# US 2001/0024683 A1 · Methods of forming a face plate assembly of a color display

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024683 A1
- Document ID: US20010024683A1
- Status: Published application
- Kind: A1
- Application number: 09/783,272
- Filed: 2001-02-12
- Published: 2001-09-27
- Earliest claimed: 1998-06-11
- Assignees: Micron Technology, Inc.
- Inventors: Jefferson O. Nemelka
- Web page: https://patentgrep.com/patent/US20010024683A1

## CPC

- C23C 26/00: Coating not provided for in groups C23C2/00 - C23C24/00
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

Methods of forming face plate assemblies are described. In one implementation, a substrate is patterned with photoresist and a first phosphor-comprising material is formed over first surface areas of the substrate. The photoresist is stripped leaving some of the first phosphor-comprising material over substrate areas other than the first areas. Photoresist is again formed over the substrate and processed to expose second substrate areas which are different from the first substrate areas. In a preferred aspect, processing the photoresist comprises using a heated aqueous developing solution comprising an acid, e.g. lactic acid, effective to dislodge and remove first phosphor-comprising material from beneath the developed photoresist. A second phosphor-comprising material is formed over the substrate and the exposed second areas, with trace deposits being left over other substrate areas. The photoresist is subsequently stripped leaving some of the second phosphor-comprising material over substrate areas other than the first and second areas. Photoresist is again formed over the substrate and processed to expose third substrate areas which are different from the first and second areas. In a preferred aspect, processing the photoresist comprises using a heated aqueous developing solution comprising an acid, e.g. lactic acid, effective to dislodge and remove first and second phosphor-comprising material from beneath the removed photoresist. A third phosphor-comprising material is formed over the substrate and the exposed third areas.

## Claims

### Claim 1

A method of forming a face plate assembly of a color display comprising:
forming a phosphor-comprising material over a surface of the face plate;
forming photoresist over the phosphor comprising material; and
removing photoresist from over portions of the face plate surface with a heated aqueous developing solution effective to also remove phosphor-comprising material from the substrate beneath said removed photoresist during said removing.

### Claim 2 (depends on 1)

The method of claim 1, wherein said developing solution comprises an inorganic acid.

### Claim 3 (depends on 2)

The method of claim 2, wherein said inorganic acid comprises phosphoric acid.

### Claim 4 (depends on 2)

The method of claim 2, wherein said inorganic acid comprises hydrochloric acid.

### Claim 5 (depends on 1)

The method of claim 1, wherein said developing solution comprises an organic acid.

### Claim 6 (depends on 5)

The method of claim 5, wherein said organic acid comprises lactic acid.

### Claim 7 (depends on 5)

The method of claim 5, wherein said organic acid comprises acetic acid.

### Claim 8 (depends on 5)

The method of claim 5, wherein said organic acid comprises glycolic acid.

### Claim 9 (depends on 5)

The method of claim 5, wherein said developing solution has a concentration of said organic acid of less than about ten percent by volume.

### Claim 10 (depends on 9)

The method of claim 9, wherein said developing solution is heated to a temperature from between about 25° C. to 50° C.

### Claim 11 (depends on 9)

The method of claim 9, wherein said developing solution is heated to a temperature from between about 35° C. to 40° C.

### Claim 12 (depends on 5)

The method of claim 5, wherein said developing solution has a concentration of said organic acid of less than about one percent by volume.

### Claim 13 (depends on 12)

The method of claim 12, wherein said organic acid comprises lactic acid.

### Claim 14 (depends on 1)

The method of claim 1 further comprising:
after said developing, forming a second phosphor-comprising material over said surface;
forming photoresist over said face plate surface;
second developing said photoresist from over different portions of the face plate surface with a developing solution effective to also remove first and second phosphor-comprising material from the substrate beneath said removed photoresist during said second developing; and
forming a third phosphor-comprising material over said different portions of the face plate surface.

