# US 2001/0024700 A1 · Ruthenium-containing ultrasonically coated substrate for use in a capacitor and method of manufacture

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024700 A1
- Document ID: US20010024700A1
- Status: Published application
- Kind: A1
- Application number: 09/872,110
- Filed: 2001-06-01
- Published: 2001-09-27
- Earliest claimed: 1997-05-01
- Inventors: Asbish Shah; Barry C. Muffoletto
- Web page: https://patentgrep.com/patent/US20010024700A1

## CPC

- H01G 9/04: Electrodes {or formation of dielectric layers thereon}
- H01G: CAPACITORS; CAPACITORS, RECTIFIERS, DETECTORS, SWITCHING DEVICES, LIGHT-SENSITIVE OR TEMPERATURE-SENSITIVE DEVICES OF THE ELECTROLYTIC TYPE (selection of specified materials as dielectric H01B3/00; capacitors having potential barriers H10D1/62, H10K10/10)

## Abstract

A deposition process for coating a substrate with an ultrasonically generated aerosol spray, is described. The resultant droplets are much smaller in size than those produced by conventional processes, thereby providing the present coating having an increased surface area. When the coated substrate is an electrode in a capacitor, a greater surface area results in an increased electrode capacitance. A preferred coating is of a ruthenium-containing oxide.

## Claims

### Claim 1

A coated substrate, which comprises:
a) a substrate of a conductive metal; and
b) a coating of at least a ruthenium-containing compound provided on a surface of the substrate, wherein the coating is characterized as comprising particles having been formed from an ultrasonically generated aerosol of the ruthenium-containing compound dissolved in a solvent substantially devoid of alcohol contacted with the substrate.

### Claim 2 (depends on 1)

The coated substrate of claim 1 wherein the ruthenium-containing compound is a ruthenium-containing oxide, or a precursor thereof.

### Claim 3 (depends on 2)

The coated substrate of claim 2 wherein the precursor of the ruthenium-containing oxide is selected from the group consisting of a nitrate, a sulfate, a phosphate and a chloride.

### Claim 4 (depends on 2)

The coated substrate of claim 2 wherein the precursor is either ruthenium nitrosyl nitrate or ruthenium chloride.

### Claim 5 (depends on 1)

The coated substrate of claim 1 wherein a majority of the particles have diameters of less than about 10 microns.

### Claim 6 (depends on 1)

The coated substrate of claim 1 wherein an internal surface area of the coating is about 10 m2/gram to about 1,500 m2/gram.

### Claim 7 (depends on 1)

The coated substrate of claim 1 wherein the coating includes a second metal.

### Claim 8 (depends on 7)

The coated substrate of claim 7 wherein the second metal is selected from the group consisting of tantalum, titanium, nickel, iridium, platinum, palladium, gold, silver, cobalt, molybdenum, niobium, ruthenium, manganese, tungsten, iron, zirconium, hafnium, rhodium, vanadium, osmium, and mixtures thereof.

### Claim 9 (depends on 1)

The coated substrate of claim 1 wherein the coating is comprised of ruthenium and tantalum.

### Claim 10 (depends on 1)

The coated substrate of claim 1 wherein the coating has a thickness of about a hundred Angstroms to about 0.1 millimeters.

### Claim 11 (depends on 1)

The coated substrate of claim 1 wherein the substrate is selected from the group consisting of tantalum, titanium, nickel, molybdenum, niobium, cobalt, stainless steel, tungsten, platinum, palladium, gold, silver, copper, chromium, vanadium, aluminum, zirconium, hafnium, zinc, iron, and mixtures thereof.

### Claim 12 (depends on 1)

The coated substrate of claim 1 wherein the substrate has a thickness of about 0.001 to 2 millimeters.

### Claim 13 (depends on 1)

The coated substrate of claim 1 wherein the substrate is characterized as having had its surface area increased prior to being coated.

### Claim 14 (depends on 13)

The coated substrate of claim 13 wherein the increased surface area is characterized as having been formed by contacting the substrate with an acid.

### Claim 15 (depends on 13)

The coated substrate of claim 13 wherein the increased surface area is characterized as having been formed by mechanical means including rough threading, grit blasting, scraping, plasma etching, abrading and wire brushing the substrate.

### Claim 16 (depends on 1)

The coated substrate of claim 1 wherein the substrate is characterized as having been cleaned by one of the group consisting of an aqueous degreasing solution, a non-aqueous degreasing solution and plasma cleaning prior to being coated.

### Claim 17 (depends on 1)

The coated substrate of claim 1 wherein the substrate is characterized as having had its surface increased in electrical conductivity.

### Claim 18 (depends on 1)

The coated substrate of claim 1 wherein the aerosol is characterized as having been formed by subjecting the solution to ultrasonic sound waves at a frequency of about 20,000 hertz and above.

### Claim 19 (depends on 1)

The coated substrate of claim 1 wherein the aerosol is characterized as having been formed by subjecting the solution to ultrasonic sound waves at a substantially atmospheric pressure of at least about 600 millimeters of mercury.

