# US 2001/0023820 A1 · Method of coating insulative substrates

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023820 A1
- Document ID: US20010023820A1
- Status: Published application
- Kind: A1
- Application number: 09/758,848
- Filed: 2001-01-11
- Published: 2001-09-27
- Earliest claimed: 2000-01-12
- Assignees: D2 In-Line Solutions, LLC
- Inventors: Donald G. Parent
- Web page: https://patentgrep.com/patent/US20010023820A1

## CPC

- C23C 14/205: {by cathodic sputtering}
- C23C 14/541: {Heating or cooling of the substrates}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A system for a method of applying a coating to an insulative substrate. The method includes applying a coating material to the insulative substrate by physical vapor deposition to a predetermined thickness at a rate and for a predetermined time which does not cause thermal damage to the insulative substrate. Then, before thermal damage can occur, moving the partially coated substrate proximate and active cooling station device to drive the temperature of the insulative substrate substantially down. The deposition and cooling steps are then repeated until the desired coating thickness is obtained to avoid thermal damage to the substrate.

## Claims

### Claim 1

A method of applying a coating to an insulative substrate, the method comprising:
applying a coating material to the insulative substrate by physical vapor deposition to a predetermined thickness at a rate and for a predetermined time which does not cause thermal damage to the insulative substrate;
before thermal damage can occur, moving the partially coated substrate proximate and active cooling station device to drive the temperature of the insulative substrate substantially down; and
repeating the above coating and cooling steps until the desired coating thickness is obtained to avoid thermal damage to the substrate.

### Claim 2 (depends on 1)

The method of claim 1 in which the coating material is metal and the same material is applied during all coating steps.

### Claim 3 (depends on 2)

The method of claim 2 in which the metal includes copper, aluminum and alloys of the same.

### Claim 4 (depends on 1)

The method of claim 1 in which the coating material is a polycrystalline substance.

### Claim 5 (depends on 1)

The method of claim 1 in which the substrate is plastic.

### Claim 6 (depends on 5)

The method of claim 5 in which the substrate is between 1-4 mm thick.

### Claim 7 (depends on 1)

The method of claim 1 in which the coating is applied to a total thickness N, there are X coating steps, and, at each coating step, a thickness of N/X is applied.

### Claim 8 (depends on 7)

The method of claim 7 in which N is between 2 to 4 microns and N/X is between ⅛ and ⅝ micron.

### Claim 9 (depends on 1)

The method of claim 1 in which the insulative substrate is the housing of an electronic device.

### Claim 10 (depends on 9)

The method of claim 9 in which the housing is a cellular telephone housing.

### Claim 11 (depends on 1)

The method of claim 1 in which the insulative substrate is a plastic lens.

### Claim 12 (depends on 1)

The method of claim 1 in which physical vapor deposition includes sputtering, cathodic arc deposition, and evaporation techniques.

### Claim 13 (depends on 1)

The method of claim 1 in which cooling includes placing the partially coated substrate proximate a heat sink and subjecting the partially coated substrate to a high conductivity gas.

### Claim 14 (depends on 13)

The method of claim 13 in which the high conductivity gas is helium.

### Claim 15 (depends on 13)

The method of claim 13 in which the heat sink is cooled by a liquid coolant.

### Claim 16 (depends on 1)

The method of claim 1 in which each coating step lasts less than one minute.

### Claim 17 (depends on 1)

The method of claim 1 in which each cooling step lasts less than one minute.

### Claim 18 (depends on 1)

The method of claim 1 in which the time span in which each partial layer of coating material is applied is the same or approximately the same time span for each cooling step.

### Claim 19 (depends on 1)

The method of claim 1 in which the substrate temperature never exceeds 60° C.

### Claim 20 (depends on 1)

The method of claim 1 in which the substrate temperature never exceeds 90° C.

### Claim 21 (depends on 1)

The method of claim 1 in which cooling drives t he temperature of the substrate from between 40-60° C. to between 5-20° C.

### Claim 22

A system for applying a coating to an insulative component, the system comprising:
a vacuum chamber;
at least one physical vapor deposition station arranged to apply a coating material to the insulative component;
at least one cooling station arranged to actively cool the insulative component and drive the temperature of the insulative component substantially down; and
a component handler designed to move the insulative component within the vacuum chamber and programmed to automatically bring the components proximate a physical vapor deposition station until the components are partially coated to a predetermined thickness and then proximate a cooling station before thermal damage can occur to the components and until they are sufficiently cooled and to then switch between physical vapor deposition stations and cooling stations until the desired coating thickness is obtained.

### Claim 23 (depends on 22)

The system of claim 22 in which there are a plurality of physical vapor deposition stations and cooling stations arranged circumferentially with cooling stations positioned between physical vapor deposition stations.

### Claim 24 (depends on 22)

The system of claim 22 in which there are a plurality of physical vapor deposition stations and cooling stations arranged linearly with cooling stations positioned between physical vapor deposition stations.

### Claim 25 (depends on 22)

The system of claim 22 in which the cooling station includes a heat sink in a subchamber and means for filling the subchamber with a high conductivity gas.

### Claim 26 (depends on 25)

The system of claim 25 in which the components include a cavity and the heat sink is shaped to fit within the cavity.

### Claim 27 (depends on 22)

The system of claim 22 in which the programming of the component handler includes logic which limits the partial coating time to less than one minute and the cooling time to less than one minute.

### Claim 28 (depends on 22)

The system of claim 22 in which the time span of partial cooling is the same as or approximately the time span of cooling.

### Claim 29 (depends on 22)

The system of claim 22 in which the components handler includes trays for holding a plurality of components.

### Claim 30 (depends on 29)

The system of claim 29 in which each cooling station includes one heat sink for each tray.

### Claim 31 (depends on 30)

The system of claim 30 in which each cooling station further includes a subchamber containing all the heat sinks and means for filling the subchamber with a high conductivity gas.