# US 2001/0024634 A1 · Method of producing hydrogen peroxide by direct synthesis and noble-metal catalyst for the method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0024634 A1
- Document ID: US20010024634A1
- Status: Published application
- Kind: A1
- Application number: 09/792,064
- Filed: 2001-02-26
- Published: 2001-09-27
- Earliest claimed: 2000-02-26
- Inventors: Birgit Bertsch-Frank; Ina Hemme; Jurgen Rollmann; Stipan Katusic; Torsten Balduf; Catrin D. Becker; Werner Wildner; Rudiger Schutte
- Web page: https://patentgrep.com/patent/US20010024634A1

## CPC

- C01B 15/029: Preparation from hydrogen and oxygen
- B01J 23/40: of the platinum group metals
- B01J 27/13: Platinum group metals
- B01J 37/22: Halogenating
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

The invention is relative to a method of producing hydrogen peroxide by direct synthesis in which hydrogen and oxygen are reacted in the presence of a heterogeneous, carrier-free or carrier-bound catalyst containing at least one noble metal in the presence or absence of a solvent and to a catalyst for carrying out the method. The use of a halide promoter and/or of a mineral acid can be avoided by using a noble-metal catalyst containing an inorganic iodine compound in an amount corresponding to 0.01 to 15% by weight iodine relative to the noble-metal content.

## Claims

### Claim 1

A method of producing hydrogen peroxide by direct synthesis comprising:
reacting hydrogen and oxygen in the presence of a heterogeneous, carrier-free or carrier-bound catalyst containing at least one noble-metal and at least one inorganic iodine compound in the presence or absence of a solvent, wherein the amount of iodine content in said catalyst is in a range of 0.01 to 15% by weight based on the weight of said noble-metal.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said noble-metal is selected from the group consisting of platinum, silver, gold, palladium and mixtures thereof.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the catalyst comprises alloyed or unalloyed forms of said noble-metal.

### Claim 4 (depends on 1)

The method according to claim 1, wherein said catalyst comprises palladium iodide or platinum iodide.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the catalyst is produced by a spray or flame pyrolysis method comprising;
(i) producing a gas-carried particle stream containing at least one noble-metal and at least one iodine compound in the particles,
(ii) pyrolyzing said particle stream in a spray or flame pyrolysis reactor at a temperature of 500 to 1500° C.,
(iii) separating solid particles formed during step (ii) and, optionally,
(iv) impregnating a catalytic carrier with said solid particles.

### Claim 6 (depends on 5)

The method according to claim 5, wherein said particle stream comprises particles containing palladium iodide, platinum iodide or mixtures thereof.

### Claim 7 (depends on 6)

The method according to claim 6, wherein said particle stream further comprises at least one precursor for forming an oxide or silicate catalytic carrier.

### Claim 8 (depends on 1)

The method according to claim 1, wherein said carrier-free or carrier-bound catalyst further comprises relative to carrier-free catalytic particles:
at least 80% by weight palladium,
0 to 15% by weight gold,
0 to 15% platinum,
0 to 5% by weight silver, and
at least one noble-metal iodide, wherein said noble-metal is selected from the group consisting of Pd, Pt, Au and Ag, and wherein said iodine content catalyst is 0.1 to 10% by weight based on the weight of the noble-metal content.

### Claim 9 (depends on 1)

The method according to claim 1, wherein said direct synthesis is conducted in a trickle-bed reactor wherein an aqueous solution containing a stabilizer for hydrogen peroxide trickles over a catalytic fixed bed.

### Claim 10

A carrier-free or carrier-bound noble-metal catalyst, comprising at least one noble metal and at least one inorganic iodine compound, wherein the amount of iodine content in said catalyst is in a range of 0.01 to 15% by weight based on the weight of said noble-metal.

### Claim 11 (depends on 10)

The noble-metal catalyst according to claim 10, wherein said noble-metal catalyst is selected from a group consisting of platinum, silver, gold, palladium and mixtures thereof.

### Claim 12 (depends on 10)

The noble-metal catalyst according to claim 10, wherein said noble-metal catalyst comprises noble-metal iodide.

### Claim 13 (depends on 12)

The noble-metal catalyst according to claim 12, wherein said noble metal iodide is palladium iodide or platinum iodide.

### Claim 14 (depends on 10)

The noble-metal catalyst according to claim 10, wherein said noble-metal catalyst is obtained by spray or flame pyrolysis method comprising:
(i) producing a gas-carried particle stream containing at least one noble-metal and at least one iodine compound in the particles;
(ii) pyrolyzing said particle stream in a spray or flame pyrolysis reactor at a temperature of 500 to 1500° C.,
(iii) separating solid particles formed during step (ii), and, optionally,
(iv) impregnating a catalytic carrier with said solid particles.

### Claim 15 (depends on 10)

The noble-metal catalyst according to claim 10, wherein said noble-metal catalyst comprises relative to carrier-free particles:
at least 80% by weight palladium,
0 to 15% by weight gold,
0 to 15% platinum,
0 to 5% by weight silver, and
at least one noble-metal iodide, wherein said noble-metal is selected from the group consisting of Pd, Pt, Au and Ag, and wherein said iodine content in said catalyst is 0.1 to 10% by weight based on the weight of the noble-metal content.

### Claim 16 (depends on 14)

The noble-metal catalyst according to claim 14, wherein in step (i), an aqueous or aqueous-organic solution of at least noble-metal compound, at least one iodine compound and, optionally, at least one precursor of an oxidic or silicatic carrier material are sprayed to produce an extremely fine aerosol and, optionally, said formed aerosol is pre-dried.

### Claim 17 (depends on 14)

The carrier-bound noble-metal catalyst according to claim 14, wherein said separated solid particles formed in step (ii) are impregnated into a porous oxide, silicate or activated-carbon carrier material.

### Claim 18 (depends on 1)

The method according to claim 1, wherein said catalyst to be used is produced by a method comprising:
contacting said noble-metal catalyst with an aqueous solution of an alkali-metal iodide or noble-metal iodide at 20 to 90° C., wherein at least part of the iodide is bound to said noble-metal catalyst and
removing free iodide by washing non-bound iodide out.

### Claim 19 (depends on 1)

A carrier-free or carrier-bound noble-metal catalyst, comprising an inorganic iodine compound wherein the iodine content in said catalyst is 001 to 15% by weight is used based on the weight of said noble-metal obtained by the method according to claim 1.