# US 2001/0023859 A1 · Method for the surfae treatment of a tribological coating

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023859 A1
- Document ID: US20010023859A1
- Status: Published application
- Kind: A1
- Application number: 09/849,828
- Filed: 2001-05-07
- Published: 2001-09-27
- Earliest claimed: 1998-09-03
- Assignees: DaimlerChrysler AG
- Inventors: Markus Beck; Tilmann Haug; Patrick Izquierdo; Michael Lahres; Peter Linden; Matthias Merkel; Matthias Merkel; Harald Pfeffinger
- Web page: https://patentgrep.com/patent/US20010023859A1

## CPC

- C23C 4/18: After-treatment
- Y10T 29/49272: with liner, coating, or sleeve
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention relates to a method for the surface working of a tribological coating of a supereutectic aluminum-silicon alloy or an aluminum-silicon composite material with a coating structure, wherein the surface is reworked after the production of the coating. Provision is made according to the invention that the surface is machined dry, without lubricant, in a one-step process, a cutting tool with a cutting material containing diamond being used. This can be followed by an additional working process. Preferably a combination process of dry machining and one-step finish honing or one-step texturing by radiation is provided.

## Claims

### Claim 1

Method for the surface treatment of a tribological coating of a supereutectic aluminum-silicon alloy or an aluminum-silicon composite material with a coating structure, wherein the surface is reworked after the coating is produced, characterized in that the surface is machined dry in a one-step procedure, using a cutting tool with at least one diamond-containing cutting material.

### Claim 2 (depends on 1)

Method according to claim 1, characterized in that a single-edge cutting tool, preferably an indexable insert, is used.

### Claim 3 (depends on 1)

Method according to claim 1, characterized in that a multi-edged tool preferably a cutting spindle provided with a plurality of indexable inserts is used.

### Claim 4

Method according to any one of the foregoing claims, characterized in that a cutting tool with a cutting material of polycrystalline diamond and/or monocrystalline diamond and/or carbide coated with a CVD diamond layer.

### Claim 5

Method according to any one of the foregoing claims, characterized in that after the dry machining hard coating components contained in the coating structure and lying at the machined surface are immediately exposed.

### Claim 6

Method according to any one of the foregoing claims, characterized in that a combination of dry machining and an additional process is used, wherein after the dry machining the surface is finish-honed in a one-step process.

### Claim 7 (depends on 1, 2, 3, 4, 5)

Method according to any one of claims 1 to 5, characterized in that a combination of the dry machining and an additional method is used, wherein after the dry machining the surface is textured in a one-step process by irradiation, by laser for example, especially with radiation grooving.

### Claim 8

Method according to any one of the foregoing claims, characterized in that a cylinder friction surface of a crankcase for a piston machine, coated with the supereutectic aluminum-silicon alloy or the supereutectic aluminum-silicon material, is reworked.

### Claim 9

Method according to any one of the foregoing claims, characterized in that the cylinder friction surface is reworked only in the area of the top dead center and that the hard coating components lying in the cylinder friction surface are exposed only in the area of the top dead center.

### Claim 10

Method according to any one of the foregoing claims, characterized in that the coating to be worked is produced by plasma spraying methods.

### Claim 11

Method according to any one of the foregoing claims, characterized in that the coating to be worked is produced from a substantially copper-free supereutectic aluminum-silicon alloy or a substantially copper-free supereutectic aluminum-silicon composite material, the copper content being less than 1 wt.-%, preferably smaller than 0.1 wt.-% and especially less than 0.01 wt.-%.

### Claim 12

Method according to any one of the foregoing claims, characterized in that to produce the coating to be worked an alloy is used which has a heterogenic coating structure of a primary aluminum solid solution, a coarse to very fine network of eutectic silicon, primary silicon segregations as well as intermetallic phases such as Mg2Si and oxides, the average size of the primary silicon segregations being less than 10 μm and the average size of the oxides being smaller than 5 μm.

### Claim 13

Method according to any one of the foregoing claims, characterized in that to produce the coating to be worked a composite material is used which has a heterogenic coating structure of a primary aluminum solid solution, a coarse to very fine network of eutectic silicon, primary silicon segregations and/or embedded silicon particles and intermetallic phases such as Mg2Si and oxides, the average size of the primary silicon segregations being less than 10 μm and the average size of the oxides being smaller than 5 μm.