# US 2001/0024860 A1 · Method for manufacturing a gate structure incorporating therein aluminum oxide as a gate dielectric

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024860 A1
- Document ID: US20010024860A1
- Status: Published application
- Kind: A1
- Application number: 09/739,292
- Filed: 2000-12-19
- Published: 2001-09-27
- Earliest claimed: 1999-12-29
- Assignees: Hyundai Electronics Industries Co., Ltd.
- Inventors: Dae-Gyu Park; Se-Aug Jang; Jeong-Youb Lee
- Web page: https://patentgrep.com/patent/US20010024860A1

## CPC

- H10D 64/0134: {with a treatment, e.g. annealing, after the formation of the insulator and before the formation of the conductor}
- H10D 64/01342: {by deposition, e.g. evaporation, ALD or laser deposition (H10D64/01344 takes precedence)}
- H10D 64/01346: {in a gaseous ambient using an oxygen or a water vapour, e.g. oxidation through a layer (H10D64/01344 takes precedence)}
- H10D 64/691: {comprising metallic compounds, e.g. metal oxides or metal silicates (insulators comprising nitrogen H10D64/693)}
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6518: {by introduction of substances into an already-existing insulating layer}
- H10P 14/6529: {by exposure to a gas or vapour}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6929: {the material containing aluminium, e.g. AlSiOx}
- H10P 32/20: Diffusion for doping of insulating layers
- H10D 64/685: {being perpendicular to the channel plane}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method for forming a gate structure begins by preparing a semiconductor substrate provided with an isolation region formed therein. An aluminum oxide (Al2O3) layer is deposited on top of the semiconductor substrate and then, silicon ions plasma doping is carried out. Thereafter, the Al2O3 layer doped with silicon ions is annealed in the presence of oxygen gas or nitrous oxygen to remove a metallic vacancy in the Al2O3 layer. Subsequently, a conductive layer is formed on top of the Al2O3 layer. Finally, the conductive layer is patterned into the gate structure.

## Claims

### Claim 1

A method for forming a gate structure in a semiconductor device, comprising the steps of:
a) preparing a semiconductor substrate with an isolation region;
b) forming an aluminum oxide (Al2O3) layer over the semiconductor substrate;
c) conducting a Si+plasma doping on the aluminum oxide (Al2O3) layer;
d) annealing the doped aluminum oxide (Al2O3) layer with silicon ions;
e) forming a conductive layer over the aluminum oxide (Al2O3) layer; and
f) patterning the conductive layer.

### Claim 2 (depends on 1)

The method as recited in claim 1, wherein the step of forming an aluminum oxide layer includes forming the aluminum oxide layer at a temperature ranging from approximately 150 □ to approximately 700 □ and a pressure ranging from approximately 0.5 Torr to approximately 10 Torr by using a chemical vapor deposition (CVD) or an atomic layer deposition (ALD).

### Claim 3 (depends on 2)

The method as recited in claim 2, wherein said aluminum oxide layer forming step uses an aluminum source including a material selected from a group of trimethyl aluminum (TMA, Al(CH4) 3), Al(CH3)2Cl and AlCl3, and an oxygen source of H2O or O2.

### Claim 4 (depends on 1)

The method as recited in claim 1, wherein the step of conducting a Si+plasma doping uses a silicon source including a material selected from a group of Si RE coil, SiH4, Si2H6 and SiCl4.

### Claim 5 (depends on 4)

The method as recited in claim 4, wherein the step of conducting a Si+plasma doping includes conducting the Si+plasma doping while applying a negative bias to a cathode with 100 eV to 2 kV, having an ion flux of approximately 1E14 to approximately 5E15 ions/cm2, using power of approximately 0.1 W/cm1, and doping Si+dopant into the aluminum oxide layer by controlling a gas flow rate.

### Claim 6 (depends on 1)

The method as recited in claim 1, wherein the step of annealing the aluminum oxide (Al2O3) layer includes annealing at a temperature of approximately 650 □ to approximately 850 □ for 10 to 60 minutes in ambient with a gas selected from a group of oxygen (O2), nitrogen (N2), N2+H2 (hydrogen), N2+D2 (deuterium) and nitrous oxygen (N2O).

### Claim 7 (depends on 1)

The method as recited in claim 1, further comprising the step of removing an organic material produced during the step of conducting a Si+plasma doping.

### Claim 8 (depends on 7)

The method as recited in claim 7, wherein the step of removing the organic material uses a UV ozone (O3) at a temperature ranging from approximately 300 □ to approximately 550 □.

### Claim 9 (depends on 1)

The method as recited in claim 1, wherein the conductive layer includes a material selected from a group of a doped poly-Si, amorphous-Si, W-polycide, Ti-polycide, Co-polycide, Mo-polycide, tungsten (W), tantalum nitride (TaN) tungsten nitride (WN) and titanium nitride (TiN).

### Claim 10 (depends on 1)

The method as recited in claim 1, further comprising the step of forming a silicon dioxide (SiO2) thin film on the semiconductor substrate before forming the aluminum oxide (Al2O3) layer.

### Claim 11 (depends on 10)

The method as recited in claim 10, wherein the step of forming a silicon dioxide (SiO2) thin film includes thermally growing the silicon dioxide (SiO2) thin film on the semiconductor substrate to a thickness ranging from approximately 3 □ to approximately 20 □ using a wet H2/O2 or dry O2 at a temperature ranging from approximately 650 □ to approximately 900 □.

### Claim 12 (depends on 10)

The method as recited in claim 10, wherein the step of forming a silicon dioxide (SiO2) thin film includes using a rapid thermal process (RTP) at a temperature ranging from approximately 700 □ to approximately 950 □ and a pressure ranging from approximately 0.01 Torr to approximately 100 Torr in O2 or N2O gas ambient.

### Claim 13 (depends on 1)

The method as recited in claim 1, wherein the step of preparing a semiconductor substrate includes forming the isolation region using a local oxidation of silicon (LOCOS) or shallow trench isolation (STI).
