# US 2001/0022958 A1 · Procedure for the production of polymeric sulfur

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0022958 A1
- Document ID: US20010022958A1
- Status: Published application
- Kind: A1
- Application number: 09/777,110
- Filed: 2001-02-05
- Published: 2001-09-20
- Earliest claimed: 2000-02-08
- Assignees: Repsol Petroleo S.A.
- Inventors: Juan Castro Pascual; Fernando Temprano Posada; Jose Carlos Rojo Gonzalez
- Web page: https://patentgrep.com/patent/US20010022958A1

## CPC

- C01B 17/12: Insoluble sulfur (mu-sulfur)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}

## Abstract

A procedure for the production of polymeric sulfur with improved stability that comprises the stages of: (a) cooling in a vessel for rapid cooling the sulfur vapor from the vaporization of molten sulfur, bringing it into direct contact with a refrigerating suspension composed of carbon disulphide, soluble sulfur and polymeric sulfur, to a temperature such that part of the sulfur vapor is transformed into a powder-like polymeric sulfur, insoluble in carbon disulphide. (b) extracting the resulting suspension from the cooling vessel; (c) recycling part of said suspension to the vessel for cooling; and (d) sending the rest of the suspension to a maturation stage to stabilize the polymeric sulfur.

## Claims

### Claim 1

A procedure for the production of polymeric sulfur with improved stability, characterised in that it comprises the stages of:
(a) rapidly cooling, in a cooling vessel, sulfur vapor while in direct contact with a refrigerating suspension comprising carbon disulphide, soluble sulfur and polymeric sulfur, to a temperature such that part of the sulfur vapor is transformed into a powdery polymeric sulfur,
(b) recovering the resulting suspension from the cooling vessel;
(c) recycling part of said suspension to the cooling vessel; and
(d) subjecting the rest of the suspension to maturation.

### Claim 2 (depends on 1)

A procedure according to claim 1, characterised in that in stage (a) the sulfur vapor enters the cooling vessel for rapid cooling at a temperature of between 450 and 750° C.

### Claim 3 (depends on 2)

A procedure according to claim 2, characterised in that in stage (a) the sulfur vapor is cooled by contact with the refrigerating suspension until it reaches a temperature of between 55 and 80° C.

### Claim 4 (depends on 3)

A procedure according to claim 3, characterised in that the concentration of solids in the output stream of the cooling vessel is between 6 and 12%.

### Claim 5 (depends on 3)

A procedure according to claim 3, characterised in that the powdery polymeric sulfur has a particle size of 5-40 microns.

### Claim 6 (depends on 4)

A procedure according to claim 4, characterised in that in the stage of maturation (d), the suspension is kept in agitation at temperatures between 55 and 80° C. for a time period of greater than 30 minutes.

### Claim 7 (depends on 6)

A procedure according to claim 6, characterised in that once the suspension in the maturation stage is thermally stabilized, insoluble sulfur is separated therefrom.

### Claim 8 (depends on 7)

A procedure according to claim 7, characterised in that in the stage of maturation (d), the suspension is kept in agitation at temperatures between 70 and 75° C. for a time period of 60 minutes.

### Claim 9 (depends on 8)

A procedure according to claim 8, characterised in that in stage (a) the sulfur vapor enters the cooling vessel at a temperature of between 650 and 700° C.

### Claim 10 (depends on 9)

A procedure according to claim 9, characterised in that in stage (a) the sulfur vapor is cooled by contact with the refrigerating suspension until it reaches a temperature of between 70 and 75° C.

### Claim 11 (depends on 10)

A procedure according to claim 10, characterised in that the concentration of solids in the output stream of the cooling vessel is 10%.

### Claim 12 (depends on 2)

A procedure according to claim 2, characterised in that in stage (a) the sulfur vapor enters the cooling vessel at a temperature of between 650 and 700° C.

### Claim 13 (depends on 12)

A procedure according to claim 12, characterised in that in stage (a) the sulfur vapor is cooled by contact with the refrigerating suspension until it reaches a temperature of between 70 and 75° C.

### Claim 14 (depends on 13)

A procedure according to claim 13, characterised in that the concentration of solids in the output stream of the cooling vessel is 10%.

### Claim 15 (depends on 3)

A procedure according to claim 3, characterised in that in stage (a) the sulfur vapor is cooled by contact with the refrigerating suspension until it reaches a temperature of between 70 and 75° C.

### Claim 16 (depends on 15)

A procedure according to claim 15, characterised in that the concentration of solids in the output stream of the cooling vessel is 10%.

### Claim 17 (depends on 4)

A procedure according to claim 4, characterised in that the concentration of solids in the output stream of the cooling vessel is 10%.