### Claim 15 (depends on 14)

The method of claim 14, wherein said developing and said second developing comprise using developing solutions comprising an organic acid.

### Claim 16

A method of forming a face plate assembly of a color display comprising:
forming a phosphor-comprising material over a substrate comprising a portion of a face plate assembly of a color display, the material being formed over first substrate areas and second substrate areas; and
after said forming, exposing the substrate to an aqueous solution comprising phosphor-removing material effective to remove phosphor-comprising material from over said second areas and outwardly expose said second areas.

### Claim 17 (depends on 16)

The method of claim 16 further comprising:
prior to said forming of said phosphor-comprising material, forming photoresist over the substrate, said photoresist defining areas within which said phosphor-comprising material is to be formed; and
prior to said exposing of the substrate to said aqueous solution, removing photoresist from over the substrate with a photoresist developing solution.

### Claim 18 (depends on 16)

The method of claim 16, wherein said phosphor-removing material comprises an inorganic acid.

### Claim 19 (depends on 16)

The method of claim 16, wherein said phosphor-removing material comprises an organic acid.

### Claim 20 (depends on 19)

The method of claim 19, wherein said aqueous solution is heated to a temperature from between about 25° C. to 50° C.

### Claim 21 (depends on 19)

The method of claim 19, wherein said aqueous solution comprises less than about ten percent of said organic acid by volume.

### Claim 22 (depends on 16)

The method of claim 16, wherein said phosphor-removing material comprises lactic acid.

### Claim 23 (depends on 22)

The method of claim 22, wherein said aqueous solution comprises less than about ten percent of said lactic acid by volume.

### Claim 24 (depends on 16)

The method of claim 16 further comprising:
after said exposing, forming a second phosphor-comprising material over said second areas;
exposing said substrate to an aqueous solution comprising a phosphor-removing material effective to remove first and second phosphor-comprising materials from over and outwardly expose third substrate areas which are different from said first and second substrate areas; and
forming a third phosphor-comprising material over the exposed third substrate areas.

### Claim 25

A method of forming a face plate assembly of a color display comprising:
providing a substrate comprising a portion of a face plate assembly of a color display and having a patterned masking layer thereover defining a plurality of openings over first substrate areas;
forming a phosphor-comprising material over the first substrate areas; and
after forming the phosphor-comprising material, exposing the substrate to an aqueous solution comprising phosphor-removing material effective to remove phosphor-comprising material from over and outwardly expose second substrate areas which are different from the first substrate areas.

### Claim 26 (depends on 25)

The method of claim 25, wherein said aqueous solution is heated to a temperature from between about 25° C. to 50° C.

### Claim 27 (depends on 25)

The method of claim 25, wherein said aqueous solution comprises less than about ten percent of an organic acid by volume.

### Claim 28 (depends on 27)

The method of claim 27, wherein said organic acid comprises lactic acid.

### Claim 29 (depends on 25)

The method of claim 25 further comprising prior to exposing said substrate to said aqueous solution, forming a second masking layer over said substrate, wherein said aqueous solution is effective to remove portions of said second masking layer from over said second substrate areas.

### Claim 30 (depends on 29)

The method of claim 29, wherein said second masking layer comprises negative photoresist and further comprising prior to said exposing, light processing photoresist other than those portions which are removed from over said second substrate areas.

### Claim 31 (depends on 29)

The method of claim 29, wherein said aqueous solution comprises less than about ten percent of an organic acid by volume.

### Claim 32 (depends on 29)

The method of claim 29 further comprising forming a second phosphor-comprising material over said second substrate areas and thereafter, exposing said substrate to an aqueous solution comprising phosphor-removing material effective to remove second phosphor-comprising material from over and outwardly expose third substrate areas which are different from the second substrate areas.

