# US 2001/0022959 A1 · Highly crystalline Mn2O3 or Mn3O4 manganese oxides

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0022959 A1
- Document ID: US20010022959A1
- Status: Published application
- Kind: A1
- Application number: 09/842,968
- Filed: 2001-04-26
- Published: 2001-09-20
- Earliest claimed: 1998-10-15
- Assignees: FMC Corporation
- Inventors: Vesselin Manev; Titus Faulkner; D. Wayne Barnette
- Web page: https://patentgrep.com/patent/US20010022959A1

## CPC

- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- C01G 45/026: Dimanganese trioxide
- C01G 45/028: Trimanganese tetraoxide
- C01G 45/1242: of the type (Mn2O4)-, e.g. LiMn2O4 or Li(MxMn2-x)O4
- C01G 53/54: of the type (Mn2O4)-, e.g. Li(NixMn2-x)O4 or Li(MyNixMn2-x-y)O4
- C01P 2002/32: spinel-type (AB2O4)
- C01P 2002/52: containing elements as dopants
- C01P 2002/54: one element only
- C01P 2004/03: obtained by SEM
- C01P 2006/10: Solid density
- C01P 2006/11: Powder tap density
- C01P 2006/12: Surface area
- C01P 2006/14: Pore volume
- C01P 2006/40: Electric properties
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present invention includes lithium manganese oxide spinel compounds having a low porosity, a high tap density and a high pellet density, and methods of preparing these compounds. In particular, the method comprises preparing a lithium manganese oxide with a spinel structure and having the formula: wherein: Li1+XMn2−YM1m1M2m2 . . . MkmkO4+Z M1, M2, . . . Mk are cations different than lithium or manganese selected from the group consisting of alkali earth metals, transition metals, B, Al, Si, Ga and Ge; X, Y, m1, m2, . . . , mk, each have a value between 0 and 0.2; Z has a value between −0.1 and 0.2; and X, Y, m1, m2, . . . mk are selected to satisfy the equation: Y=X+m1+m2+. . .+mk.

## Claims

### Claim 1

A lithium manganese oxide with a spinel structure and having the formula:
Li1+XMn2−YM1m1M2m2 . . . MkmkO4+Z
wherein:
M1, M2, . . . Mk are cations different than lithium or manganese selected from the group consisting of alkali earth metals, transition metals, B, Al, Si, Ga and Ge;
X, Y, m1, m2, . . . mk each have a value between 0 and 0.2;
Z has a value between −0.1 and 0.2; and
X, Y, m1, m2, . . . mk are selected to satisfy the equation:
Y=X+m1+m2+. . .+mk
and wherein the pore volume of pores having a mean radius of less than 1 micron in said lithium manganese oxide is no more than 20% of the total pore volume of said lithium manganese oxide.

### Claim 2 (depends on 1)

The spinel compound according to claim 1 wherein the pore volume of pores having a mean radius of less than 1 micron is no more than 15% of the total pore volume of said lithium manganese oxide.

### Claim 3 (depends on 1)

The spinel compound according to claim 1 wherein the pore volume of pores having a mean radius of less than 1 micron is no more than 10% of the total pore volume of said lithium manganese oxide.

### Claim 4 (depends on 1)

The spinel compound according to claim 1 wherein the pellet density is greater than 2.85 g/cm3.

### Claim 5 (depends on 1)

The spinel compound according to claim 1 wherein the pellet density is greater than 2.90 g/cm3.

### Claim 6 (depends on 1)

The spinel compound according to claim 1 wherein the pellet density is greater than 2.95 g/cm3.

### Claim 7 (depends on 1)

The spinel compound according to claim 1 wherein the tap density is greater than 1.9 g/cm3.

### Claim 8 (depends on 1)

The spinel compound according to claim 1 wherein the tap density is greater than 2.1 g/cm3.

### Claim 9 (depends on 1)

The spinel compound according to claim 1 wherein the specific area is less than 0.8 m2/g.

