# US 2001/0023719 A1 · Method of producing superplastic alloys and superplastic alloys produced by the method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023719 A1
- Document ID: US20010023719A1
- Status: Published application
- Kind: A1
- Application number: 09/814,687
- Filed: 2001-03-15
- Published: 2001-09-27
- Earliest claimed: 1998-06-15
- Inventors: Lillianne P. Troeger; Edgar A. Starke JR.; Roy Crooks
- Web page: https://patentgrep.com/patent/US20010023719A1

## CPC

- C22F 1/05: of alloys of the Al-Si-Mg type, i.e. containing silicon and magnesium in approximately equal proportions
- C22C 21/08: with silicon
- C22F 1/047: of alloys with magnesium as the next major constituent
- C22F: CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS AND NON-FERROUS ALLOYS (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass, C23F17/00)
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

A method for producing new superplastic alloys by inducing in an alloy the formation of precipitates having a sufficient size and homogeneous distribution that a sufficiently refined grain structure to produce superplasticity is obtained after subsequent PSN processing. An age-hardenable alloy having at least one dispersoid phase is selected for processing. The alloy is solution heat-treated and cooled to form a supersaturated solid solution. The alloy is plastically deformed sufficiently to form a high-energy defect structure useful for the subsequent heterogeneous nucleation of precipitates. The alloy is then aged, preferably by a multi-stage low and high temperature process, and precipitates are formed at the defect sites. The alloy then is subjected to a PSN process comprising plastically deforming the alloy to provide sufficient strain energy in the alloy to ensure recrystallization, and statically recrystallizing the alloy. A grain structure exhibiting new, fine, equiaxed and uniform grains is produced in the alloy. An exemplary 6xxx alloy of the type capable of being produced by the present invention, and which is useful for aerospace, automotive and other applications, is disclosed and claimed. The process is also suitable for processing any age-hardenable aluminum or other alloy.

## Claims

### Claim 1

A method for producing a superplastic alloy, said method comprising:
providing an alloy for processing, said alloy comprising a matrix phase and at least two alloying elements, at least one of said alloying elements being, or being capable of forming, a dispersoid phase substantially insoluble in said matrix phase;
solution heat treating said alloy;
cooling the alloy to form a supersaturated solid solution;
plastically deforming said alloy in a first deformation step sufficiently to form a high-energy defect structure, thereby forming nucleation sites useful for the subsequent nucleation of precipitates;
aging said alloy, thereby forming precipitates at said nucleation sites; and
plastically deforming said alloy in a second deformation step, and statically recrystallizing said alloy, through a particle-stimulated nucleation process.

### Claim 2 (depends on 1)

The method of claim 1, wherein said step of providing an alloy for processing comprises providing an aluminum alloy.

### Claim 3 (depends on 2)

The method of claim 2, wherein said aluminum alloy is selected from the group consisting of aluminum alloys 6013, 6111, 6061, 6063, and 6066.

### Claim 4 (depends on 1)

The method of claim 1, wherein said cooling step comprises quenching.

### Claim 5 (depends on 1)

The method of claim 1, wherein said first deformation step comprises plastically deforming said alloy sufficiently to form deformation bands.

### Claim 6 (depends on 1)

The method of claim 1, wherein said first deformation step comprises cold rolling said alloy.

### Claim 7 (depends on 6)

The method of claim 6, wherein said first deformation step further comprises cold rolling said alloy at room temperature.

### Claim 8 (depends on 7)

The method of claim 7, wherein said first deformation step further comprises cold rolling said alloy to a reduction of at least about 30%.

### Claim 9 (depends on 1)

The method of claim 1, wherein said aging step comprises a first heating step at a first temperature and a second heating step at a second higher temperature.

### Claim 10 (depends on 9)

The method of claim 9, wherein said precipitates are formed during said first heating step and coarsened during said second heating step.

### Claim 11 (depends on 9)

The method of claim 9, wherein said alloy is cooled after said first heating step and after said second heating step.

### Claim 12 (depends on 1)

The method of claim 1, wherein said second deformation step comprises cold rolling said alloy.

### Claim 13 (depends on 12)

The method of claim 12, wherein said second deformation step further comprises cold rolling said alloy at room temperature.

### Claim 14 (depends on 1)

The method of claim 1, wherein said static recrystallization step comprises rapidly heating said alloy to a temperature at which recrystallization occurs.

### Claim 15 (depends on 1)

The method of claim 1, wherein said static recrystallization step comprises heating said alloy to a temperature in the range of a solution heat-treatment temperature for said alloy.

### Claim 16 (depends on 1)

The method of claim 1, wherein said static recrystallization step comprises heating said alloy to a superplastic forming temperature of said alloy.

### Claim 17

A method for producing a superplastic aluminum alloy, said method comprising:
providing an alloy for processing, said alloy being a 6013/6111 alloy;
solution heat treating said alloy;
cooling the alloy to form a supersaturated solid solution;
plastically deforming said alloy in a first deformation step sufficiently to form a high-energy defect structure, thereby forming nucleation sites useful for the subsequent nucleation of precipitates;
aging said alloy, thereby forming precipitates at said nucleation sites;
plastically deforming said alloy in a second deformation step to provide sufficient strain energy in said alloy to ensure recrystallization; and
statically recrystallizing said alloy.

