# US 2001/0023724 A1 · Procedure for the thermal treatment of rails

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023724 A1
- Document ID: US20010023724A1
- Status: Published application
- Kind: A1
- Application number: 09/864,288
- Filed: 2001-05-25
- Published: 2001-09-27
- Earliest claimed: 1992-07-15
- Assignees: VOEST-ALPINE SCHIENEN GmbH, Leoben AUSTRIA
- Inventors: Alfred Moser; Georg Prskawetz; Peter Pointner
- Web page: https://patentgrep.com/patent/US20010023724A1

## CPC

- C21D 9/04: for rails
- C21D 1/60: Aqueous agents
- C21D 1/63: for bath quenching
- C21D 2221/02: Edge parts
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)

## Abstract

A method for the thermal treatment of rails, in particular of the rail head, in which cooling is carried out in a cooling agent that contains a synthetic cooling agent additive starting at temperatures above 720° C. The treatment is carried out by immersion in the cooling agent until withdrawal of the immersed areas occurs, at a surface temperature between 450 and 550° C. results without temperature equalization across the whole of the cross-section, thereby avoiding hardening of the rail web while maintaining an optimal cooling rate for the rail head.

## Claims

### Claim 1

A method for the thermal treatment of a rail head of a rail in which cooling is carried out, comprising:
immersing the rail head at an initial temperature of above 720° C. in a cooling agent that contains a synthetic cooling agent additive; and
withdrawing the rail head from the cooling agent upon obtaining a surface temperature of the rail head of between 450 and 550° C.;
wherein the rail head includes an inner portion and an outer portion, the outer portion being closer to a surface of the rail head than the inner portion, and wherein the rail head is withdrawn from the cooling agent while a temperature of the inner portion of the rail head is still higher than a temperature of the outer portion of the rail head.

### Claim 2 (depends on 1)

A method set forth in claim 1, wherein the synthetic additive is a glycol or polyglycol included in the cooling agent in a quantity at which a bath temperature of the cooling agent between 35-55° C. has a transition from film boiling to a boiling phase at a temperature between 450 and 550° C. so as to indicate the time when the rail head should be withdrawn from the cooling agent.

### Claim 3 (depends on 2)

A method as set forth in claim 2, wherein the rail includes a rail foot which is cooled by at least one of compressed air and a water-air mixture.

### Claim 4 (depends on 2)

A method as set forth in claim 2, wherein the rail is steel having a guide analysis of 0.65-0.85% C, 0.01-1.2% Si, 0.5-3.5% Mn, 0.01-1.0% Cr, and the rest Fe and impurities.

### Claim 5 (depends on 4)

A method as set forth in claim 4, wherein the rail includes a rail foot which is cooled by at least one of compressed air and a water-air mixture.

### Claim 6 (depends on 1)

A method as set forth in claim 1, wherein the rail includes a rail foot which is cooled by at least one of compressed air and a water-air mixture.

### Claim 7 (depends on 1)

A method as set forth in claim 1, wherein the rail is steel having a guide analysis of 0.65-0.85% C, 0.01-1.2% Si, 0.5-3.5% Mn, 0.01-1.0% Cr, and the rest Fe and impurities.

### Claim 8 (depends on 7)

A method as set forth in claim 7, wherein the rail includes a rail foot which is cooled by at least one of compressed air and a water-air mixture.

### Claim 9

A method for the thermal treatment of a rail head of a rail in which cooling is carried out, comprising:
immersing the rail head at an initial temperature of above 720° C. in a cooling agent that contains a synthetic cooling agent additive selected from at least one of glycols and polyglycols; and
withdrawing the rail head from the cooling agent upon obtaining a surface temperature of said rail head of between 450 and 550° C.;
wherein the rail head is withdrawn from the cooling agent while the temperature of the rail head at a distance of approximately 25 mm from a surface of the rail head is still higher than said surface temperature.

### Claim 10

A method for the thermal treatment of a rail head of a rail in which cooling is carried out, comprising:
immersing the rail head at an initial temperature of above 720° C. in a cooling agent with a bath temperature between 35 and 55° C. and which has a transition from film boiling to a boiling phase at a temperature at which the rail head should be withdrawn; and
withdrawing the rail head when the transition occurs.

### Claim 11 (depends on 10)

A method as set forth in claim 10, wherein the transition occurs between 450 and 550° C.

### Claim 12 (depends on 11)

A method as set forth in claim 11, wherein the cooling agent comprises a synthetic cooling agent additive.

### Claim 13 (depends on 12)

A method as set forth in claim 12, wherein the synthetic cooling agent additive is one of a glycol and a polyglycol.