# US 2001/0023725 A1 · Brake disk for motor vehicles, as well as a steel alloy and a method for producing them

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023725 A1
- Document ID: US20010023725A1
- Status: Published application
- Kind: A1
- Application number: 09/794,168
- Filed: 2001-02-28
- Published: 2001-09-27
- Earliest claimed: 2000-03-24
- Assignees: Edelstahl Werke Buderus AG
- Inventors: Walter Grimm
- Web page: https://patentgrep.com/patent/US20010023725A1

## CPC

- C22C 38/22: with molybdenum or tungsten
- C22C 38/44: with molybdenum or tungsten
- F16D 65/12: Discs; Drums for disc brakes
- F16D 2200/0021: Steel
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- F16D: COUPLINGS FOR TRANSMITTING ROTATION; CLUTCHES; BRAKES

## Abstract

The proposed brake disk consists of steel of a composition of 0.1 to 0.4% of carbon, up to 1.0% of silicon, up to 2.0% of manganese, up to 0.02% of sulfur, 11 to 16% of chromium, up to 1.0% of nickel and 0.5 to 1.5% of molybdenum, the remainder being iron and production-related impurities.

## Claims

### Claim 1

A brake disk for motor vehicles, consisting of steel of the composition
0.1 to 0.4% of carbon
up to 1.0% of silicon
up to 2.0% of manganese
up to 0.02% of sulfur
11 to 16% of chromium
up to 1.0% of nickel
0.5 to 1.5% of molybdenum,
the remainder being iron and production-related impurities.

### Claim 2

A steel alloy for brake disks of motor vehicles, characterized in that it consists of
0.2 to 0.3% of carbon
up to 1.0% of silicon
up to 1.5% of manganese
up to 0.01% of sulfur
12 to 15% of chromium
up to 1.0% of nickel
0.6 to 1.2% of molybdenum,
the remainder being iron and production-related impurities.

### Claim 3 (depends on 1)

A method for producing a motor vehicle brake disk in accordance with claim 1 by stamping, precision cutting or cold forming from hot- and cold-rolled steel strips.

### Claim 4 (depends on 3)

The method in accordance with claim 3, characterized in that the steel is set to strengths between 600 and 1000 N/mm2 by means of a heat treatment, such as annealing or hardening and tempering.