# US 2001/0024736 A1 · Aluminum alloy member and production method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024736 A1
- Document ID: US20010024736A1
- Status: Published application
- Kind: A1
- Application number: 09/779,736
- Filed: 2001-02-09
- Published: 2001-09-27
- Earliest claimed: 2000-02-09
- Assignees: Honda Giken Kogyo Kabushiki Kaisha
- Inventors: Hiroyuki Oketani; Hiroyuki Uchida; Shigeyuki Hara; Yuji Marui
- Web page: https://patentgrep.com/patent/US20010024736A1

## CPC

- C23C 30/00: Coating with metallic material characterised only by the composition of the metallic material, i.e. not characterised by the coating process (C23C26/00, C23C28/00 take precedence)
- B32B 15/017: {one layer being formed of aluminium or an aluminium alloy, another layer being formed of an alloy based on a non ferrous metal other than aluminium}
- C22C 21/02: with silicon as the next major constituent
- F02F 3/00: Pistons
- F05C 2201/021: Aluminium
- Y10S 428/925: Relative dimension specified
- Y10S 428/926: Thickness of individual layer specified
- Y10T 29/49249: Piston making
- Y10T 29/49256: with assembly or composite article making
- Y10T 29/49263: by coating or cladding
- Y10T 29/49272: with liner, coating, or sleeve
- Y10T 428/12472: Microscopic interfacial wave or roughness
- Y10T 428/12708: Sn-base component
- Y10T 428/12736: Al-base component
- Y10T 428/12993: Surface feature [e.g., rough, mirror]
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F02F: CYLINDERS, PISTONS OR CASINGS, FOR COMBUSTION ENGINES; ARRANGEMENTS OF SEALINGS IN COMBUSTION ENGINES
- F05C: INDEXING SCHEME RELATING TO MATERIALS, MATERIAL PROPERTIES OR MATERIAL CHARACTERISTICS FOR MACHINES, ENGINES OR PUMPS OTHER THAN NON-POSITIVE-DISPLACEMENT MACHINES OR ENGINES
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

To provide an aluminum alloy member having a high machinability while keeping a sufficient mechanical strength and a sufficient wear resistance, and a method of producing the aluminum alloy member. In an aluminum alloy member formed from an aluminum-silicon alloy by casting, eutectic silicon grains are exposed from at least part of an exposed plane of the aluminum alloy member. A coating layer having a thickness nearly equal to or thinner than a diameter of each of the eutectic silicon grains is formed on the exposed plane from which the eutectic silicon grains are exposed.

## Claims

### Claim 1

An aluminum alloy member formed from an aluminum-silicon alloy by casting, comprising:
eutectic silicon grains exposed from at least part of an exposed plane of said aluminum alloy member.

### Claim 2 (depends on 1)

The aluminum alloy member according to claim 1, wherein said aluminum alloy member is a piston for an internal combustion engine.

### Claim 3 (depends on 2)

The aluminum alloy member according to claim 2, wherein said eutectic silicon grains are exposed from a side portion, including at least a piston ring groove, of said piston.

### Claim 4 (depends on 1)

The aluminum alloy member according to claim 1, wherein said aluminum alloy member is a cylinder of an internal combustion engine.

### Claim 5 (depends on 1)

The aluminum alloy member according to claim 1, wherein a coating layer having a thickness nearly equal to or thinner than a diameter of each of said eutectic silicon grains is formed on said exposed plane from which said eutectic silicon grains are exposed.

### Claim 6 (depends on 2)

The aluminum alloy member according to claim 2, wherein a coating layer having a thickness nearly equal to or thinner than a diameter of each of said eutectic silicon grains is formed on said exposed plane from which said eutectic silicon grains are exposed.

### Claim 7 (depends on 3)

The aluminum alloy member according to claim 3, wherein a coating layer having a thickness nearly equal to or thinner than a diameter of each of said eutectic silicon grains is formed on said exposed plane from which said eutectic silicon grains are exposed.