### Claim 10 (depends on 1)

The spinel compound according to claim 1 wherein the specific area is less than 0.6 m2/g.

### Claim 11 (depends on 1)

The spinel compound according to claim 1 wherein the specific area is less than 0.5 m2/g.

### Claim 12 (depends on 1)

The spinel compound according to claim 1 wherein said cations M1,M2, . . . , Mk include cobalt.

### Claim 13

A highly crystalline Mn2O3 or Mn3O4 manganese oxide having a specific area of less than 2.0 m2/g and a low porosity such that the pore volume of pores having a mean radius of less than 1 micron in said manganese oxide is no more than 20% of the total pore volume of said manganese oxide.

### Claim 14 (depends on 13)

The manganese oxide of claim 13 wherein the specific area is less than 1.5 m2/g.

### Claim 15 (depends on 13)

The manganese oxide of claim 13 wherein the specific area is less than 1.0 m2/g.

### Claim 16 (depends on 13)

The manganese oxide of claim 13 further having a tap density of greater than 2.2 g/cm3.

### Claim 17 (depends on 13)

The manganese oxide of claim 13 further having a tap density of greater than 2.4 g/cm3.

### Claim 18

A method of preparing a lithium manganese oxide with a spinel structure and having the formula:
Li1+XMn2−YM1m1M2m2 . . . MkmkO4+Z
wherein:
M1, M2, . . . Mk are cations different than lithium or manganese selected from the group consisting of alkali earth metals, transition metals, B, Al, Si, Ga and Ge;
X, Y, m1, m2, . . . , mk, each have a value between 0 and 0.2;
Z has a value between −0.1 and 0.2; and
X, Y, m1, M2, . . . mk are selected to satisfy the
Y=X+m1+m2+. . .+mk
equation: ps said method comprising the step of:
calcining a mixture comprising:
at least one highly crystalline manganese oxide selected from the group consisting of Mn2O3 and Mn3O4, said manganese oxide having a specific area of less than 2.0 m2/g and a low porosity such that the pore volume of pores having a mean radius of less than 1 micron in said manganese oxide is no more than 20% of the total pore volume of said manganese oxide; and
at least one lithium source compound;
in at least one firing step at a temperature between about 400° C. and about 900° C. to form the lithium manganese oxide spinel compound.

### Claim 19 (depends on 18)

The method according to claim 18 wherein said calcining step comprises calcining said at least one manganese oxide, said at least one lithium source compound, and at least one M1, M2, . . . Mk source compound.

### Claim 20 (depends on 18)

The method according to claim 18 wherein said calcining step comprises calcining a mixture wherein the manganese oxide has a specific area of less than 1.5 m2/g.

### Claim 21 (depends on 18)

The method according to claim 18 wherein said calcining step comprises calcining a mixture wherein the manganese oxide has a specific area of less than 1.0 m2/g.

### Claim 22 (depends on 18)

The method according to claim 18 wherein said calcining step comprises calcining a mixture wherein the manganese oxide has a tap density of greater than 2.2 g/cm3.

### Claim 23 (depends on 18)

The method according to claim 18 wherein said calcining step comprises calcining a mixture wherein the manganese oxide has a tap density of greater than 2.4 g/cm3.

### Claim 24

A method of preparing a lithium manganese oxide with a spinel structure and having the formula:
Li1+XMn2−YM1m1M2m2 . . . MkmkO4+Z
wherein:
M1, M2, . . . , Mk are cations different than lithium or manganese selected from the group consisting of alkali earth metals, transition metals, B, Al, Si, Ga and Ge;
X, Y, m1, m2, . . . , mk, each have a value between 0 and 0.2;
Z has a value between −0.1 and 0.2; and
X, Y, m1, M2, . . . mk are selected to satisfy the equation:
Y=X+m1+m2+. . .+mk
said method comprising the steps of:
preparing at least one manganese oxide selected from the group consisting of Mn2O3 and Mn3O4 by firing β-MnO2 at a temperature between about 500° C. and about 1000° C.; and
calcining a mixture comprising said manganese oxide and at least one lithium source compound in at least one firing step at a temperature between about 400° C. and about 900° C. to form the lithium manganese oxide spinel compound.

