- Number: US 2001/0024759 A1
- Document ID: US20010024759A1
- Status: Published application
- Kind: A1
- Application number: 09/849,185
- Filed: 2001-05-04
- Published: 2001-09-27
- Earliest claimed: 1998-06-11
- Inventors: Andre J. Uzee; Michael O. Myers; Calvin P. Esneault
- Web page: https://patentgrep.com/patent/US20010024759A1

## CPC

- C08L 53/02: of vinyl-aromatic monomers and conjugated dienes
- C08F 283/008: {on to unsaturated polymers}
- C08F 290/06: Polymers provided for in subclass C08G
- C08F 297/04: polymerising vinyl aromatic monomers and conjugated dienes
- G03F 7/033: the binders being polymers obtained by reactions only involving carbon-to-carbon unsaturated bonds, e.g. vinyl polymers
- G03F 7/0388: {with ethylenic or acetylenic bands in the side chains of the photopolymer}
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

A photo-curable composition comprising (a) an elastomeric component containing one or more unsaturated, high molecular weight, endgroup-modified polymers; (b) a photopolymerization initiating system; optionally (c) one or more cross-linking agents; and optionally (d) other additives. Photo-curable compositions of the present invention exhibit faster cross-linking (i.e., curing) rates (i.e., lower minimum exposure times) than similar compositions containing no endgroup-modified polymers. Cured compositions of the present invention exhibit lower solvent swell, and similar or increased softness (i.e., lower hardness as measured by Shore A hardness) when compared to cured compositions containing no unsaturated, high molecular weight, endgroup-modified polymers.

## Claims

### Claim 1

A photo-cured composition, comprising:
(a) an elastomeric component containing one or more unsaturated polymers having a number average molecular weight of greater than about 30,000 and having a reactive endgroup, the reactive endgroup being one capable of free-radical addition polymerization, co-polymerization, oligomerization, or dimerization initiated by a photo-initiator in the presence of actinic radiation; and
(b) a photopolymerization initiating system wherein the composition of (a) and (b) has been exposed to at least about 4.11 Joules/cm2 of actinic radiation.

### Claim 2 (depends on 1)

The photo-cured composition according to claim 1, wherein at least about 10% by weight of all polymers present in said elastomeric component are endgroup-modified polymers.

### Claim 3 (depends on 1)

The photo-cured composition according to claim 1, wherein the composition further comprises one or more cross-linking agents.

### Claim 4 (depends on 3)

The photo-cured composition according to claim 3, wherein one or more cross-linking agents are photopolymerizable, ethylenically unsaturated, low molecular weight compounds.

### Claim 5 (depends on 4)

The photo-cured composition according to claim 4, wherein the composition contains from about 0.1% to about 10% by weight of photopolymerizable, ethylenically unsaturated, low molecular weight compounds

### Claim 6 (depends on 1)

The photo-cured composition according to claim 1, wherein one or more of the polymers having a reactive endgroup also has a number average molecular weight of greater than about 50,000.

### Claim 7 (depends on 1)

The photo-cured composition according to claim 1, wherein one or more of the polymers having a reactive endgroup also has a number average molecular weight of greater than about 70,000.

### Claim 8 (depends on 1)

The photo-cured composition according to claim 1, wherein one or more of the polymers having a reactive endgroup also has a number average molecular weight of less than about 300,000.

### Claim 9 (depends on 1)

The photo-cured composition according to claim 1, wherein one or more of the polymers having a reactive endgroup also has a number average molecular weight of less than about 250,000.

### Claim 10 (depends on 1)

The photo-cured composition according to claim 1, wherein one or more of the polymers having a reactive endgroup also has a number average molecular weight of less than about 200,000.

### Claim 11 (depends on 1)

The photo-cured composition according to claim 1, wherein the reactive endgroup is an acrylate group, an alkylacrylate, a methacrylate group, a maleate group, a fumarate, a vinyl ether group, or a vinyl ester group.

### Claim 12 (depends on 1)

The photo-cured composition according to claim 1, wherein the reactive endgroup is an acrylate group, a methacrylate group, or a maleate group.

### Claim 13 (depends on 1)

The photo-cured composition of claim 1 wherein the composition has been exposed to up to about 12.94 Joules/cm2 of actinic radiation.

### Claim 14 (depends on 1)

The photo-cured composition of claim 1 wherein the composition has been exposed to up to about 8.21 Joules/cm2 of actinic radiation.