one of its principal components, and the gate insulating film and the gate electrode are elements of an insulated gate field effect transistor over a major surface of a substrate region,
the fabrication process comprising:
(x) after patterning the gate electrode, performing heat treatment, in a heat treatment chamber of a single wafer processing furnace by lamp heating under a mixed gas ambient including hydrogen gas and water vapor synthesized from hydrogen gas and oxygen gas by catalyst, of a wafer including the substrate region so as to oxidize the silicon-base region without oxidizing the refractory metal region.

### Claim 19 (depends on 18)

A process according to claim 18, wherein said water vapor synthesized from hydrogen gas and oxygen gas is transferred into the heat treatment chamber while maintaining its gas state.

### Claim 20 (depends on 19)

A process according to claim 19, wherein said synthesis of water vapor is performed at a temperature lower than that of the heat treatment of the wafer.

### Claim 21 (depends on 20)

A process according to claim 20, wherein a gate length of the insulated gate field effect transistor is not longer than 0.25 μm.

### Claim 22 (depends on 21)

A process according to claim 21, wherein a thickness of the gate insulating film is not thicker than 5 nm.

### Claim 23 (depends on 22)

A process according to claim 22, wherein the composition of hydrogen and oxygen in a gas provided to synthesize the r vapor is hydrogen-rich.

### Claim 24 (depends on 23)

A process according to claim 23, wherein the heat treatment is performed at a temperature not lower than 800 degrees centigrade.

### Claim 25

A process for the fabrication of a semiconductor integrated circuit device, comprising:
(a) forming a first insulating film over a surface region, said surface region including silicon as its principal component, over a major surface of a wafer, wherein said first insulating film is to be a gate insulating film of an insulated gate field effect transistor;
(b) forming a first silicon-containing film over the first insulating film, wherein said first silicon-containing film includes silicon as its principal component;
(c) forming a first refractory metal film over the first silicon containing film, wherein said first refractory metal film includes refractory metal as its principal component;
(d) forming a gate electrode of the insulated gate field effect transistor by patterning the first silicon-containing film and the first refractory metal film;
(e) after step (d), performing heat treatment, in a heat treatment chamber of a single wafer processing furnace by lamp heating under a mixed gas ambient including hydrogen gas and water vapor synthesized from hydrogen gas and oxygen gas by catalyst, of the wafer so as to oxidize the surface region and the first silicon-containing film without oxidizing the first refractory metal film.

### Claim 26 (depends on 25)

A process according to claim 25, wherein said water vapor synthesized from hydrogen gas and oxygen gas is transferred into the heat treatment chamber while maintaining its gas state.

### Claim 27 (depends on 26)

A process according to claim 26, wherein the synthesis of water vapor is performed at a temperature lower than that of the heat treatment of the wafer.

### Claim 28 (depends on 27)

A process according to claim 27, wherein a gate length of the gate electrode of the insulated gate field effect transistor is not longer than 0.25 μm.

### Claim 29 (depends on 28)

A process according to claim 28, wherein a thickness of the gate insulating film is not thicker than 5 nm.

### Claim 30 (depends on 29)

A process according to claim 29, wherein the composition of hydrogen and oxygen in a gas provided to synthesize the water vapor is hydrogen-rich.

### Claim 31 (depends on 30)

A process according to claim 30, wherein the heat treatment of the wafer is performed at a temperature not lower than 800 degrees centigrade.

### Claim 32

A process for the fabrication of a semiconductor integrated circuit device, comprising:
(a) forming a first insulating film over a silicon surface region over a major surface of a wafer, wherein said first insulating film is to be a gate insulating film of an insulated gate field effect transistor;
(b) forming a first silicon-containing film over the first insulating film, wherein said first silicon-containing film includes silicon as its principal component;
(c) forming a first refractory metal film over the first silicon-containing film;
(d) forming a gate electrode of the insulated gate field effect transistor by patterning the first silicon-containing film and the first refractory metal film;
(e) after step (d), performing heat treatment, in a heat treatment chamber of a single wafer processing furnace by lamp heating under a mixed gas ambient including hydrogen gas and water vapor synthesized from hydrogen gas and oxygen gas by catalyst, of the wafer so as to oxidize the surface region and the first silicon-containing film without oxidizing the first refractory metal film.

### Claim 33 (depends on 32)

A process according to claim 32, wherein said water vapor synthesized from hydrogen gas and oxygen gas is transferred into the heat treatment chamber while maintaining its gas state.

### Claim 34 (depends on 33)

A process according to claim 33, wherein the synthesis of water vapor is performed at a temperature lower than that of the heat treatment of the wafer.

### Claim 35 (depends on 34)

A process according to claim 34, wherein a gate length of the gate electrode of the insulated gate field effect transistor is not longer than 0.25 μm.

### Claim 36 (depends on 35)

A process according to claim 35, wherein a thickness of the gate insulating film is not thicker than 5 nm.

### Claim 37 (depends on 36)

A process according to claim 36, wherein the composition of hydrogen and oxygen in a gas provided to synthesize the water vapor is hydrogen-rich.

### Claim 38 (depends on 37)

A process according to claim 37, wherein the heat treatment of the wafer is performed at a temperature not lower than 800 degrees centigrade.