- Web page: https://patentgrep.com/patent/US20010024081A1

## CPC

- H01J 9/04: of thermionic cathodes
- H01J 1/142: with alkaline-earth metal oxides, or such oxides used in conjunction with reducing agents, as an emissive material
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A cathode for an electron tube and a preparing method therefor are provided. In the cathode for an electron tube having a base metal and an electron-emitting material layer, the particle size of the micro structure of the surface of the base metal is controlled to be in the range of 3 to 50 μm. The cathode for an electron tube has an excellent effect of diffusing intermediate products generated during the operation of the cathode, and is capable of consistently supplying a diffusion path of a reducing agent. Also, the cut off drift rate can be reduced, thereby attaining a long life span characteristic.

## Claims

### Claim 1

A cathode for an electron tube having a base metal and an electron-emitting material layer, wherein the particle size of the micro structure of the surface of the base metal is controlled to be in the range of 3 to 50 μm.

### Claim 2 (depends on 1)

The cathode according to claim 1, wherein the particle size of the micro structure of the surface the base metal is controlled by thermal treatment.

### Claim 3 (depends on 2)

The cathode according to claim 2, wherein the thermal treatment is performed by the steps of:
(a) an oxidative thermal treatment step of heating a base metal at a temperature of 300 to 1100° C. under the atmosphere to form a metal oxide layer;
(b) a dry reducing thermal treatment step of heating the base metal having the metal oxide layer at a temperature of 500 to 1200° C. under a hydrogen atmosphere in which a dew point is kept at −50 to −90° C., to remove the metal oxide layer; and
(c) a wet reducing thermal treatment step of heating the base metal treated with the step (b) at a temperature of 500 to 1200° C. under a hydrogen atmosphere in which a dew point is kept at −10 to −40° C.

### Claim 4 (depends on 3)

The cathode according to claim 3, wherein the oxidative thermal treatment step is maintained at the uppermost temperature for 3 to 60 minutes.

### Claim 5 (depends on 3)

The cathode according to claim 3, wherein the dry reducing thermal treatment step is maintained at the uppermost temperature for 3 to 60 minutes.

### Claim 6 (depends on 3)

The cathode according to claim 3, wherein the wet reducing thermal treatment step is maintained at the uppermost temperature for 3 to 60 minutes.

### Claim 7

A method for preparing a cathode for an electron tube, comprising the steps of:
(a) an oxidative thermal treatment step of heating a base metal at a temperature of 300 to 1100° C. under the atmosphere to form a metal oxide layer;
(b) a dry reducing thermal treatment step of heating the base metal having the metal oxide layer at a temperature of 500 to 1200° C. under a hydrogen atmosphere in which a dew point is kept at −50 to −90° C., to remove the metal oxide layer; and
(c) a wet reducing thermal treatment step of heating the base metal treated with the step (b) at a temperature of 500 to 1200° C. under a hydrogen atmosphere in which a dew point is kept at −10 to −40° C.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the oxidative thermal treatment step is maintained at the uppermost temperature for 3 to 60 minutes.

### Claim 9 (depends on 7)

The method according to claim 7, wherein the dry reducing thermal treatment step is maintained at the uppermost temperature for 3 to 60 minutes.

### Claim 10 (depends on 7)

The method according to claim 7, wherein the wet reducing thermal treatment step is maintained at the uppermost temperature for 3 to 60 minutes.