# US 2001/0022375 A1 · Method to fabricate a new structure with multi-self-aligned for split-gate flash

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0022375 A1
- Document ID: US20010022375A1
- Status: Published application
- Kind: A1
- Application number: 09/777,303
- Filed: 2001-02-06
- Published: 2001-09-20
- Earliest claimed: 2000-02-18
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chia-Ta Hsieh; Tai-Fen Lin; Wen-Ting Chu; Chuang-Ke Yeh; Hung-Cheng Sung; Di-Son Kuo
- Web page: https://patentgrep.com/patent/US20010022375A1

## CPC

- H10B 41/30: characterised by the memory core region
- H10B 69/00: Erasable-and-programmable ROM [EPROM] devices not provided for in groups H10B41/00 - H10B63/00, e.g. ultraviolet erasable-and-programmable ROM [UVEPROM] devices
- H10D 30/685: {from the channel}
- H10D 30/6891: {characterised by the shapes, relative sizes or dispositions of the floating gate electrode}
- H10B: ELECTRONIC MEMORY DEVICES
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

A method is disclosed for forming a split-gate flash memory cell where the floating gate of the cell is self-aligned to isolation, to source and to word line. This multi-self-aligned structure, which provides the maximum shrinkage of the cell that is possible, is also disclosed. The multi-self-alignment is accomplished by first defining the floating gate at the same time the trench isolation is formed, and then self-aligning the source to the floating gate by using a nitride layer as a hard mask in place of the traditional polyoxide, and finally forming a polysilicon spacer to align the word line to the floating gate. Furthermore, a thin floating gate is used to form a thin and sharp poly tip through the use of a “smiling effect” to advantage. The tip substantially decreases the coupling ratio of the floating gate to the word line for fast erasing speed, while at the same time increasing the coupling of the source to the floating gate with the attendant increase in the programming speed of the split gate flash memory cell.

## Claims

### Claim 1

A method of forming a multi-self aligned structure for a split-gate flash comprising the steps of:
providing a semiconductor substrate having shallow trench isolation (STI) formed therein and active regions defined;
forming a gate oxide layer over said substrate;
forming a thin floating gate over said gate oxide layer, wherein said floating gate is vertically self-aligned to said STI;
forming a high temperature oxide (HTO) layer over said thin floating gate;
forming a thick nitride layer over said HTO layer;
growing an inter-poly oxide layer over said thick nitride layer, wherein a sharp thin poly tip is formed employing smiling effect in said thin floating gate;
forming a spacer control gate over said inter-poly oxide wherein said spacer control gate is vertically self-aligned to said floating gate;
forming a common source line self-aligned to said floating gate and said control gate; and
forming a drain to complete forming of said split-gate flash memory cell.

### Claim 2 (depends on 1)

The method of claim 1, wherein said gate oxide layer has a thickness between about 70 to 100 Å.

### Claim 3 (depends on 1)

The method of claim 1, wherein said thin floating gate comprises polysilicon having a thickness between about 50 to 150 Å.

### Claim 4 (depends on 1)

The method of claim 1, wherein said HTO layer has a thickness between about 50 to 100 Å.

### Claim 5 (depends on 1)

The method of claim 1, wherein said nitride layer has a thickness between about 900 to 1100 Å.

### Claim 6 (depends on 1)

The method of claim 1, wherein said inter-poly oxide has a thickness between about 100 to 200 Å.

### Claim 7 (depends on 1)

The method of claim 1, wherein said spacer control gate comprises polysilicon having a thickness between about 1500 to 3000 Å.

### Claim 8 (depends on 1)

The method of claim 1, wherein said forming a common source is accomplished by implanting phosphorus ions at a dosage level between about 1×1015 to 1×1016 atoms/cm2 at an energy between about 20 to 60 KeV.

### Claim 9 (depends on 1)

The method of claim 1, wherein said forming said drain is accomplished by implanting phosphorus ions at a dosage level between about 1×1015 to 1×1016 atoms/cm2 at an energy between about 20 to 60 KeV.

### Claim 10

A method of forming a multi-self aligned structure for a split-gate flash comprising the steps of:
providing a semiconductor substrate;
forming a gate oxide layer over said substrate;
forming a first polysilicon layer over said gate oxide layer;
forming a first nitride layer over said first polysilicon layer;
forming shallow trench isolation (STI) and defining active regions in said substrate;
forming isolation oxide in said STI;
forming high temperature oxide (HTO) over said substrate;
forming second nitride layer over said HTO layer;
forming a first photoresist mask to define a floating gate;
etching said second nitride layer, said HTO layer, and underlying said first polysilicon layer through said first photoresist mask to form a floating gate, wherein said floating gate is vertically self-aligned to said STI;
removing said first photoresist mask;
growing inter-poly oxide layer over said second nitride layer, wherein a sharp thin poly tip is formed employing smiling effect in said floating gate;
forming a second polysilicon layer over said substrate, including over said inter-poly oxide layer;
etching said second polysilicon layer to form a spacer control gate;
forming a second photoresist mask over said substrate;
removing portions of said second polysilicon layer and isolation oxide over source line region;
forming a common source self-aligned to said floating gate and said spacer control gate;
removing said second photoresist mask; and
forming a drain to complete forming of said split-gate flash memory cell.

