# US 2001/0023989 A1 · Semiconductor dielectric structure and method for making the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023989 A1
- Document ID: US20010023989A1
- Status: Published application
- Kind: A1
- Application number: 09/864,441
- Filed: 2001-05-23
- Published: 2001-09-27
- Earliest claimed: 1999-06-25
- Assignees: Philips Electronics North America Corporation
- Inventors: Rao V. Annapragada; Milind G. Weling
- Web page: https://patentgrep.com/patent/US20010023989A1

## CPC

- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 14/6532: {by exposure to a plasma}
- H10P 14/6682: {the compound being a silane, e.g. disilane, methylsilane or chlorosilane}
- H10W 20/071: {of dielectric parts thereof}
- H10W 20/092: {by smoothing the dielectric parts}
- H10W 20/098: {by filling between adjacent conductive parts}
- H10P 14/6336: {in the presence of a plasma [PECVD]}
- H10P 50/283: {by chemical means}
- H10W 20/48: Insulating materials thereof
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method for fabricating inter-metal oxide in semiconductor devices and semiconductor devices is provided. The method begins by providing a semiconductor substrate having a plurality of patterned conductive features. The method then moves to where a high density plasma (HDP) operation is performed and is configured to deposit an oxide layer over the plurality of patterned conductive features. The HDP operation includes a deposition component and a sputtering component. The deposition component is driven by a deposition gas and the sputtering component is driven by a sputtering gas. The HDP operation forms oxide pyramids over the plurality of patterned conductive features. The method now moves to where the deposition gas is removed to close off the deposition component in the HDP operation. Now, the HDP operation is run with the sputtering gas while retaining the sputtering component. The sputtering component is configured to substantially remove the oxide pyramids from over the plurality of patterned conductive features. Preferably, the plurality of patterned conductive features are either patterned metallization features or patterned polysilicon features.

## Claims

### Claim 1

A method for fabricating inter-metal oxide in semiconductor devices, comprising:
providing a semiconductor substrate having a plurality of patterned conductive features;
performing a high density plasma (HDP) operation that is configured to deposit an oxide layer over the plurality of patterned conductive features, the HDP operation includes a deposition component and a sputtering component, the deposition component is driven by a deposition gas and the sputtering component is driven by a sputtering gas, the HDP operation forms oxide pyramids over the plurality of patterned conductive features;
closing the deposition gas to remove the deposition component from the HDP operation; and
running the HDP operation with the sputtering gas to retain the sputtering component, the sputtering component is configured to substantially remove the oxide pyramids from over the plurality of patterned conductive features.

### Claim 2 (depends on 1)

A method for fabricating inter-metal oxide in semiconductor devices as recited in claim 1, wherein the plurality of patterned conductive features are one of patterned metallization features and patterned polysilicon features.

### Claim 3 (depends on 1)

A method for fabricating inter-metal oxide in semiconductor devices as recited in claim 1, wherein the HDP operation is performed in a process chamber.

### Claim 4 (depends on 1)

A method for fabricating inter-metal oxide in semiconductor devices as recited in claim 1, wherein the oxide layer is a silicon dioxide (SiO2) layer.

### Claim 5 (depends on 3)

A method for fabricating inter-metal oxide in semiconductor devices as recited in claim 3, wherein the deposition gas of the deposition component includes a silane gas and an oxygen gas, the method further comprises:
introducing the silane gas into the process chamber at a flow rate of about 75 standard cubic centimeters per minute (sccm); and
introducing the oxygen gas into the process chamber at a flow rate of between about 120 sccm and 180 sccm.

### Claim 6 (depends on 3)

A method for fabricating inter-metal oxide in semiconductor devices as recited in claim 3, wherein the sputtering gas of the sputtering component includes an argon gas, the method further comprising:
introducing the argon gas into the process chamber at a flow rate ranging between about 100 sccm and about 120 sccm.

### Claim 7 (depends on 6)

A method for fabricating inter-metal oxide in semiconductor devices as recited in claim 6, further comprising:
maintaining a power level for the sputtering component, the maintaining includes, setting a bottom power of the process chamber to range between about 500 watts and about 4,500 watts;
setting a top power of the process chamber to range between about 600 watts and about 2,000 watts; and
setting a side power of the process chamber to range between about 1,000 and about 4,500 watts.

### Claim 8 (depends on 6)

A method for fabricating inter-metal oxide in semiconductor devices as recited in claim 6, further comprising:
maintaining a pressure level for the sputtering component, the maintaining includes,
setting a pressure for the process chamber to range between about 3 mTorr and about 10 mTorr.

