# US 2001/0023715 A1 · Magnetic powder and isotropic bonded magnet

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023715 A1
- Document ID: US20010023715A1
- Status: Published application
- Kind: A1
- Application number: 09/755,953
- Filed: 2001-01-05
- Published: 2001-09-27
- Earliest claimed: 2000-01-07
- Assignees: Seiko Epson Corporation
- Inventors: Akira Arai; Hiroshi Kato
- Web page: https://patentgrep.com/patent/US20010023715A1

## CPC

- H01F 1/0579: {with exchange spin coupling between hard and soft nanophases, e.g. nanocomposite spring magnets}
- B82Y 25/00: Nanomagnetism, e.g. magnetoimpedance, anisotropic magnetoresistance, giant magnetoresistance or tunneling magnetoresistance
- H01F 1/0578: {bonded together}
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES
- B82Y: SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES

## Abstract

Disclosed herein is a magnetic powder which can provide a bonded magnet having excellent magnetic properties and having excellent reliability especially excellent heat stability. The magnetic powder is composed of an alloy composition represented by Rx(Fe1-yCoy)100-x-z-wBzAlw (where R is at least one kind of rare-earth element, x is 7.1-9.9 at %, y is 0-0.30, z is 4.6-6.9 at %, and w is 0.02-1.5 at %), the magnetic powder being constituted from a composite structure having a soft magnetic phase and a hard magnetic phase, wherein the magnetic powder has magnetic properties in which, when the magnetic powder is formed into an isotropic bonded magnet having a density ρ [Mg/m3] by mixing with a binding resin and then molding it, the maximum magnetic energy product (BH)max[kJ/m3] of the bonded magnet at the room temperature satisfies the relationship represented by the formula (BH)max/ρ2[×10−9J·m3/g2]≧2.1, and the intrinsic coercive force (HCJ) of the bonded magnet at the room temperature is in the range of 320-720 kA/m.

## Claims

### Claim 1

Magnetic powder composed of an alloy composition represented by Rx(Fe1-yCoy)100-x-z-wBzAlw (where R is at least one kind of rare-earth element, x is 7.1-9.9 at %, y is 0-0.30, z is 4.6-6.9 at %, and w is 0.02-1.5 at %), the magnetic powder being constituted from a composite structure having a soft magnetic phase and a hard magnetic phase, wherein the magnetic powder has magnetic properties in which, when the magnetic powder is formed into an isotropic bonded magnet having a density ρ [Mg/m3] by mixing with a binding resin and then molding it, the maximum magnetic energy product (BH)max[kJ/m3] of the bonded magnet at the room temperature satisfies the relationship represented by the formula (BH)max/ρ2[×10−9J·m3/g2]≧2.1, and the intrinsic coercive force (HCJ) of the bonded magnet at the room temperature is in the range of 320-720 kA/m.

### Claim 2 (depends on 1)

The magnetic powder as claimed in claim 1, wherein when the magnetic powder is formed into an isotropic bonded magnet having a density ρ [Mg/m3] by mixing with a binding resin and then molding it, the remanent magnetic flux density Br[T] at the room temperature satisfies the relationship represented by the formula of Br/ρ [×10−6T·m3/g]≧0.125.

### Claim 3

Magnetic powder composed of an alloy composition represented by Rx(Fe1-yCoy)100-x-z-wBzAlw (where R is at least one kind of rare-earth element, x is 7.1-9.9 at %, y is 0-0.30, z is 4.6-6.9 at %, and w is 0.02-1.5 at %), the magnetic powder being constituted from a composite structure having a soft magnetic phase and a hard magnetic phase, wherein the magnetic powder has magnetic properties in which, when the magnetic powder is formed into an isotropic bonded magnet having a density ρ [Mg/m3] by mixing with a binding resin and then molding it, the remanent magnetic flux density Br[T] at the room temperature satisfies the relationship represented by the formula of Br/ρ [×10−6T·m3/g]≧0.125.

### Claim 4 (depends on 3)

The magnetic powder as claimed in claim 3, wherein when the magnetic powder is formed into an isotropic bonded magnet by mixing with a binding resin and then molding it, the intrinsic coercive force (HCJ) of the magnet at the room temperature is in the range of 320-720 kA/m.

### Claim 5 (depends on 1, 2, 3, 4)

The magnetic powder as claimed in any one of claims 1 to 4, wherein when the magnetic powder is formed into an isotropic bonded magnet by mixing with a binding resin and then molding it, the absolute value of the irreversible flux loss (initial flux loss) is equal to or less than 6.2%.

### Claim 6 (depends on 1, 2, 3, 4, 5)

The magnetic powder as claimed in any one of claims 1 to 5, wherein said R comprises rare-earth elements mainly containing Nd and/or Pr.

### Claim 7 (depends on 1, 2, 3, 4, 5, 6)

The magnetic powder as claimed in any one of claims 1 to 6, wherein said R includes Pr and its ratio with respect to the total mass of said R is 5-75%.