### Claim 20

A method for providing a coated substrate, comprising the steps of:
a) providing the substrate having a surface to be coated;
b) providing a solution comprised of a solvent substantially devoid of alcohol and having a ruthenium-containing compound dissolved therein;
c) heating the substrate;
d) subjecting the solution to ultrasonic sound waves thereby causing the solution to form into an aerosol;
e) contacting the heated substrate with the aerosol thereby forming a coating of ultrasonically generated particles of the ruthenium-containing compound on the substrate, wherein the substrate is heated to a first temperature of at least about 100° C. and sufficient to at least partially evaporate the solvent from the substrate; and
f) further heating the ultrasonically coated substrate to a second temperature of at least about 300° C. to cause the ruthenium-containing compound to completely form and adhere to the substrate.

### Claim 21 (depends on 20)

The method of claim 20 wherein the ruthenium-containing compound is a ruthenium-containing oxide or a precursor thereof.

### Claim 22 (depends on 21)

The method of claim 21 wherein the precursor of the ruthenium-containing oxide is selected from the group consisting of a nitrate, a sulfate, a phosphate and a chloride.

### Claim 23 (depends on 21)

The method of claim 21 including providing the precursor as either ruthenium nitrosyl nitrate or ruthenium chloride.

### Claim 24 (depends on 20)

The method of claim 20 including providing a majority of the particles having diameters of less than about 10 microns.

### Claim 25 (depends on 20)

The method of claim 20 including providing an internal surface area of the coating of about 10 m2/gram to about 1,500 m2/gram.

### Claim 26 (depends on 20)

The method of claim 20 including providing the coating having a thickness of about a hundred Angstroms to about 0.1 millimeters.

### Claim 27 (depends on 20)

The method of claim 20 including providing a second metal in the solution.

### Claim 28 (depends on 27)

The method of claim 27 including selecting the second metal from the group consisting of tantalum, titanium, nickel, iridium, platinum, palladium, gold, silver, cobalt, molybdenum, ruthenium, manganese, tungsten, iron, zirconium, hafnium, rhodium, vanadium, osmium, niobium, and mixtures thereof.

### Claim 29 (depends on 20)

The method of claim 20 including providing a second metal in the solution and wherein the solution includes a mixture of ruthenium and tantalum.

### Claim 30 (depends on 20)

The method of claim 20 including selecting the substrate from the group consisting of tantalum, titanium, nickel, molybdenum, niobium, cobalt, stainless steel, tungsten, platinum, palladium, gold, silver, copper, chromium, vanadium, aluminum, zirconium, hafnium, zinc, iron, and mixtures thereof.

### Claim 31 (depends on 20)

The method of claim 20 including increasing the surface area of the substrate prior to contacting the aerosol.

### Claim 32 (depends on 19)

The method of claim 19 including increasing the substrate surface area by contacting the substrate with an acid.

### Claim 33 (depends on 31)

The method of claim 31 including increasing the substrate surface area by a mechanical process selected from the group consisting of rough threading, grit blasting, scraping, plasma etching, abrading and wire brushing.

### Claim 34 (depends on 20)

The method of claim 20 including cleaning the substrate by one of the group selected from an aqueous degreasing solution, a non-aqueous degreasing solution and a plasma cleaning process prior to being coated.

### Claim 35 (depends on 20)

The method of claim 20 including increasing the electrical surface conductivity of the substrate prior to contacting the substrate with the aerosol.

### Claim 36 (depends on 20)

The method of claim 20 including providing the substrate having a thickness of about 0.001 to about 2 millimeters.

### Claim 37

A method for providing a coated substrate, comprising the steps of:
a) providing the substrate having a surface to be coated;
b) providing a solution comprised of a solvent substantially devoid of alcohol and having a ruthenium-containing oxide compound or a precursor thereof dissolved therein;
c) heating the substrate to a first temperature of at least about 100° C.;
d) subjecting the solution to ultrasonic sound waves, thereby causing the solution to form into an aerosol;
e) contacting the heated substrate with the aerosol, thereby at least partially evaporating the solvent from the substrate and forming a coating of ultrasonically generated particles of the ruthenium-containing oxide or precursor thereof on the substrate; and
f) further heating the ultrasonically coated substrate to a second temperature of at least about 300° C. to cause the ruthenium-containing oxide compound to completely form and adhere to the substrate or to convert the precursor thereof to the ruthenium-containing oxide compound adhered to the substrate.

### Claim 38

A method for providing a coated substrate, comprising the steps of:
a) providing the substrate having a surface to be coated;
b) providing a solution comprised of a solvent substantially devoid of alcohol and having a ruthenium-containing oxide compound or a precursor thereof dissolved therein;
c) heating the substrate to a first temperature of at least about 100° C.;
d) subjecting the solution to ultrasonic sound waves, thereby causing the solution to form into an aerosol;
e) contacting the heated substrate with the aerosol, thereby at least partially evaporating the solvent from the substrate and beginning forming a coating of ultrasonically generated particles on the substrate; and
f) further heating the ultrasonically coated substrate to at least a second temperature of at least about 300° C. at a rate of about 1° C./minute to about 6° C./minute to cause the ruthenium-containing oxide compound to completely form and adhere to the substrate or to convert the precursor thereof to the ruthenium-containing oxide compound adhered to the substrate.