### Claim 11 (depends on 10)

The method of claim 10, wherein said gate oxide layer is formed at a temperature between about 750 to 950° C., and has a thickness between about 70 to 100 Å.

### Claim 12 (depends on 10)

The method of claim 10, wherein said first polysilicon layer is formed through LPCVD method employing silane SiH4 as a silicon source material at a temperature between about 550 to 650° C. to a thickness between about 50 to 150 Å.

### Claim 13 (depends on 10)

The method of claim 10, wherein said first nitride layer is formed by reacting dichlorosilane (SiCl2H2), or silane (SiH4), with ammonia (NH3) in an LPCVD chamber at a temperature between about 650 to 800° C., having a thickness between about 1400 to 1600 Å.

### Claim 14 (depends on 10)

The method of claim 10, wherein said isolation oxide is an LPCVD oxide having a thickness between about 2500 to 4500 Å.

### Claim 15 (depends on 10)

The method of claim 10, wherein said HTO layer is formed at a temperature between about 750 to 900° C. and to a thickness between about 50 to 100 Å.

### Claim 16 (depends on 10)

The method of claim 10, wherein said second nitride layer has a thickness between about 900 to 1100 Å.

### Claim 17 (depends on 10)

The method of claim 10, wherein said inter-poly oxide is grown at a temperature between about 750 to 900° C., and has a thickness between about 100 to 200 Å.

### Claim 18 (depends on 10)

The method of claim 10, wherein said second polysilicon layer has a thickness between about 1500 to 3000 Å.

### Claim 19 (depends on 10)

The method of claim 10, wherein said forming a common source is accomplished by implanting phosphorus ions at a dosage level between about 1×1015 to 1×1016 atoms/cm2 at an energy between about 20 to 60 KeV.

### Claim 20 (depends on 10)

The method of claim 10, wherein said forming said drain is accomplished by implanting phosphorus ions at a dosage level between about 1×1015 to 1×106 atoms/cm2 at an energy between about 20 to 60 KeV.

### Claim 21

A multi-self aligned split-gate flash memory cell comprising:
a semiconductor substrate having shallow trench isolation (STI);
a gate oxide layer over said substrate;
a thin floating gate over said gate oxide layer, wherein said floating gate is vertically self-aligned to said STI;
a thin sharp poly tip in said floating gate;
a high temperature oxide (HTO) layer over said thin floating gate;
a thick nitride layer over said HTO layer;
an inter-poly oxide layer over said thick nitride layer;
a spacer control gate over said inter-poly oxide wherein said spacer control gate is vertically self-aligned to said floating gate;
a common source line self-aligned to said floating gate and said control gate; and
a drain to complete said split-gate flash memory cell.

### Claim 22 (depends on 21)

A multi-self aligned split-gate flash memory cell of claim 21, wherein said gate oxide layer has a thickness between about 70 to 100 Å.

### Claim 23 (depends on 21)

A multi-self aligned split-gate flash memory cell of claim 21, wherein said thin floating gate comprises polysilicon having a thickness between about 50 to 150 Å.

### Claim 24 (depends on 21)

A multi-self aligned split-gate flash memory cell of claim 21, wherein said thin sharp poly tip has a thickness between about 50 to 150 Å.

### Claim 25 (depends on 21)

A multi-self aligned split-gate flash memory cell of claim 21, wherein said HTO layer has a thickness between about 50 to 100 Å.

### Claim 26 (depends on 21)

A multi-self aligned split-gate flash memory cell of claim 21, wherein said nitride layer has a thickness between about 900 to 1100 Å.

### Claim 27 (depends on 21)

A multi-self aligned split-gate flash memory cell of claim 21, wherein said inter-poly oxide has a thickness between about 100 to 200 Å.

### Claim 28 (depends on 21)

A multi-self aligned split-gate flash memory cell of claim 21, wherein said sp acer control gate comprises polysilicon having a thickness between about 1500 to 3000 Å.

### Claim 29 (depends on 21)

A multi-self aligned split-gate flash memory cell of claim 21, wherein said forming a common source is accomplished by implanting phosphorus ions at a dosage level between about 1×1015 to 1×1016 atoms/cm2 at an energy between about 20 to 60 KeV.

### Claim 30 (depends on 21)

A multi-self aligned split-gate flash memory cell of claim 21, wherein said forming said drain is accomplished by implanting phosphorus ions at a dosage level between about 1×1015 to 1×1016 atoms/cm2 at an energy between about 20 to 60 KeV.