### Claim 33 (depends on 32)

The method of claim 32 further comprising:
prior to exposing said third substrate areas, forming a third masking layer over said substrate;
wherein said aqueous solution which is effective to remove second phosphor-comprising material is also effective to remove portions of said third masking layer from over said third substrate areas; and
after said exposing of said third substrate areas, forming a third phosphor-comprising material over said third substrate areas.

### Claim 34

A method of forming a face plate assembly of a color display comprising:
forming a matrix material over a surface of a face plate, said matrix material defining a plurality of areas over which phosphor-comprising material is to be formed;
forming a phosphor-comprising material over the face plate within one of said areas;
forming photoresist over the matrix material and the phosphor-comprising material;
exposing selected portions of the photoresist to radiant energy;
developing unexposed portions of the photoresist with a developing solution effective to remove said unexposed portions from over areas which are different from said one area;
after said developing, treating said different areas with a heated aqueous solution comprising a phosphor-removing material effective to remove trace deposits of said phosphor-comprising material within said different areas.

### Claim 35 (depends on 34)

The method of claim 34, wherein said heated aqueous solution comprises an acid having a concentration less than about ten percent by volume.

### Claim 36 (depends on 35)

The method of claim 35, wherein said acid comprises an organic acid.

### Claim 37 (depends on 35)

The method of claim 35, wherein said acid comprises an inorganic acid.

### Claim 38

A method of forming a face plate assembly of a color display comprising:
electrophoretically depositing a first phosphor-comprising material on first portions of a surface of a face plate, at least some of said first phosphor-comprising material forming on second portions of said surface;
forming photoresist over the first phosphor-comprising material received on the first and second portions of said surface;
light processing the photoresist on the first and second portions differently;
after said light processing, stripping photoresist from over the second portions of the face plate surface with a stripping solution effective to also remove first phosphor-comprising material from the substrate beneath said stripped photoresist during said stripping; and
after the stripping, electrophoretically depositing a second phosphor comprising material on the second portions of said surface.

### Claim 39 (depends on 38)

The method of claim 38, wherein said stripping solution comprises an aqueous solution comprising an organic acid.

### Claim 40 (depends on 39)

The method of claim 39, wherein said organic acid comprises lactic acid.

### Claim 41 (depends on 39)

The method of claim 39, wherein said organic acid comprises acetic acid.

### Claim 42 (depends on 39)

The method of claim 39, wherein said aqueous solution has a concentration of said organic acid of less than about ten percent by volume.

### Claim 43 (depends on 39)

The method of claim 39, wherein said aqueous solution has a concentration of said organic acid of less than about one percent by volume.

### Claim 44 (depends on 39)

The method of claim 39, further comprising:
after electrophoretically depositing said second phosphor-comprising material, forming photoresist at least over said first portion of said surface;
second light processing said photoresist on said first portion differently;
after said second light processing, second stripping said photoresist from over and outwardly exposing some of said first portion of said surface with a stripping solution effective to also remove first and second phosphor-comprising material from the substrate beneath said stripped photoresist during said second stripping; and
after said second stripping, electrophoretically depositing a third phosphor-comprising material on said exposed first portion.

### Claim 45

A method of forming a face plate assembly of a color display comprising:
forming a first phosphor-comprising material over a surface of the face plate;
forming negative photoresist over the first phosphor-comprising material;
masking first portions of the negative photoresist while leaving second portions exposed;
exposing the second portions to selected light;
after the exposing, removing the mask;
after removing the mask, exposing the negative photoresist to a solution comprising aqueous organic acid effective to strip the non-light-exposed photoresist and first phosphor-comprising material therebeneath from over the face plate surface; and
after stripping the non-light exposed photoresist and first phosphor-comprising material therebeneath, forming second phosphor-comprising material at least over the surface of the face plate from which the non-light-exposed photoresist and first phosphor-comprising material was stripped.

### Claim 46 (depends on 45)

The method of claim 45, wherein said organic acid comprises lactic acid.