### Claim 8 (depends on 1, 2, 3, 4, 5, 6, 7)

The magnetic powder as claimed in any one of claims 1 to 7, wherein said R includes Dy and its ratio with respect to the total mass of said R is equal to or less than 14%.

### Claim 9 (depends on 1, 2, 3, 4, 5, 6, 7, 8)

The magnetic powder as claimed in any one of claims 1 to 8, wherein the magnetic powder is obtained by quenching the alloy of a molten state.

### Claim 10 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9)

The magnetic powder as claimed in any one of claims 1 to 9, wherein the magnetic powder is obtained by milling a melt spun ribbon of the alloy which is manufactured by using a cooling roll.

### Claim 11 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10)

The magnetic powder as claimed in any one of claims 1 to 10, wherein the magnetic powder is subjected to a heat treatment for at least once during the manufacturing process or after its manufacture.

### Claim 12 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11)

The magnetic powder as claimed in any one of claims 1 to 11, wherein the average particle size of the magnetic powder lies in the range of 0.5-150 μm.

### Claim 13

An isotropic bonded magnet formed by binding a magnetic powder containing Al with a binding resin, wherein the isotropic bonded magnet is characterized in that, when the density of the isotropic bonded magnet is ρ [Mg/m3], the maximum magnetic energy product (BH)max[kJ/m3] at the room temperature satisfies the relationship represented by the formula (BH)max/ρ2[×10−9J·m3/g2]≧2.1, and the intrinsic coercive force (HCJ) of the bonded magnet at the room temperature is in the range of 320-720 kA/m.

### Claim 14 (depends on 13)

The isotropic bonded magnet as claimed in claim 13, wherein when the density of the isotropic bonded magnet is ρ [Mg/m3], the remanent magnetic flux density Br[T] at the room temperature satisfies the relationship represented by the formula of Br/ρ [×10−6T·m3/g]≧0.125.

### Claim 15

An isotropic bonded magnet formed by binding a magnetic powder containing Al with a binding resin, wherein the isotropic bonded magnet is characterized in that, when the density of the isotropic bonded magnet is ρ [Mg/m3], the remanent magnetic flux density Br[T] at the room temperature satisfies the relationship represented by the formula of Br/ρ [×10−6T·m3/g]≧0.125.

### Claim 16 (depends on 15)

The isotropic bonded magnet as claimed in claim 15, wherein the intrinsic coercive force (HCJ) of the bonded magnet at the room temperature is in the range of 320-720 kA/m.

### Claim 17 (depends on 13, 14, 15, 16)

The isotropic bonded magnet as claimed in any one of claims 13 to 16, wherein said magnetic powder is formed of R-TM-B-Al based alloy (where R is at least one rare-earth element and TM is a transition metal containing Iron as a major component thereof).

### Claim 18 (depends on 13, 14, 15, 16, 17)

The isotropic bonded magnet as claimed in any one of claims 13 to 17, wherein the magnetic powder is composed of an alloy composition represented by Rx(Fe1-yCoy)100-x-z-wBzAlw (where R is at least one kind of rare-earth element, x is 7.1-9.9 at %, y is 0-0.30, z is 4.6-6.9 at %, and w is 0.02-1.5 at %).

### Claim 19 (depends on 17, 18)

The isotropic bonded magnet as claimed claim 17 or 18, wherein said R comprises rare-earth elements mainly containing Nd and/or Pr.

### Claim 20 (depends on 17, 18, 19)

The isotropic bonded magnet as claimed in any one of claims 17 to 19, wherein said R includes Pr and its ratio with respect to the total mass of said R is 5-75%.

### Claim 21 (depends on 17, 18, 19, 20)

The isotropic bonded magnet as claimed in any one of claims 17 to 20, wherein said R includes Dy and its ratio with respect to the total mass of said R is equal to or less than 14%.

### Claim 22 (depends on 13, 14, 15, 16, 17, 18, 19, 20, 21)

The isotropic bonded magnet as claimed in any one of claims 13 to 21, wherein the average particle size of the magnetic powder lies in the range of 0.5-150 μm.

### Claim 23 (depends on 13, 14, 15, 16, 17, 18, 19, 20, 21, 22)

The isotropic bonded magnet as claimed in any one of claims 13 to 22, wherein the absolute value of the irreversible flux loss (initial flux loss) is equal to or less than 6.2%.

### Claim 24 (depends on 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23)

The isotropic bonded magnet as clamed in any one of claims 13 to 23, wherein the magnetic powder is constituted from a composite structure having a soft magnetic phase and a hard magnetic phase.

### Claim 25 (depends on 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24)

The isotropic bonded magnet as claimed in any one of claims 13 to 24, wherein the isotropic bonded magnet is to be subjected to multipolar magnetization or has already been subjected to multipolar magnetization.

### Claim 26 (depends on 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25)

The isotropic bonded magnet as claimed in any one of claims 13 to 25, wherein the isotropic bonded magnet is used for a motor.