### Claim 8 (depends on 4)

The aluminum alloy member according to claim 4, wherein a coating layer having a thickness nearly equal to or thinner than a diameter of each of said eutectic silicon grains is formed on said exposed plane from which said eutectic silicon grains are exposed.

### Claim 9 (depends on 5)

The aluminum alloy member according to claim 5, wherein said coating layer is a tin plating layer.

### Claim 10 (depends on 6)

The aluminum alloy member according to claim 6, wherein said coating layer is a tin plating layer.

### Claim 11 (depends on 7)

The aluminum alloy member according to claim 7, wherein said coating layer is a tin plating layer.

### Claim 12 (depends on 8)

The aluminum alloy member according to claim 8, wherein said coating layer is a tin plating layer.

### Claim 13 (depends on 9)

The aluminum alloy member according to claim 9, wherein the diameter of each of said eutectic silicon grains is in a range of 1 to 1.5 μm and the content of said eutectic silicon grains is in a range of 10 to 13 wt %, and the thickness of said tin plating layer is in a range of 2 to 3 μm.

### Claim 14 (depends on 10)

The aluminum alloy member according to claim 10, wherein the diameter of each of said eutectic silicon grains is in a range of 1 to 1.5 μm and the content of said eutectic silicon grains is in a range of 10 to 13 wt %, and the thickness of said tin plating layer is in a range of 2 to 3 μm.

### Claim 15 (depends on 11)

The aluminum alloy member according to claim 11, wherein the diameter of each of said eutectic silicon grains is in a range of 1 to 1.5 μm and the content of said eutectic silicon grains is in a range of 10 to 13 wt %, and the thickness of said tin plating layer is in a range of 2 to 3 μm.

### Claim 16 (depends on 12)

The aluminum alloy member according to claim 12, wherein the diameter of each of said eutectic silicon grains is in a range of 1 to 1.5 μm and the content of said eutectic silicon grains is in a range of 10 to 13 wt %, and the thickness of said tin plating layer is in a range of 2 to 3 μm.

### Claim 17

A method of producing an aluminum alloy member formed from an aluminum-silicon alloy, comprising the steps of:
casting an aluminum-silicon alloy having an eutectic composition to form an aluminum alloy raw material;
machining the surface of the aluminum alloy raw material formed by casting;
etching the machined surface, to expose eutectic silicon grains therefrom; and
forming a coating layer on the surface from which the eutectic silicon grains are exposed.

### Claim 18 (depends on 17)

The method of producing an aluminum alloy member according to claim 17, wherein the diameter of each of the eutectic silicon grains is in a range of 1 to 1.5 μm and the content of the eutectic silicon grains is in a range of 10 to 13 wt %, and the thickness of the coating layer is in a range of 2 to 3 μm.

### Claim 19 (depends on 17)

The method of producing an aluminum alloy member according to claim 17, wherein the etching is performed by eroding the machined surface with a nitric acid-hydrofluoric acid solution at room temperature.

### Claim 20

A method of producing an aluminum alloy member formed from an aluminum-silicon alloy, comprising the steps of:
casting an aluminum-silicon alloy having a hypo-eutectic composition to form an aluminum alloy raw material;
machining the surface of the aluminum alloy raw material formed by casting;
etching the machined surface, to expose eutectic silicon grains therefrom; and
forming a coating layer on the surface from which the eutectic silicon grains are exposed.

### Claim 21 (depends on 20)

The method of producing an aluminum alloy member according to claim 20, wherein the diameter of each of the eutectic silicon grains is in a range of 1 to 1.5 μm and the content of the eutectic silicon grains is in a range of 10 to 13 wt %, and the thickness of the coating layer is in a range of 2 to 3 μm.

### Claim 22 (depends on 20)

The method of producing an aluminum alloy member according to claim 20, wherein the etching is performed by eroding the machined surface with a nitric acid-hydrofluoric acid solution at room temperature.