# US 2001/0024835 A1 · Ferroelastic lead germanate thin film and deposition method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024835 A1
- Document ID: US20010024835A1
- Status: Published application
- Kind: A1
- Application number: 09/814,273
- Filed: 2001-03-21
- Published: 2001-09-27
- Earliest claimed: 1999-04-28
- Assignees: Sharp Laboratories of America, Inc.
- Inventors: Tingkai Li; Fengyan Zhang; Yoshi Ono; Sheng Teng Hsu
- Web page: https://patentgrep.com/patent/US20010024835A1

## CPC

- H10P 14/69398: {the material having a perovskite structure, e.g. BaTiO3}
- C23C 16/40: Oxides
- H10P 14/6334: {using decomposition or reaction of gaseous or vapour phase compounds, i.e. chemical vapour deposition (deposition by physical ablation of a target H10P14/6329)}
- H10P 14/6342: {Liquid deposition, e.g. spin-coating, sol-gel techniques or spray coating}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A Pb3GeO5 phase PGO thin film is provided. This film has ferroelastic properties that make it ideal for many microelectromechanical applications or as decoupling capacitors in high speed multichip modules. This PGO film is uniquely formed in a MOCVD process that permits a thin film, less than 1 mm, of material to be deposited. The process mixes Pd and germanium in a solvent. The solution is heated to form a precursor vapor which is decomposed. The method provides deposition temperatures and pressures. The as-deposited film is also annealed to enhanced the film's ferroelastic characteristics. A ferroelastic capacitor made from the present invention PGO film is also provided.

## Claims

### Claim 1

A method for forming a ferroelastic lead germanium oxide (PGO) film on an integrated circuit (IC) wafer comprising the steps of:
a) mixing [Pb(thd)2] and [Ge(ETO)4] to form a PGO mixture having a molar ratio in the range of approximately 2:1 to 4:1;
b) dissolving the mixture of Step a) with a solvent of tetrahydrofuran, isopropanol, and tetraglyme to form a precursor solution;
c) heating the solution formed in Step b) to create a precursor gas; and
d) decomposing the precursor gas formed in Step c) on the IC wafer to form a PGO thin film, including a first phase of Pb3GeO5, whereby the PGO film having ferroelastic properties is formed.

### Claim 2 (depends on 1)

A method as in claim 1 in which Step a) includes mixing the [Pb(thd)2] and [Ge(ETO)4] in a molar ratio of approximately 3:1.

### Claim 3 (depends on 1)

A method as in claim 1 in which Step b) includes the solvents tetrahydrofuran, isopropanol, and tetraglyme being in a molar ratio of approximately 8:2:1, respectively.

### Claim 4 (depends on 1)

A method as in claim 1 in which Step b) includes forming a precursor solution having a concentration of approximately 0.1 to 0.5 moles of PGO mixture per liter of solvent.

### Claim 5 (depends on 1)

A method as in claim 1 wherein a liquid pump and precursor vaporizer are provided, in which Step c) includes using the precursor vaporizer to heat the precursor solution to a temperature in the range of approximately 180 to 250 degrees C., whereby the precursor gas is formed, and including a further step, following Step b), and preceding Step c), of:
b1) using the liquid pump to introduce the precursor solution of Step b) to the precursor vaporizer in Step c) at a rate in the range of approximately 0.1 to 0.5 milliliters per minute (ml/min).

### Claim 6 (depends on 1)

A method as in claim 1 in wherein the IC wafer is located in a reactor, and a further steps of:
c1) mixing the precursor gas in the chamber with an argon gas shroud flow in the range of approximately 4000 to 6000 square cubic centimeters per minute (sccm), preheated to a temperature in the range of approximately 170 to 250 degrees C.; and
c2) introducing an oxygen flow to the reactor in the range of approximately 1000 to 3000 sccm.

### Claim 7 (depends on 1)

A method as in claim 1 wherein the IC wafer is located on a wafer chuck in a reactor, in which Step c) includes establishing a precursor vapor pressure in the range of approximately 30 to 50 torr (T), and in which Step d) includes heating the wafer chuck to a temperature in the range of approximately 500 to 650 degrees C. and establishing a reactor chamber pressure in the range of approximately 5 to 10 T.

### Claim 8 (depends on 1)

A method as in claim 1 including further steps following Step d) of:
e) cooling the PGO film to approximately room temperature in an oxygen atmosphere; and
f) annealing the PGO film formed in Step d) in an atmosphere selected from the group of oxygen and oxygen with Pb atmospheres, whereby the ferroelastic properties of the PGO film are improved.

### Claim 9 (depends on 8)

A method as in claim 8 wherein a ferroelastic device is formed with the PGO film of in Step d), and including further steps following Step f) of:
g) forming a conductive electrode overlying the PGO film; and
h) annealing the PGO film in an atmosphere selected from the group of oxygen and oxygen with Pb atmospheres, whereby the interface between the PGO film, formed in Step d), and the electrode formed in Step g), is improved.

### Claim 10 (depends on 9)

A method as in claim 9 in which Steps f) and h) include the oxygen being introduced at a partial pressure greater than approximately 20%.

### Claim 11 (depends on 9)

A method as in claim 9 in which Steps f) and h) include using annealing methods selected from the group consisting of furnace annealing at a temperature in the range of approximately 500 to 600 degrees C. for a duration of approximately 30 minutes to 2 hours, and rapid thermal annealing (RTA) at a temperatures in the range of approximately 500 to 750 degrees C.

### Claim 12 (depends on 9)

A method as in claim 9 in which Steps f) and h) in which the RTA includes a duration in the range of approximately 10 to 1800 seconds, and a thermal temperature ramp-up in the range of approximately 10 to 200 degrees C. per second.

### Claim 13 (depends on 9)

A method as in claim 9 in which Steps d), f), and h) include the Pb3GeO5 first phase having a grain size in the range of approximately 1 to 2 microns.

### Claim 14 (depends on 1)

A method as in claim 1 including a further step, preceding Step a), of:
depositing a conductive electrode overlying the IC wafer, the conductive electrode being selected from the group consisting of Ir and Pt.

### Claim 15 (depends on 1)

A method as in claim 1 in which Step d) includes forming a PGO film having a film thickness of less than approximately 1 millimeter (mm).

### Claim 16

A lead germanium oxide (PGO) thin film having ferroelastic properties comprising:
a first phase of Pb3GeO5; and
in which the thickness of said first phase of Pb3GeO5 is less than approximately 1 mm, whereby said Pb3GeO, phase improves the ferroelastic properties of the PGO film.

### Claim 17 (depends on 16)

A PGO film as in claim 16 in which said first phase Pb3GeO, has a grain size in the range of approximately 1 to 2 microns.

### Claim 18

A capacitor having ferroelastic properties comprising:
a first conductive electrode;
a PGO thin film including a first phase of Pb3GeO5 overlying said first electrode; and
a second conductive electrode overlying said PGO film, whereby a PGO film capacitor is formed having ferroelastic properties.

### Claim 19 (depends on 18)

A capacitor as in claim 18 in which the ferroelastic properties include a dielectric constant in the range of approximately 50 to 100.

### Claim 20 (depends on 18)

A capacitor as in claim 18 in which the ferroelastic properties include a leakage current of 4×10−6 A/cm2 at 100 kV/cm.

### Claim 21 (depends on 18)

A capacitor as in claim 18 in which the minimum polarization voltage is approximately 1 volt and the saturation voltage is approximately 5 volts.