# US 2001/0024684 A1 · Process for producing antireflection coatings

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024684 A1
- Document ID: US20010024684A1
- Status: Published application
- Kind: A1
- Application number: 09/739,245
- Filed: 2000-12-19
- Published: 2001-09-27
- Earliest claimed: 1998-06-30
- Assignees: Universität Konstanz
- Inventors: Ullrich Steiner; Stefan Walheim; Erik Schaffer; Stefan Eggert; Jurgen Mlynek
- Web page: https://patentgrep.com/patent/US20010024684A1

## CPC

- G02B 1/111: using layers comprising organic materials
- C03C 17/007: {containing a dispersed phase, e.g. particles, fibres or flakes, in a continuous phase}
- C03C 17/32: with synthetic or natural resins (C03C17/30 takes precedence)
- C03C 17/3405: {with at least two coatings of organic materials (C03C17/36, C03C17/42 take precedence)}
- C03C 2217/425: consisting of a porous layer
- C03C 2217/732: made of a single layer
- C03C 2217/77: Coatings having a rough surface
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

The invention relates to a method for producing an element comprising a substrate and at least one anti-reflection coating with pores. The dimensions of the anti-reflection coating are below the wavelength of visible light or the neighbouring spectral ranges. The invention also relates to an element produced according to this method with at least one anti-reflection coating, for example optical lenses, mirrors or other optical components. The optical anti-reflection coating of these elements is essentially improved.

## Claims

### Claim 1

Process for producing an element comprising a substrate and at least one antireflection coating having pores, the dimensions of the antireflection coating being below the wavelength of visible light or neighboring spectral regions, comprising the steps
preparing a substrate,
applying a solution of at least two mutually incompatible polymers which are dissolved in a common solvent in such a manner that a common intermixed phase is produced, to a substrate, phase separation on its surface producing a coating having essentially laterally alternating polymer phases, and
exposing this coating to another solvent so that at least one polymer remains undissolved.

### Claim 2 (depends on 1)

Process according to claim 1, in which the antireflection coating is first produced on a carrier substrate from which it is subsequently detached and then transferred to the substrate to be coated.

### Claim 3 (depends on 1, 2)

Process according to claim 1 or 2, the mixture ratio of the polymers being set as a function of the desired refractive index of the antireflection coating.

### Claim 4 (depends on 1, 2, 3)

Process according to one of the claims 1 to 3, in which at least two coatings are produced on different surfaces and the second coating, and if necessary all additional coatings, are subsequently detached from their respective substrates and then superimposed on the first coating.

### Claim 5 (depends on 1, 2, 3)

Process according to one of the claims 1 to 3, in which a first coating is produced, a second coating is subsequently applied directly to the first coating and the multicoating thus produced is subsequently exposed to a solvent which selectively dissolves at least one of the polymers.

### Claim 6 (depends on 5)

Process according to claim 5, in which this process is repeated several times in such a manner that the solvent of the coating to be produced does not dissolve at least one of the polymers of the subjacent coating(s).

### Claim 7 (depends on 1, 2, 3)

Process according to one of the claims 1 to 3, in which the coating is exposed to a selective solvent only briefly so that no polymer components are completely removed to obtain an antireflection gradient coating.

### Claim 8 (depends on 7)

Process according to claim 7, the percent by volume of the dissolved-out pores being a function of the distance from the coating surface, so that the coating produced in such a manner has a gradient of the refractive index, so that the refractive index gradually changes from the refractive index of the first medium to that of the second medium.

### Claim 9

Process according to one or more of the preceding claims, in which a single or multiple coating is first produced, one or more phases are subsequently dissolved out by suitable solvents and then exposed to an etching solution for so long a time that pores having a suitable depth are produced on the substrate at the sites not covered by the polymer(s).

### Claim 10

Process according to one or more of the preceding claims, in which a single or multiple coating is first produced, one or more phases are subsequently dissolved out by suitable solvents, then exposed to a suitable solution of precursor molecules, and a sol-gel procedure is subsequently carried out with the precursor molecules being separated out.

### Claim 11

Process according to one or more of the preceding claims, in which a single or multiple coating is first produced, suitable precursor molecules having already been added to one or more solutions, a sol-gel procedure is then carried out with the precursor molecules being separated out, and one or more of the polymer phases are subsequently removed.

### Claim 12

Process according to one or more of the preceding claims, in which a single or multiple coating is first produced, one or more phases are subsequently dissolved out by suitable solvents and the coating thus obtained is then vapor-plated with a material in such a manner that the pores present in the coating are filled.

### Claim 13 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12)

Element comprising a substrate and at least one antireflection coating having pores, the dimensions of the antireflection coating being below the wavelength of visible light or neighboring spectral ranges, obtainable by the process according to one of the claims 1 to 12.

### Claim 14 (depends on 13)

Element according to claim 13, the refractive index of the antireflection coating being less than 1.3.

### Claim 15 (depends on 13, 14)

Element according to claim 13 or 14 which is an optical lens or a mirror.