# US 2001/0024867 A1 · Semiconductor device and method of manufacturing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024867 A1
- Document ID: US20010024867A1
- Status: Published application
- Kind: A1
- Application number: 09/874,309
- Filed: 2001-06-06
- Published: 2001-09-27
- Earliest claimed: 1997-06-30
- Assignees: Kabushiki Kaisha Toshiba
- Inventors: Shigehiko Saida; Yoshitaka Tsunashima
- Web page: https://patentgrep.com/patent/US20010024867A1

## CPC

- H10P 14/69433: {the material being a silicon nitride not containing oxygen, e.g. SixNy or SixByNz}
- C23C 16/0218: {in a reactive atmosphere (C23C16/0227 takes precedence)}
- C23C 16/0272: {Deposition of sub-layers, e.g. to promote the adhesion of the main coating}
- C23C 16/345: {Silicon nitride}
- H10P 14/6526: {introduced into an oxide material, e.g. changing SiO to SiON}
- H10P 14/662: {Laminate layers, e.g. stacks of alternating high-k metal oxides (adhesion layers or buffer layers H10P14/6508, H10P14/6548)}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10B 12/033: {the capacitor extending over the transistor}
- H10B 12/038: {the capacitor being in a trench in the substrate}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H10B: ELECTRONIC MEMORY DEVICES

## Abstract

A semiconductor device comprises a semiconductor substrate and a silicon nitride film formed on the semiconductor substrate. The silicon nitride film is substantially free from an Si—H bond and has an Si—H density per unit area of 1×1015 cm−2 or less.

## Claims

### Claim 1

A semiconductor device comprising:
a semiconductor substrate; and
a silicon nitride film formed on the semiconductor substrate, the silicon nitride film being substantially free from an Si—H bond.

### Claim 2 (depends on 1)

The semiconductor device according to claim 1, wherein the density of Si—H contained in a unit area of said silicon nitride film is 1×1015 cm−2 or less.

### Claim 3 (depends on 1)

The semiconductor device according to claim 1, wherein the silicon nitride film has a film thickness within 4 nm to 8 nm.

### Claim 4 (depends on 1)

The semiconductor device according to claim 1, wherein the silicon nitride film has a stacked structure having unit layers of 2 nm or less in thickness stacked one upon another.

### Claim 5 (depends on 1)

The semiconductor device according to claim 1, wherein the silicon nitride film is used in at least one of a capacitor insulating film and a gate insulating film.

### Claim 6 (depends on 1)

The semiconductor device according to claim 1, wherein the silicon nitride film is substantially free from an N—H bond.

### Claim 7

A method of manufacturing a semiconductor device comprising the steps of:
loading a substrate in a low pressure CVD apparatus; and
forming a silicon nitride film substantially free from an Si—H bond by introducing a predetermined silicon source gas into the low pressure CVD apparatus.

### Claim 8 (depends on 7)

The method of manufacturing the semiconductor device according to claim 7, wherein the step of forming the silicon nitride film includes a step of forming a silicon nitride film having a Si—H density per unit area of 1×1015 cm−2 or less.

### Claim 9 (depends on 7)

The method of manufacturing the semiconductor device according to claim 7, wherein a silicon source gas free from an Si—H bond is used as said predetermined silicon source gas.

### Claim 10 (depends on 7)

The method of manufacturing the semiconductor device according to claim 7, wherein the predetermined silicon source gas contains silicon whose bonds are entirely bonded to at least one element selected from the group consisting of silicon, nitrogen, and halogen.

### Claim 11 (depends on 7)

The method of manufacturing semiconductor device according to claim 7, wherein the predetermined silicon source gas is one of tetrachlorosilane, hexachlorodisilane, tetrakisdimethylaminosilane and trichlorosilylazide.

### Claim 12 (depends on 7)

The method of manufacturing a semiconductor device according to claim 7, wherein the step of forming a silicon nitride film further comprises the steps of:
forming the silicon nitride film by using the predetermined silicon source gas having an Si—H bond;
reducing hydrogen contained in the silicon nitride film by a heat treatment; and
forming a silicon nitride film having an Si—H density per unit area of 1×1015 cm−2 or less.

### Claim 13 (depends on 12)

The method of manufacturing semiconductor device according to claim 12, wherein the heat treatment is performed at a temperature within a range of 900° C. to 1100° C.

### Claim 14

A method of manufacturing a semiconductor device comprising:
a step of loading a semiconductor substrate into a chamber;
a first step of introducing a silicon-containing gas into a chamber;
a second step of performing a first annealing of the semiconductor substrate in the silicon-containing gas at a temperature within 600 to 900° C. and a pressure within 0.1 Torr to 10 Torr;
a third step of exhausting the silicon-containing gas after the first annealing;
a fourth step of introducing a nitrogen-containing gas after the third step;
a fifth step of performing a second annealing of the semiconductor substrate in the nitrogen-containing gas at a temperature within 600 to 1000° C. and a pressure within 0.5 Torr to 100 Torr;
a sixth step of exhausting the nitrogen-containing gas after the fifth step; and
a step of repeating the first to sixth steps a plurality of times.

### Claim 15 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the silicon-containing gas includes at least one of tetrachlorosilane, trichlorosilane, and dichlorosilane.

### Claim 16 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the nitrogen-containing gas includes at least one of ammonia, nitrogen trifluoride, hydrazine, dimethylhydrazine and monomethylhydrazine.

### Claim 17 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, further comprising, a step of thermally nitriding the semiconductor substrate before the first step.

### Claim 18 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, further comprising, before the first step, the steps of:
forming a native oxide film on a surface of a semiconductor substrate; and
removing the native oxide film.

### Claim 19 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, further comprising, before the first step, the steps of:
forming a native oxide film on a surface of the semiconductor substrate; and
annealing the native oxide film in hexachlorodisilane.

### Claim 20 (depends on 19)

The method of manufacturing a semiconductor device according to claim 19, wherein a temperature of the step of annealing performed in hexachlorodisilane is 400° C. or less.

### Claim 21 (depends on 14)

The method of manufacturing a semiconductor device according to claim 14, wherein the third and sixth steps include the step of replacing anyone of the silicon containing gas and the nitrogen containing gas with anyone of an inert gas, a hydrogen chloride gas and a hydrogen gas.

### Claim 22 (depends on 17)

The method of manufacturing a semiconductor device according to claim 17, wherein an Si—H density per unit area of the silicon nitride film formed in the fifth step is 1×1015 cm−2 or less.

### Claim 23 (depends on 17)

The method of manufacturing a semiconductor device according to claim 17, wherein the silicon nitride film formed in said fifth step has a film thickness of 2 nm or less.