# US 2001/0024744 A1 · Active material for positive electrode for alkaline secondary cell and method for producing the same, and alkaline secondary cell using the active material for positive electrode and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024744 A1
- Document ID: US20010024744A1
- Status: Published application
- Kind: A1
- Application number: 09/749,789
- Filed: 2000-12-28
- Published: 2001-09-27
- Earliest claimed: 1999-12-28
- Assignees: Toshiba Battery Co., Ltd.
- Inventors: Kunihiko Miyamoto; Naomi Bando
- Web page: https://patentgrep.com/patent/US20010024744A1

## CPC

- H01M 4/52: of nickel, cobalt or iron
- H01M 10/28: Construction or manufacture
- H01M 10/342: {Gastight lead accumulators (H01M10/121 takes precedence)}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

Provided is a active material for positive electrode for an alkaline secondary cell, which advantageously exhibits improved overdischarge characteristics, improved utilization of the active material and an improved effect of suppressing the rise in cell internal pressure, a method for producing the same, and an alkaline secondary cell using the above active material for positive electrode, especially a nickel-hydrogen secondary cell. The above active material comprises nickel hydroxide particles each having a surface to which a cobalt oxide sticks, wherein the cobalt oxide contains 20 to 40 % by mole of cobalt(II) oxide, wherein the nickel hydroxide particles form an eutectic together with Co and Zn or/and Y, and the Co content of the eutectic is 2 % by mass or less, and the nickel hydroxide particles have a value of a half width of the peak ascribed to the (101) crystal face diffraction of 0.8°/2θ(Cu-Kα) or more as measured by powder X-ray diffractometry.

## Claims

### Claim 1

A active material for positive electrode for an alkaline secondary cell, comprising nickel hydroxide particles each having a surface to which a cobalt oxide sticks,
wherein a part of said cobalt oxide comprises an oxide of cobalt(II).

### Claim 2 (depends on 1)

The active material for positive electrode according to claim 1, wherein said oxide of cobalt(II) is present in an amount of 20 to 40% by mole, based on the total mole of said cobalt oxide.

### Claim 3 (depends on 1, 2)

The active material for positive electrode according to claim 1 or 2, wherein said nickel hydroxide particles form an eutectic together with cobalt and zinc or/and yttrium, and the content of said cobalt in the eutectic is 2% by mass or less.

### Claim 4 (depends on 1, 2, 3)

The active material for positive electrode according to any one of claims 1 to 3, wherein said nickel hydroxide particles have a crystallinity wherein the value of a half width of the peak ascribed to the (101) crystal face diffraction is 0.8°/2θ(Cu-Kα) or more as measured by powder X-ray diffractometry.

### Claim 5

A method for producing a active material for positive electrode for an alkaline secondary cell, said method comprising:
mixing and stirring nickel hydroxide particles each having a surface to which a cobalt(II) compound sticks or/and mixture particles of nickel hydroxide particles and particles of metallic cobalt or a cobalt(II) compound with an alkaline aqueous solution in the presence of oxygen; and
subjecting the resultant mixed and stirred system to heat treatment by radiation while mixing and stirring.

### Claim 6 (depends on 5)

The method according to claim 5, wherein said radiation is a microwave from a magnetron.

### Claim 7 (depends on 1, 2, 3, 4)

An alkaline secondary cell having incorporated thereinto a positive electrode comprising the active material for positive electrode according to any one of claims 1 to 4.

### Claim 8

A nickel-hydrogen secondary cell, comprising:
a cell casing;
an alkaline electrolytic liquid; and
an electrode group comprising a positive electrode which comprises a conductive core material having carried thereon an active material comprised mainly of nickel hydroxide particles each having a surface coated with a sodium-containing cobalt oxide, or an active material comprised mainly of a mixture of nickel hydroxide particles each having a surface coated with a sodium-containing cobalt oxide and metallic cobalt or a cobalt(II) compound, a negative electrode which comprises a conductive core material having carried thereon a negative electrode preparation comprised mainly of a metal alloy having hydrogen occluded therein, and a separator disposed between the positive electrode and the negative electrode,
wherein said electrode group is sealed in said cell casing together with said alkaline electrolytic liquid,
wherein said alkaline electrolytic liquid contains 0.3 to 1.2 mole of lithium hydroxide.

### Claim 9 (depends on 8)

The nickel-hydrogen secondary cell according to claim 8, wherein said sodium-containing cobalt oxide is present in an amount of 0.5 to 20% by mass in terms of the mass of cobalt, based on the total mass of the active material.

### Claim 10 (depends on 8, 9)

The nickel-hydrogen secondary cell according to claim 8 or 9, wherein said sodium is present in an amount of 0.05 to 5% by mass, based on the total mass of the active material.

### Claim 11 (depends on 8, 9, 10)

The nickel-hydrogen secondary cell according to any one of claims 8 to 10, wherein said negative electrode preparation has incorporated thereinto metallic cobalt or/and a cobalt(II) compound.

### Claim 12 (depends on 8)

A method for producing the nickel-hydrogen secondary cell according to claim 8, wherein the alkaline electrolytic liquid is poured into the cell casing and the cell casing is sealed up, and then, the resultant casing is allowed to stand in an environment at a temperature of 40 to 100° C. for 1 day or more.