### Claim 9 (depends on 1)

A method for fabricating inter-metal oxide in semiconductor devices as recited in claim 1, wherein when the oxide pyramid have a vertical height ranging between about 500 angstroms and about 2,500 angstroms, the method further comprises:
continuing the running of the HDP operation for a period of time ranging between about 10 seconds and about 45 seconds.

### Claim 10 (depends on 1)

A method for fabricating inter-metal oxide in semiconductor devices as recited in claim 1, further comprising:
depositing a PECVD oxide over the oxide layer deposited by the HDP operation after the sputtering component of the HDP operation substantially removes the oxide pyramids from over the plurality of patterned conductive features.

### Claim 11

A semiconductor device, comprising:
a semiconductor substrate having a plurality of patterned conductive features; and
an oxide layer having suppressed oxide pyramids defined over the plurality of patterned conductive features, the oxide layer being defined by a high density plasma (HDP) operation, the HDP operation including a deposition component and a sputtering component, the deposition component being driven by a deposition gas, and the sputtering component being driven by a sputtering gas, the deposition and sputtering components being performed together during a first part of the formation of the oxide layer and the deposition component not being performed during a second part of the formation of the oxide layer.

### Claim 12 (depends on 11)

The semiconductor device of claim 11, wherein the plurality of patterned conductive features are one of patterned metallization features and patterned polysilicon features.

### Claim 13 (depends on 11)

The semiconductor device of claim 11, wherein the oxide layer is a silicon dioxide (SiO2) layer.

### Claim 14 (depends on 11)

The semiconductor device of claim 11, wherein the deposition gas of the deposition component includes a silane gas.

### Claim 15 (depends on 1)

The semiconductor device of claim 1 1, wherein the sputtering gas of the sputtering component includes an argon gas.

### Claim 16 (depends on 11)

The semiconductor device of claim 11, further comprising:
a PECVD oxide layer spread over the oxide layer having the suppressed oxide pyramids that are defined over the plurality of patterned conductive features.

### Claim 17

A method for fabricating inter-metal oxide in semiconductor integrated circuit devices, comprising:
providing a semiconductor substrate having a plurality of patterned conductive features, some of the patterned conductive features defining high aspect ratio gaps;
starting a high density plasma (HDP) operation that is configured to deposit an oxide layer over the plurality of patterned conductive features and in the high aspect ratio gaps, the HDP operation includes a deposition component and a sputtering component, the deposition component is driven by a deposition gas and the sputtering component is driven by a sputtering gas, the HDP operation forms oxide pyramids over the plurality of patterned conductive features;
continuing the HDP operation without the deposition gas to remove the deposition component while retaining the sputtering component; and
completing the HDP operation when the oxide pyramids are substantially smoothed.

### Claim 18 (depends on 17)

A method for fabricating inter-metal oxide in semiconductor integrated circuit devices as recited in claim 17, wherein the plurality of patterned conductive features are one of patterned metallization features and patterned polysilicon features.

### Claim 19 (depends on 17)

A method for fabricating inter-metal oxide in semiconductor integrated circuit devices as recited in claim 17, wherein the HDP operation is performed in a process chamber.

### Claim 20 (depends on 19)

A method for fabricating inter-metal oxide in semiconductor integrated circuit devices as recited in claim 19, wherein the deposition gas of the deposition component includes a silane gas, the method further comprises:
introducing the silane gas into the process chamber at a flow rate of about 75 standard cubic centimeters per minute (sccm); and
introducing the oxygen gas into the process chamber at a flow rate of between about 120 sccm and 180 sccm.

### Claim 21 (depends on 20)

A method for fabricating inter-metal oxide in semiconductor integrated circuit devices as recited in claim 20, wherein the sputtering gas of the sputtering component includes an argon gas, the method further comprising:
introducing the argon gas into the process chamber at a flow rate ranging between about 100 sccm and about 120 sccm.

### Claim 22 (depends on 20)

A method for fabricating inter-metal oxide in semiconductor integrated circuit devices as recited in claim 20, wherein when the oxide pyramid have a vertical height ranging between about 500 angstroms and about 2,500 angstroms.

### Claim 23 (depends on 22)

A method for fabricating inter-metal oxide in semiconductor integrated circuit devices as recited in claim 22, wherein the continuing is set for a period of time ranging between about 10 seconds and about 45 seconds.