### Claim 47 (depends on 45)

The method of claim 45, wherein said organic acid comprises lactic acid having a concentration of less than about ten percent by volume.

### Claim 48

A method of forming a face plate assembly of a color display comprising:
providing a substrate having a first patterned masking layer defining a first plurality of openings over first substrate areas, the substrate comprising a portion of a face plate assembly of a color display;
forming a first phosphor-comprising material over the first substrate areas;
removing the first patterned masking layer;
forming a second patterned masking layer over the substrate defining a second plurality of openings over second substrate areas which are different from the first substrate areas, said forming of the second patterned masking layer comprising exposing the substrate to a phosphor-removing solution which is effective to remove at least some of any remnant first phosphor-comprising material from within the second openings over said second substrate areas; and
forming a second phosphor-comprising material over the second substrate areas.

### Claim 49 (depends on 48)

The method of claim 48, wherein said phosphor-removing solution comprises an aqueous organic acid solution.

### Claim 50 (depends on 49)

The method of claim 49, wherein said solution comprises a concentration of less than about ten percent lactic acid by volume.

### Claim 51 (depends on 48)

The method of claim 48 further comprising:
forming a third patterned masking layer over the substrate defining a third plurality of openings over third substrate areas which are different from said second substrate areas, said forming of said third patterned masking layer comprising exposing said substrate to a phosphor-removing solution which is effective to remove at least some of any remnant first and second phosphor-comprising materials from within the third openings over said third substrate areas; and
forming a third phosphor-comprising material over said third substrate areas.

### Claim 52 (depends on 51)

The method of claim 51, wherein both of said phosphor-removing solutions comprise aqueous organic acid solutions having a concentration of less than about ten percent organic acid by volume.

### Claim 53 (depends on 52)

The method of claim 52, wherein the organic acid in one of said solutions comprises lactic acid.

### Claim 54

A method of forming a face plate assembly of a color display comprising:
providing a substrate having a first patterned masking layer defining a first plurality of openings over first substrate areas, the substrate comprising a portion of a face plate assembly of a color display and comprising second substrate areas;
forming a first phosphor-comprising material within the first openings over the first substrate areas and over the first patterned masking layer over the second substrate areas;
removing the first patterned masking layer and leaving some first phosphor-comprising material over the substrate in the second substrate areas;
forming a second patterned masking layer comprising photoresist over the substrate leaving a second plurality of openings over the second substrate areas, said forming of the second patterned masking layer comprising exposing the substrate to a photoresist-developing solution which is effective to substantially remove second masking layer material and the first phosphor-comprising material from over said second substrate areas; and
forming a second phosphor-comprising material over the second substrate areas.

### Claim 55 (depends on 54)

The method of claim 54, wherein said photoresist-developing solution comprises an aqueous organic acid solution.

### Claim 56 (depends on 55)

The method of claim 55, wherein said photoresist-developing solution comprises a concentration of less than about ten percent lactic acid by volume.

### Claim 57 (depends on 55)

The method of claim 55, wherein said photoresist-developing solution comprises a concentration of less than about ten percent acetic acid by volume.

### Claim 58 (depends on 54)

The method of claim 54 further comprising:
removing said second patterned masking layer and leaving some second phosphor-comprising material over the substrate in third substrate areas;
forming a third patterned masking layer comprising photoresist over said substrate leaving a third plurality of openings over said third substrate areas, said forming of said third patterned masking layer comprising exposing the substrate to a photoresist-developing solution which is effective to substantially remove third masking layer material and first and second phosphor-comprising material from over said third substrate areas; and
forming a third phosphor-comprising material within said third openings over said third substrate areas.

### Claim 59 (depends on 58)

The method of claim 58, wherein both of said developing solutions comprise aqueous organic acid solutions.

### Claim 60 (depends on 59)

The method of claim 59, wherein one of the solutions comprises a concentration of lactic acid of less than about ten percent by volume.