# US 2001/0024728 A1 · Article coated with water-repellent film, liquid composition for coating with water-repellent film, and process for producing article coated with water-repellent film

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024728 A1
- Document ID: US20010024728A1
- Status: Published application
- Kind: A1
- Application number: 09/822,719
- Filed: 2001-03-30
- Published: 2001-09-27
- Earliest claimed: 1999-08-02
- Assignees: Nippon Sheet Glass Co., Ltd., Japan
- Inventors: Kazutaka Kamitani; Hiroaki Yamamoto
- Web page: https://patentgrep.com/patent/US20010024728A1

## CPC

- C09D 183/00: Coating compositions based on macromolecular compounds obtained by reactions forming in the main chain of the macromolecule a linkage containing silicon, with or without sulfur, nitrogen, oxygen, or carbon only; Coating compositions based on derivatives of such polymers
- C03C 17/009: {Mixtures of organic and inorganic materials, e.g. ormosils and ormocers}
- C09D 1/00: Coating compositions, e.g. paints, varnishes or lacquers, based on inorganic substances
- Y10T 428/31612: As silicone, silane or siloxane
- Y10T 428/31663: As siloxane, silicone or silane
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

There are provided articles coated with high-performance water-repellent films with high hardness that can withstand outdoor use, which are water-repellent film-coated articles that comprise a substrate and a water-repellent film composed mainly of silicon oxide and having a water-repellent group coated on the surface of the substrate, and are characterized by containing at least one type of metal oxide selected from the group consisting of magnesium oxide, calcium oxide, strontium oxide and boron oxide, as well as a process for preparation of such water-repellent film-coated articles at a high rate of productivity and a coating liquid composition for preparation of such water-repellent film-coated articles.

## Claims

### Claim 1

A water-repellent film-coated article comprising
a substrate and
a water-repellent film, composed of silicon oxide and at least one of metal oxide selected from the group consisting of magnesium oxide, calcium oxide, strontium oxide and boron oxide and having a water-repellent group, coated on the surface of the substrate.

### Claim 2 (depends on 1)

A water-repellent film-coated article according to claim 1, wherein said water-repellent film contains
silicon oxide at 70-99 mole percent (based on SiO2),
at least one of metal oxide selected from the group consisting of magnesium oxide, calcium oxide, strontium oxide and boron oxide at a total of 1-30 mole percent (based on MgO, CaO, Sro and BO3/2), and
a water-repellent group at 0.01-20 wt %.

### Claim 3 (depends on 2)

A water-repellent film-coated article according to claim 2, wherein said water-repellent film further contains, in terms of mole percent, at least one of metal oxide selected from the group consisting of zirconium oxide, aluminum oxide, gallium oxide, indium oxide, scandium oxide, yttrium oxide, lanthanum oxide, cerium oxide, cobalt oxide, iron oxide, nickel oxide, copper oxide and zinc oxide at 0.5-5%, based on ZrO2, AlO3/2 GaO3/2, InO3/2, SCO3/2, YO3/21 LaO3/2, CeO3/2, CoO, FeO3/2, NiO2, CuO and ZnO.

### Claim 4 (depends on 1)

A water-repellent film-coated article according to claim 1, wherein said water-repellent film contains
silicon oxide at 70-98 mole percent (based on SiO2),
magnesium oxide and/or calcium oxide at 1-29 mole percent (based on MgO and Cao),
boron oxide and/or zirconium oxide at 1-29 mole percent (based on BO3/2 and ZrO2) and
a water-repellent group at 0.01-20 wt %.

### Claim 5 (depends on 4)

A water-repellent film-coated article according to claim 4, wherein said water-repellent film further contains, in terms of mole percent, at least one of metal oxide selected from the group consisting of aluminum oxide, gallium oxide, indium oxide, scandium oxide, yttrium oxide, lanthanum oxide, cerium oxide, cobalt oxide, iron oxide, nickel oxide, copper oxide and zinc oxide at 0.5-5%, based on AlO3/2, GaO3/2, InO3/2, ScO3/2, YO3/2, LaO3/2, CeO3/2, CoO, FeO3/2, NiO2, CuO and ZnO.

