# US 2001/0024862 A1 · Method for forming a lower electrode by using an electroplating method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024862 A1
- Document ID: US20010024862A1
- Status: Published application
- Kind: A1
- Application number: 09/735,528
- Filed: 2000-12-14
- Published: 2001-09-27
- Earliest claimed: 1999-12-27
- Assignees: Hyundai Electronics Industries Co., Ltd.
- Inventors: Kwon Hong; Heung-Sik Kwak; Chung-Tae Kim; Hyung-Bok Choi
- Web page: https://patentgrep.com/patent/US20010024862A1

## CPC

- H10D 1/692: {Electrodes}
- H10B 12/315: {with the capacitor higher than a bit line}
- H10W 20/063: {by forming conductive members before forming protective insulating material}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for manufacturing a semiconductor device can form a thick lower electrode made of Pt. The method begins with the preparation of an active matrix provided with at least one transistor, a plurality of conductive plugs electrically connected to the transistors and an insulating layer formed around the conductive plugs. Thereafter, a seed layer is formed on top of the active matrix and a dummy oxide layer is formed on top of the seed layer. And then, the dummy oxide layer is patterned into a predetermined configuration, thereby exposing portions of the seed layer which are located on top of the conductive plugs. The exposed portions are filled with a conductive material to a predetermined thickness. And, the dummy oxide layer and portions of the seed layer which are not covered with the conductive material are removed, thereby obtaining lower electrodes. A capacitor dielectric layer is on the lower electrodes. Finally, an upper electrode layer is formed on the capacitor dielectric layer.

## Claims

### Claim 1

A method for manufacturing a semiconductor device, the method comprising the steps of:
a) preparing an active matrix provided with at least one transistor, a plurality of conductive plugs electrically connected to the transistors and an insulating layer formed around the conductive plugs;
b) forming a seed layer on top of the active matrix;
c) forming a dummy oxide layer on the seed layer;
d) patterning the dummy oxide layer into a predetermined configuration, thereby exposing portions of the seed layer which are located on top of the conductive plugs;
e) filling the exposed portions with a conductive material to a predetermined thickness;
f) removing the dummy oxide layer;
g) removing portions of the seed layer which are not covered with the conductive material, thereby obtaining lower electrodes;
h) forming a capacitor dielectric on the lower electrodes; and
i) forming an upper electrode layer on the capacitor dielectric layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein the capacitor dielectric layer includes barium strontium titanate (BST).

### Claim 3 (depends on 2)

The method of claim 2, before the step b), further comprising the step of forming barrier metals on top of the conductive plugs.

### Claim 4 (depends on 3)

The method of claim 3, wherein the barrier metals includes a material selected from a group consisting of TiN, TiSiN, TiAlN, TaSiN, TaAlN or the like.

### Claim 5 (depends on 3)

The method of claim 3, before the formation of the barrier metals, further comprising the step of forming a layer of TiSx in a thickness ranging from approximately 100 Å to approximately 300 Å to reduce contact resistance between the conductive plugs and the barrier metals.

### Claim 6 (depends on 2)

The method of claim 2, before the step b), further comprising the step of forming anti-reflection coating (ARC) films on portions of the active matrix which are not covered with the diffusion barriers.

### Claim 7 (depends on 6)

The method of claim 6, wherein the ARC films includes a material having a high etch selectivity with respect to the dummy oxide layer and formed in a thickness ranging from approximately 300 Å to approximately 1,000 Å.

### Claim 8 (depends on 7)

The method of claim 7, wherein the ARC films includes SiON.

### Claim 9 (depends on 1)

The method of claim 1, wherein the seed layer includes a material selected from a group consisting of Pt, Ru, Ir, Os, W, Mo, Co, Ni, Au, Ag or the like.

### Claim 10 (depends on 9)

The method of claim 9, wherein the step e) is carried out by electroplating the exposed portions with a conductive material corresponding to that of the seed layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein if the seed layer is made of Pt, the seed layer has a thickness ranging from approximately 50 Å to approximately 1,000 Å.

### Claim 12 (depends on 10)

The method of claim 10, wherein the electroplating process is carried out with a current density ranging from approximately 0.1 mA/cm2 to approximately 10 mA/cm2.

### Claim 13 (depends on 1)

The method of claim 1, wherein the dummy oxide layer includes PSG and has a thickness ranging from approximately 5,000 Å to approximately 20,000 Å.

### Claim 14 (depends on 1)

The method of claim 1, wherein the dummy oxide layer includes USG and has a thickness ranging from approximately 5,000 Å to approximately 10,000 Å.

### Claim 15 (depends on 14)

The method of claim 14, wherein a thickness of Pt ranges from approximately 3,000 Å to approximately 10,000 Å.

### Claim 16 (depends on 1)

The method of claim 1, wherein the step g) is carried out by using a dry etch back.

### Claim 17 (depends on 2)

The method of claim 2, wherein the capacitor dielectric layer is formed by using a chemical vapor deposition (CVD) at a temperature ranging from approximately 400° C. to approximately 600° C. in a thickness ranging from approximately 150 Å to approximately 500 Å.

### Claim 18 (depends on 2)

The method of claim 2, further comprising the step of crystallizing the capacitor dielectric layer by using a rapid thermal process (RTP) at a temperature ranging from approximately 500° C. to approximately 700° C. in the presence of N2 for 30-180 seconds.

### Claim 19 (depends on 1)

The method of claim 1, wherein the step e) is carried out by using a CVD.

### Claim 20 (depends on 1)

The method of claim 1, between the steps d) and e), further comprising the step of dipping the exposed portions of seed layer into a solution selected from a group consisting of a 90% H2SO4 solution, H2SO4/H2O2 solution, HF/H2O solution, HF/HN4F solution during 2-3600 seconds to remove particles or foreign material remaining thereon.