### Claim 25 (depends on 24)

The method according to claim 24 wherein said calcining step comprises calcining a mixture of said manganese oxide, said at least one lithium source compound, and at least one M1, M2, . . . Mk source compound.

### Claim 26 (depends on 24)

The method according to claim 24, wherein said preparing step comprises firing β-MnO2 at a temperature between about 600° C. and about 800° C. to form Mn2O3.

### Claim 27 (depends on 24)

The method according to claim 24 wherein said preparing step comprises firing the β-MnO2 at a starting temperature of about 500° C. and raising the temperature at a rate of less than 1° C./min to a temperature between about 600° C. and about 650° C. to thermally decompose the β-MnO2 and form Mn2O3.

### Claim 28 (depends on 24)

The method according to claim 24, further comprising the step of firing Mn(NO3)2 at a temperature between about 200° C. and about 400° C. to thermally decompose the Mn(NO3)2 and form β-MnO2 prior to said preparing step.

### Claim 29 (depends on 24)

The method according to claim 24, wherein said preparing step comprises firing β-MnO2 having a mean particle size between about 5 μm and about 20 μm.

### Claim 30 (depends on 29)

The method according to claim 29, wherein said preparing step further comprises grinding the β-MnO2 to between about 5 μm and about 20 μm prior to said firing the β-MnO2.

### Claim 31 (depends on 24)

The method according to claim 24, further comprising the step of mildly dispersing the lithium manganese oxide spinel compound after said calcining step.

### Claim 32 (depends on 24)

The method according to claim 24, wherein said calcining step comprises firing the mixture in more than one firing step at firing temperatures between about 450° C. and about 850° C.

### Claim 33 (depends on 24)

The method according to claim 24, further comprising the step of preventing agglomeration of the spinel compounds during at least a portion of said calcining step.

### Claim 34 (depends on 33)

The method according to claim 33, wherein at least a portion of said calcining step comprises calcining the mixture in a fluid bed furnace or rotary calciner.

### Claim 35 (depends on 33)

The method according to claim 33, wherein said calcining step comprises grinding the resulting spinel compound during at least a portion of said calcining step.

### Claim 36

A lithium manganese oxide with a spinel structure and having the formula:
Li1+XMn2−YM1m1M2m2 . . . MkmkO4+Z
wherein:
M1, M2, . . . Mk are cations different than lithium or manganese selected from the group consisting of alkali earth metals, transition metals, B, Al, Si, Ga and Ge;
X, Y, m1, m2, . . . mk, each have a value between 0 and 0.2;
Z has a value between −0.1 and 0.2; and
X, Y, m1, m2, . . . mk are selected to satisfy the equation:
Y=X+m1+m2+. . .+mk
and wherein the tap density is greater than 1.9 g/cm3, the pellet density is greater than about 2.85 g/cm3, the specific area is less than 0.8 m2/g, and the full width at half maximum of x-ray diffraction peaks from planes (400) and (440) using CuKa rays is less than about 0.15° 2θ.

### Claim 37 (depends on 36)

The spinel compound according to claim 36, wherein the tap density is greater than 2.1 g/cm3.

### Claim 38 (depends on 36)

The spinel compound according to claim 36, wherein the specific area is less than 0.6 m2/g.

### Claim 39 (depends on 36)

The spinel compound according to claim 36, wherein the specific area is less than 0.5 m2/g.

### Claim 40 (depends on 36)

The spinel compound according to claim 36, wherein the full width at half maximum of x-ray diffraction peaks from planes (400) and (440) using CuKa rays is less than about 0.125° 2θ.