# US 2001/0023526 A1 · Method for making titanium wire face guard

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0023526 A1
- Document ID: US20010023526A1
- Status: Published application
- Kind: A1
- Application number: 09/791,145
- Filed: 2001-02-22
- Published: 2001-09-27
- Earliest claimed: 2000-02-28
- Assignees: Mad Partners
- Inventors: P. David Halstead; Garry W. McNabb; David E. Wright
- Web page: https://patentgrep.com/patent/US20010023526A1

## CPC

- B21F 15/08: making use of soldering or welding
- A42B 3/20: Face guards, e.g. for ice hockey (A42B3/22 takes precedence)
- Y10S 72/702: Overbending to compensate for springback
- Y10T 29/49826: Assembling or joining
- Y10T 29/49888: Subsequently coating
- B21F: WORKING OR PROCESSING OF METAL WIRE (rolling of metal wire B21B1/16; by drawing, auxiliary operations used in connection with metal-working without essentially removing material B21C)
- A42B: HATS; HEAD COVERINGS (headbands A41D20/00; head-scarves A41D23/00)
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A method of making a face mask including the steps of providing a plurality of lengths of Grade 2, commercially pure titanium wire, having a diameter of from about 0.21 to about 0.24 inches; forming each length at room temperature to a desired bend angle by bending the member at room temperature using rotary bending apparatus to a first bend angle that is from about 1.25 to about 1.35 times greater than the desired bend angle; and welding each of the thus formed lengths to at least one other of the lengths in an ambient, oxygen containing environment.

## Claims

### Claim 1

A method of making a face mask, comprising the steps of:
providing a plurality of lengths of Grade 2, commercially pure titanium wire, having a diameter of from about 0.21 to about 0.24 inches;
forming each length at room temperature to a desired bend angle by bending the member at room temperature using rotary bending apparatus to a first bend angle that is from about 1.25 to about 1.35 times greater than the desired bend angle;
welding each of the thus formed lengths to at least one other of the lengths in an ambient, oxygen containing environment.

### Claim 2 (depends on 1)

The method of claim 1, wherein the step of providing a plurality of lengths of Grade 2, commercially pure titanium wire, having a diameter of from about 0.21 to about 0.24 inches comprises providing lengths of titanium wire in an amount such that each length has a length of from about 6 to about 20 inches and the combined weight of all of the lengths is less than about 10 ounces.

### Claim 3 (depends on 1)

The method of claim 1, further comprising the step of forming additional desired bends in end portions of one or more of the lengths, wherein each additional bend has a second desired bend angle and bending is accomplished by bending the end portions of the lengths at room temperature using press brake bending apparatus to a second bend angle that is from about 1.05 to about 1.15 times greater than the second desired bend angle.

### Claim 4 (depends on 1)

The method of claim 1, wherein the step of welding comprises welding using a press-type projection welder in the presence of air.

### Claim 5 (depends on 1)

The method of claim 1, further comprising the step of coating the face guard with a vinyl compound.

### Claim 6 (depends on 1)

The method of claim 1, wherein the step of welding comprises welding using a press-type projection welder in the presence of air and having a transformer setting for the welder set at about 7, with welder control settings selected so that a squeeze setting of the welder is about 10, a weld/heat setting is about 24, a percent current setting is about 28 and a hold setting is about 1.