### Claim 6 (depends on 1, 2, 3, 4, 5)

A water-repellent film-coated article according to any one of claims 1 to 5, wherein said water-repellent group is an alkyl group or fluoroalkyl group.

### Claim 7

A water-repellent film-coating composition containing
(A) a thoroughly hydrolyzable silane compound,
(B) a silane compound with a water-repellent group,
(C) an acid and
(D) a compound of at least one of metal selected from the group consisting of magnesium, calcium, strontium and boron.

### Claim 8 (depends on 7)

A water-repellent film-coating composition according to claim 7 which contains said silane compound (A) at 0.01-2 wt % based on SiO2, said silane compound (B) at 0.00001-0.15 wt % based on Sio2, said acid at 0.001-3 N, water at 0-5 wt % and said compound (D) at a molar ratio of 0.01-0.4, based on MgO, CaO, SrO and BO3/2, with respect to said silane compound.

### Claim 9 (depends on 7, 8)

A water-repellent film-coating composition according to claim 7 or 8 which contains an alcohol as a solvent.

### Claim 10

A water-repellent film-coating composition containing
(A) a thoroughly hydrolyzable silane compound or its hydrolysate at 0.01-2 wt % (based on SiO2),
(B) a silane compound with a water-repellent group at 0.00001-0.15 wt % (based on SiO2),
(C) an acid at 0.001-3 N,
(D-1) a magnesium and/or calcium compound at a molar ratio of 0.01-0.4, based on MgO and CaO, with respect to said silane compound (A) (based on SiO2),
(D-2) a boron and/or zirconium compound at a molar ratio of 0.01-0.4, based on BO3/2 and ZrO2, with respect to said silane compound (A) (based on SiO2),
(E) a compound of at least one of metal selected from the group consisting of cobalt, iron, nickel, copper, aluminum, gallium, indium, scandium, yttrium, lanthanum, cerium and zinc at a molar ratio of 0-0.4, based on CoO, FeO3/2, NiC2, CuO, AlO3/2, GaO3/2, InO3/2, ScO3/2, YO3/2, LaO3/2, CeO3/2 and ZnO, with respect to said silane compound (A) (based on SiO2), and
(F) water at 0-20 wt %.

### Claim 11 (depends on 10)

A water-repellent film-coating composition according to claim 10 which contains an alcohol as the solvent.

### Claim 12 (depends on 7, 8, 9, 10, 11)

A water-repellent film-coating composition according to any one of claims 7 to 11, wherein said silane compound (A) is a tetraalkoxysilane or tetrachlorosilane.

### Claim 13 (depends on 7, 8, 9, 10, 11, 12)

A water-repellent film-coating composition according to any one of claims 7 to 12, wherein said acid is hydrochloric acid, nitric acid, acetic acid, formic acid or trifluoroacetic acid.

### Claim 14 (depends on 7, 8, 9, 10, 11, 12, 13)

A process for preparation of a water-repellent film-coated article, characterized by applying a water-repellent film-coating composition according to any one of claims 7 to 13 onto a substrate surface and drying it.

### Claim 15 (depends on 14)

A process for preparation of a water-repellent film-coated article according to claim 14, wherein said drying is carried out at room temperature.

### Claim 16 (depends on 14, 15)

A process for preparation of a water-repellent film-coated article according to claim 14 or 15, wherein said drying is carried out in an atmosphere at 40% relative humidity or lower.

### Claim 17 (depends on 14, 15, 16)

A process for preparation of a water-repellent film-coated article according to any one of claims 14 to 16, wherein said drying is followed by heating at a temperature of from room temperature up to 300° C.

### Claim 18 (depends on 14, 15, 16)

A process for preparation of a water-repellent film-coated article according to any one of claims 14 to 16, wherein said drying is followed by heating at a temperature of from room temperature up to 150° C.