# US 2001/0024692 A1 · Novel method for the production of a dehumidifying element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024692 A1
- Document ID: US20010024692A1
- Status: Published application
- Kind: A1
- Application number: 09/794,908
- Filed: 2001-02-28
- Published: 2001-09-27
- Earliest claimed: 2000-03-01
- Assignees: Proflute AB
- Inventors: Per-Johan Aronson
- Web page: https://patentgrep.com/patent/US20010024692A1

## CPC

- B01J 20/10: comprising silica or silicate
- B01D 53/28: Selection of materials for use as drying agents
- B01J 20/0248: {Compounds of B, Al, Ga, In, Tl (B01J20/08 takes precedence)}
- B01J 20/0281: {Sulfates of compounds other than those provided for in B01J20/045}
- B01J 20/0292: {Phosphates of compounds other than those provided for in B01J20/048}
- B01J 20/0296: {Nitrates of compounds other than those provided for in B01J20/04}
- B01J 20/045: {containing sulfur, e.g. sulfates, thiosulfates, gypsum}
- B01J 20/046: {containing halogens, e.g. halides}
- B01J 20/18: Synthetic zeolitic molecular sieves
- B01J 20/28038: {Membranes or mats made from fibers or filaments}
- B01J 20/3204: {Inorganic carriers, supports or substrates}
- B01J 20/3206: {Organic carriers, supports or substrates}
- B01J 20/3225: {involving a post-treatment of the coated or impregnated product}
- B01J 20/3234: {Inorganic material layers}
- B01J 20/3236: {containing metal, other than zeolites, e.g. oxides, hydroxides, sulphides or salts}
- B01J 20/3238: {containing any type of zeolite}
- D21H 17/66: Salts, e.g. alums
- B01J 2220/46: Materials comprising a mixture of inorganic and organic materials (materials coated or impregnated on a carrier B01J20/32)
- B01J 2220/4831: having been subjected to further processing, e.g. paper, cellulose pulp
- D21H 27/40: at least one of the sheets being non-planar, e.g. crêped (crêping or corrugating paper B31F)
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B01D: SEPARATION (separating solids from solids by wet methods B03B, B03D; by pneumatic jigs or tables B03B; by other dry methods B07; magnetic or electrostatic separation of solid materials from solid materials or fluids, separation by high-voltage electric fields B03C; centrifuges, vortex apparatus B04; presses per se for squeezing-out liquid from liquid-containing material B30B9/02; treatment of water C02F, e.g. softening by ion-exchange C02F1/42; {arrangements of air intake cleaners in gas turbine plants F02C7/05} ; arrangements or mounting of filters in air-conditioning, air-humidification or ventilation F24F13/28)
- D21H: PULP COMPOSITIONS; PREPARATION THEREOF NOT COVERED BY SUBCLASSES D21C OR D21D; IMPREGNATING OR COATING OF PAPER; TREATMENT OF FINISHED PAPER NOT COVERED BY CLASS B31 OR SUBCLASS D21G; PAPER NOT OTHERWISE PROVIDED FOR

## Abstract

The present invention relates to a method of impregnating paper with a suspension of a molecular sieve in waterglass, such as soda waterglass or potassium waterglass, wherein the impregnated paper can be used as a dehumidifying element, and wherein the method comprises the steps of a) providing a piece of paper, such as facing paper and/or fluted paper; b) immersing the paper into a highly concentrated waterglass solution in which a molecular sieve has been suspended, at a temperature in the range of 45-95° C., wherein said suspension of highly concentrated waterglass/molecular sieve has a viscosity of at least 350 mPa.s at a temperature of 45° C.; and c) cooling the immersed paper with air at a temperature of at most 35° C. and preferably at most 25° C.

## Claims

### Claim 1

A method of impregnating paper with waterglass, such as soda waterglass or potassium waterglass wherein the impregnated paper can be used as a dehumidifying element, and wherein the method comprises the steps of
a) providing a piece of paper, such as facing paper and/or fluted paper;
b) immersing the paper into a highly concentrated waterglass solution in which a molecular sieve has been suspended, at a temperature in the range of 45-95° C., wherein said suspension of highly concentrated waterglass/molecular sieve has a viscosity of at least 350 mPa.s at a temperature of 45° C.; and
c) cooling the immersed paper with air at a temperature of at most 35° C. and preferably at most 25° C.

### Claim 2 (depends on 1)

A method according to claim 1, characterised in that the suspension includes 5-40 kg molecular sieve suspended in 100 kg highly concentrated waterglass.

### Claim 3 (depends on 1, 2)

A method according to claim 1 or claim 2, characterised in that the highly concentrated waterglass solution has a viscosity of at most 800 mPa.s at a temperature of 95° C.

### Claim 4 (depends on 1, 2, 3)

A method according to any one of claims 1-3, characterised in that the waterglass is a soda waterglass.

### Claim 5 (depends on 4)

A method according to claim 4, characterised in that the SiO2/Na2O mole ratio in the soda waterglass is 3.2-3.5.

### Claim 6 (depends on 5)

A method according to claim 5, characterised in that the SiO2/Na2O mole ratio in the soda waterglass is 3.3-3.4.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6)

A method according to any one of claims 1-6, characterised in that the paper is produced from inorganic fibres, such as ceramic fibres, glass fibres, slag fibres, carbon fibres or mineral fibres, with an admixture of 0-20% cellulose fibres or syntethic fibres.

### Claim 8 (depends on 7)

A method according to claim 7, characterised in that the weight of the paper is 20-50 g/m2.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

A method according to any one of claims 1-8, characterised by immersing the paper after step c) in an aqueous solution of a metal salt, such as aluminium sulphate, magnesium sulphate, primary aluminium phosphate (Al2O3. IP2O5), magnesium chloride or aluminium nitrate, and an acid, such as sulphuric acid, phosphoric acid, hydrochloric acid or nitric acid.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

A method according to any one of claims 1-8, characterised by placing the paper in a carbon dioxide atmosphere after step c).

### Claim 11

The use of a suspension of highly concentrated waterglass and a molecular sieve to impregnate paper in conjunction with the manufacture of a dehumidifying element, wherein said suspension has a viscosity of at least 350 mPa.s at a temperature of 45° C.

### Claim 12 (depends on 11)

The use according to claim 11, characterised in that the suspension has a viscosity of at most 800 mPa.s at a temperature of 95° C.