# US 2001/0023889 A1 · The interconnection of aluminium components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023889 A1
- Document ID: US20010023889A1
- Status: Published application
- Kind: A1
- Application number: 09/808,698
- Filed: 2001-03-14
- Published: 2001-09-27
- Earliest claimed: 2000-03-22
- Assignees: GEA Spiro-Gills Ltd.
- Inventors: Peter Neil Roy Bendall; Steve Robert Williams
- Web page: https://patentgrep.com/patent/US20010023889A1

## CPC

- F28F 21/084: {from aluminium or aluminium alloys}
- B23K 1/0012: {Brazing of heat exchangers}
- B23K 1/19: taking account of the properties of the materials to be soldered
- B23K 1/20: Preliminary treatment of work or areas to be soldered, e.g. in respect of a galvanic coating
- C23C 22/68: using aqueous solutions with pH between 6 and 8
- C23C 22/83: Chemical after-treatment
- F28F 3/025: {the means being corrugated, plate-like elements}
- B23K 35/3605: {Fluorides}
- B23K 2101/14: Heat exchangers
- B23K 2103/10: Aluminium or alloys thereof
- F28F: DETAILS OF HEAT-EXCHANGE AND HEAT-TRANSFER APPARATUS, OF GENERAL APPLICATION (water and air traps, air venting F16)
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A method of interconnecting components (10, 16) of aluminum having a purity of at least 95%, the method comprising brazing the components (10, 16) together and then surface treating the assembled components (10, 16) by subjecting them to a Bohmitting procedure.

## Claims

### Claim 1

A method of interconnecting components of aluminium having a purity of at least 95% comprising brazing the components together and thereafter surface treating assembled components by subjecting them to a Bohmitting procedure.

### Claim 2 (depends on 1)

A method as claimed in claim 1, in which the components are brazed together in a dry oxygen containing atmosphere in the presence of the suitable flux or paste.

### Claim 3 (depends on 1, 2)

A method as claimed in claim 1 or claim 2, in which at least one component is extruded.

### Claim 4 (depends on 2, 3)

A method as claimed in claim 2 or claim 3, in which the atmosphere in which the brazing is carried out is ambient air.

### Claim 5 (depends on 2, 3, 4)

A method as claimed in any of claims 2, 3 or 4, in which the brazing flux is an insoluble flux consisting of potassium tetrafluoraluminate with solid foils or particles of aluminium silicate (AlSi10) powder, or coated core material.

### Claim 6 (depends on 2, 3, 4)

A method as claimed in any of claims 2, 3 or 4, in which the brazing paste includes potassium tetrafluoralumante with a constituent creating a thixotrophic characteristic and aluminium silicate (AlSi) powder.

### Claim 7

A method as claimed in any one of the preceding claims, in which the components allow a brazing temperature in the range 590°-625° C. simultaneously and remain at this temperature for substantially six minutes.

### Claim 8

A method as claimed in any one of the preceding claims, in which the Bohmitting procedure comprises subjecting the components to deionized water at a temperature of about 100° C.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7)

A method as claimed in any one of claims 1 to 7, in which the Bohmitting procedure comprises subjecting the components to wet steam at a temperature of about 150° C.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

A method as claimed in any one of claims 1 to 9, in which the assembled components are further surface treated by a solution of silicate of sodium (Na2Si O4) in water at about 90-10020 C.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

A method as claimed in any one of claims 1 to 9, in which the assembled components are further surface treated by:
a) subjecting them to 10% boracic acid at about 80-100° C. mixed with water or;
b) subjecting them to 5-10% borax at about 80-100° C. mixed with water or;
c) subjecting them to waterglass (Na2Si O4) at about 90-100° C. mixed with water or;
d) subjecting them to a low viscosity resin coating.

### Claim 12

A method as claimed in any one of the preceding claims, in which the Bohmitting procedure is carried out only on the material surface of the conduit.

### Claim 13

A method of interconnecting components substantially as hereinbefore described.

### Claim 14

Any novel subject matter or combination including novel subject matter disclosed herein, whether or not within the scope of or relating to the same invention as any of the preceding claims.