# US 2001/0023754 A1 · Method of spray forming readily weldable and machinable metal deposits

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023754 A1
- Document ID: US20010023754A1
- Status: Published application
- Kind: A1
- Application number: 09/875,847
- Filed: 2001-06-06
- Published: 2001-09-27
- Earliest claimed: 1998-11-04
- Assignees: Ford Global Technologies, LLC
- Inventors: Jeffrey Alan Kinane; David Robert Collins; Matthew John Zaluzec; Paul Earl Pergande; Grigoriy Grinberg
- Web page: https://patentgrep.com/patent/US20010023754A1

## CPC

- B22F 3/1283: {Container formed as an undeformable model eliminated after consolidation}
- B22C 9/061: {Materials which make up the mould}
- B22D 23/003: {Moulding by spraying metal on a surface}
- B22F 3/115: by spraying molten metal, i.e. spray sintering, spray casting
- B33Y 80/00: Products made by additive manufacturing
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B22C: FOUNDRY MOULDING (moulding refractory materials in general B28B)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING

## Abstract

A method of spray forming a weldable metal deposit. The method comprises (a) providing a ceramic spray forming pattern, (b) heating the spray forming pattern to a sustained temperature sufficient to prevent internal stress formation in deposited carbon steel having a carbon content of less than about 0.3 weight percent when deposited on the heated spray forming pattern, (c) spraying metallic particles onto the spray forming pattern heated to the sustained temperature, and (d) allowing the sprayed metallic particles to cool to form a metal deposit. The metallic particles have a carbon content which is sufficient to result in metal particles having a carbon content of less than about 0.3 weight percent when deposited on the heated spray forming pattern. The resulting deposit has a carbon content of less than about 0.3 weight percent.

## Claims

### Claim 1

A method of spray forming a weldable metal deposit; said method comprising:
(a) providing a ceramic spray forming pattern;
(b) heating the spray forming pattern to a sustained temperature sufficient to prevent internal stress formation in carbon steel having a carbon content of less than about 0.3 weight percent deposited on the heated spray forming pattern;
(c) spraying metallic particles onto the spray forming pattern heated to the sustained temperature, the metallic particles having a carbon content which is sufficient to result in metal particles having a carbon content of less than about 0.3 weight percent when deposited on the heated spray forming pattern; and
(d) allowing the sprayed metallic particles to cool to form a metal deposit having a carbon content of less than about 0.3 weight percent.

### Claim 2 (depends on 1)

The method of claim 1 wherein the sustained temperature is above about 500° C.

### Claim 3 (depends on 1)

The method of claim 1 wherein the sustained temperature is above about 600° C.

### Claim 4 (depends on 1)

The method of claim 1 wherein the sustained temperature is above about 700° C.

### Claim 5 (depends on 1)

The method of claim 1 wherein at least one thermal spray gun is provided for spraying the metallic particles onto the heated spraying pattern.

### Claim 6 (depends on 1)

The method of claim 1 wherein carbon steel having a carbon content of less than about 0.6 weight percent is provided for forming the sprayed metallic particles.

### Claim 7 (depends on 6)

The method of claim 6 wherein the carbon steel has a carbon content of less than about 0.3 weight percent.

### Claim 8 (depends on 7)

The method of claim 7 wherein the carbon steel has a carbon content of less than about 0.1 weight percent.

### Claim 9 (depends on 5)

The method of claim 5 wherein each of the thermal spray guns include a gun tip which is oriented about 7-14 inches from the spray forming pattern, each of the guns having a current spray in the range of about 100-250 amperes.

### Claim 10 (depends on 9)

The method of claim 9 wherein each of the thermal spray guns include a gun tip which is oriented about 8-10 inches from the spray forming pattern, each of the guns having a current spray in the range of about 150-200 amperes.

### Claim 11 (depends on 9)

The method of claim 9 wherein the metallic particles in step (c) are maintained at a temperature above about 300° C. during step (c).

### Claim 12 (depends on 1)

The method of claim 1 wherein the metal deposit has a Rockwell C hardness of less than about 35.