### Claim 18 (depends on 17)

The method of claim 17, wherein said 6013/6111 alloy has the approximate composition 97.3 wt % Al-0.8 wt % Mg-0.7 wt % Si-0.8 wt % Cu-0.3 wt % Mn-0.1 wt % Fe.

### Claim 19 (depends on 17)

The method of claim 17, wherein said solution heat treating step is performed at a temperature of about 540° C. for about one hour.

### Claim 20 (depends on 17)

The method of claim 17, wherein said cooling step comprises quenching.

### Claim 21 (depends on 17)

The method of claim 17, wherein said first deformation step comprises cold rolling said alloy.

### Claim 22 (depends on 21)

The method of claim 21, wherein said first deformation step comprises cold rolling said alloy to a reduction of at least about 30%.

### Claim 23 (depends on 22)

The method of claim 22, wherein said first deformation step comprises cold rolling said alloy to a reduction of at least about 60%.

### Claim 24 (depends on 17)

The method of claim 17, wherein said first deformation step comprises plastically deforming said alloy sufficiently to form deformation bands.

### Claim 25 (depends on 17)

The method of claim 17, wherein said first deformation step is performed such that, after subsequent aging, said alloy exhibits globular or near-spheroid shaped precipitates.

### Claim 26 (depends on 17)

The method of claim 17, wherein said aging step comprises a first heating step at a first temperature and a second heating step at a second higher temperature.

### Claim 27 (depends on 26)

The method of claim 26, wherein said precipitates are formed during said first heating step and coarsened during said second heating step.

### Claim 28 (depends on 26)

The method of claim 26, wherein said alloy is cooled after said first heating step and after said second heating step.

### Claim 29 (depends on 26)

The method of claim 26, wherein said first heating step is performed at about 300° C. and said second heating step is performed at about 380° C.

### Claim 30 (depends on 29)

The method of claim 29, wherein the duration of said first heating step is about 24 hours, and the duration of said second heating step is about 24 hours.

### Claim 31 (depends on 26)

The method of claim 26, wherein said first heating step is performed at about 300° C. and said second heating step is performed at about 450° C.

### Claim 32 (depends on 31)

The method of claim 31, wherein the duration of said first heating step is about 24 hours, and the duration of said second heating step is about 2 hours.

### Claim 33 (depends on 17)

The method of claim 17, wherein said aging step comprises heating said alloy at a temperature of about 450° C. for about 2 hours.

### Claim 34 (depends on 17)

The method of claim 17, wherein said second deformation step comprises cold rolling said alloy.

### Claim 35 (depends on 34)

The method of claim 34, wherein said second deformation step comprises cold rolling said alloy to a reduction of at least about 80%.

### Claim 36 (depends on 35)

The method of claim 35, wherein said second deformation step comprises cold rolling said alloy to a reduction of at least about 87%.

### Claim 37 (depends on 36)

The method of claim 36, wherein said second deformation step comprises cold rolling said alloy to a reduction of at least about 92%.

### Claim 38 (depends on 17)

The method of claim 17, wherein said static recrystallization step comprises rapidly heating said alloy to a temperature at which recrystallization occurs.

### Claim 39 (depends on 38)

The method of claim 38, wherein said static recrystallization step comprises heating said alloy to a temperature of about 540° C. for about 5 minutes.

### Claim 40

A 6xxx aluminum alloy having a microstructure comprising grains having an average size in the range of about 9.5 μm to about 11.6 μm, said grain sizes having a standard deviation in the range of about 4.7 μm to about 5.6 μm, and said grains further having an average grain aspect ratio in the range of about 1.6 to about 1.9, said grain aspect ratios having a standard deviation in the range of about 0.6 to about 0.8.

### Claim 41 (depends on 40)

The 6xxx aluminum alloy of claim 40, wherein said alloy has a grain roundness in the range of about 1.6 to about 1.8.

### Claim 42 (depends on 40)

The 6xxx aluminum alloy of claim 40, wherein said alloy comprises grains having an average size of about 9.5 μm, said grain sizes having a standard deviation of about 4.7 μm, and said grains further having an average grain aspect ratio of about 1.6, said grain aspect ratios having a standard deviation of about 0.6.

### Claim 43 (depends on 40)

The 6xxx aluminum alloy of claim 40, wherein said alloy exhibits a maximum elongation of at least about 350%.

### Claim 44 (depends on 40)

The 6xxx aluminum alloy of claim 40, wherein said alloy exhibits a maximum strain rate sensitivity of at least about 0.5.

### Claim 45 (depends on 44)

The 6xxx aluminum alloy of claim 44, wherein said alloy exhibits a maximum elongation of at least about 375%.

### Claim 46

A superplastic 6xxx aluminum alloy having a maximum strain rate sensitivity of at least about 0.5 and exhibiting a maximum elongation of at least about 350%, and being produced according to a process comprising:
providing an alloy for processing, said alloy comprising a matrix phase and at least two alloying elements, at least one of said alloying elements being, or being capable of forming, a dispersoid phase substantially insoluble in said matrix phase;
solution heat-treating said alloy;
cooling the alloy to form a supersaturated solid solution;
plastically deforming said alloy in a first deformation step sufficiently to form a high-energy defect structure, thereby forming nucleation sites useful for the subsequent nucleation of precipitates;
aging said alloy, thereby forming precipitates at said nucleation sites; and
plastically deforming said alloy in a second deformation step, and statically recrystallizing said alloy, through a particle-stimulated nucleation process.