# US 2001/0024726 A1 · Oxidation resistant carbonaceous material and method for producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024726 A1
- Document ID: US20010024726A1
- Status: Published application
- Kind: A1
- Application number: 09/802,581
- Filed: 2001-03-08
- Published: 2001-09-27
- Earliest claimed: 2000-03-23
- Assignees: NGK Insulators, Ltd.
- Inventors: Shigeru Hanzawa; Kenji Nakano
- Web page: https://patentgrep.com/patent/US20010024726A1

## CPC

- C04B 41/009: {characterised by the material treated}
- C04B 41/5059: {Silicon carbide}
- C04B 41/87: Ceramics
- Y10T 428/30: Self-sustaining carbon mass or layer with impregnant or other layer
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

To provide an innovative oxidation resistant carbonaceous material usable as an oxidation resistant carbonaceous material practically prevented from oxidation for a long duration even at a high temperature at lowest 800° C. in the atmospheric air at a reasonable price and satisfying the properties such as light weight property in terms of saving energy and easy workability additionally to high strength (high heat impact resistance) at a high temperature, high reliability (toughness, impact resistance, wear resistance) as a material, and durability to environments (corrosion resistance, oxidation resistance, radiation resistance) and to provide a method for producing the same oxidation resistant carbonaceous material. This oxidation resistant carbonaceous material coated with an oxidation resistant protective layer of silicon carbide practically insusceptible to oxidation even being exposed at a high temperature at lowest 800° C. in the atmospheric air for a long duration can be obtained by forming the oxidation resistant protective layer of silicon carbide by applying a coating agent containing metallic silicon and a phenol resin in a desired thickness to at least a part of the surface of a carbonaceous material, carbonizing the phenol resin by prefiring the coating agent at 1000° C. or lower in an inert atmosphere, heating the material to 1420 to 2200° C. in the same atmosphere, and causing reaction of the practically entire amount of the metallic silicon with carbon in the same temperature range.

## Claims

### Claim 1

An oxidation resistant carbonaceous material which is a carbonaceous material coated with an oxidation resistant protective layer of silicon carbide practically insusceptible to oxidation even at a high temperature of 800° C. or higher

### Claim 2 (depends on 1)

An oxidation resistant carbonaceous material as claimed in claim 1, wherein said carbonaceous material is selected from the group consisting of a C/C composite, a Si—SiC type composite material, and a SiC type composite material.

### Claim 3 (depends on 1)

An oxidation resistant carbonaceous material as claimed in claim 1, wherein the oxidation resistant carbonaceous material is a formed product.

### Claim 4

A method for producing an oxidation resistant carbonaceous material whose surface is coated with an oxidation resistant protective layer of silicon carbide practically insusceptible to oxidation even if the material is exposed for a long duration to a high temperature of 800° C. or higher in the presence of the atmospheric air, comprising applying a coating agent containing metallic silicon and a phenol resin to at least a part of the surface of a carbonaceous material, carbonizing the phenol resin by prefiring the coating agent at 1000° C. or lower in an inert atmosphere, heating the material to 1420 to 2200° C. in the same atmosphere, and reacting the practically total amount of the metallic silicon with carbon in the same temperature range to form the oxidation resistant protective layer of silicon carbide.

### Claim 5 (depends on 4)

A method for producing an oxidation resistant carbonaceous material as claimed in claim 4, wherein the thickness of the applied coating agent is 50 to 500 μm.

### Claim 6 (depends on 4)

A method for producing an oxidation resistant carbonaceous material as claimed in claim 4, wherein the carbonaceous material is selected from the group consisting of a C/C composite, a Si—SiC type composite material, and a SiC type composite material.