# US 2001/0022354 A1 · Oxide magnetic material, coil components using the same, and method for producing oxide magneticmaterials and coil components

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0022354 A1
- Document ID: US20010022354A1
- Status: Published application
- Kind: A1
- Application number: 09/764,089
- Filed: 2001-01-19
- Published: 2001-09-20
- Earliest claimed: 2000-01-21
- Assignees: TDK Corporation
- Inventors: Ko Ito; Yukio Takahashi
- Web page: https://patentgrep.com/patent/US20010022354A1

## CPC

- C04B 35/265: {Compositions containing one or more ferrites of the group comprising manganese or zinc and one or more ferrites of the group comprising nickel, copper or cobalt}
- H01F 1/344: {Ferrites, e.g. having a cubic spinel structure (X2+O)(Y23+O3), e.g. magnetite Fe3O4}
- H01F 41/046: {structurally combined with ferromagnetic material}
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- H01F: MAGNETS; INDUCTANCES; TRANSFORMERS; SELECTION OF MATERIALS FOR THEIR MAGNETIC PROPERTIES

## Abstract

To use a media agitating mill of a wet internal circulation type when grinding materials, and offer oxide magnetic materials and coils in which influences of ZrO2 and Y2O3 mixing when using partially stabilized zirconia as media beads are improved. The magnetic materials and coils are characterized in that Fe2O3, ZnO, NiO and CuO are main components, and Y2O3, ZrO2 and Bi2O3 are contained with respect to these main components, where an amount of Y2O3 is 0.007 to 0.028 wt % for the total amount, an amount of ZrO2 is 0.12 to 0.55 wt % therefor and an amount of Bi2O3 is 0.03 to 10.12 wt % for the same.

## Claims

### Claim 1

An oxide magnetic material comprising:
Fe2O3 of 35 to 51 mol %, ZnO less than 35 mol %, NiO more than 5 mol % and CuO of 1 to 35 mol % as main components, and
Y2O3, ZrO2 and Bi2O3 are contained with respect to these main components, where an amount of Y2O3 is 0.007 to 0.028 wt %, an amount of ZrO2 is 0.12 to 0.55 wt % and an amount of Bi2O3 is 0.03 to 10.12 wt % for the total amount.

### Claim 2

Coil components of bulk type comprising:
a sintered substance of an oxide magnetic material comprising: Fe2O3 of 35 to 51 mol %, ZnO less than 35 mol %, NiO more than 5 mol % and CuO of 1 to 35 mol % as main components, and Y2O3, ZrO2 and Bi2O3 are contained with respect to these main components, where an amount of Y2O3 is 0.007 to 0.028 wt %, an amount of ZrO2 is 0.12 to 0.55 wt % and an amount of Bi2O3 is 0.03 to 10.12 wt % for the total amount.

### Claim 3

A laminated coil component comprising:
a sintered substance of an oxide magnetic material comprising: Fe2O3 of 35 to 51 mol %, ZnO less than 35 mol %, NiO more than 5 mol % and CuO of 1 to 35 mol % as main components, and Y2O3, ZrO2 and Bi2O3 are contained with respect to these main components, where an amount of Y2O3 is 0.007 to 0.028 wt %, an amount of ZrO2 is 0.12 to 0.55 wt % and an amount of Bi2O3 is 0.03 to 10.12 wt % for the total amount;
wherein said sintered substance is formed with an electric conductive layer.

### Claim 4 (depends on 3)

A laminated coil component as set forth in claim 3, wherein the electric conductive layers are Ag or Ag.Pd alloy being a main component.

### Claim 5

A method of producing an oxide magnetic material comprising Fe2O3 of 35 to 51 mol %, ZnO less than 35 mol %, NiO more than 5 mol % and CuO of 1 to 35 mol % as main components, the method comprising the steps of:
employing a media agitating mill of wet internal circulation type when grinding materials having passed through mixture and grind of raw materials and pre-sintering, using partially stabilized zirconia beads as media beads;
containing Y2O3 whose amount is 0.007 to 0.028 wt % and ZrO2 whose amount is 0.12 to 0.55 wt %; and
separately adding Bi2O3 whose amount is 0.03 to 10.12 wt %.

### Claim 6

A method of producing oxide magnetic materials for coil components, comprising Fe2O3 of 35 to 51 mol %, ZnO less than 35 mol %, NiO more than 5 mol % and CuO of 1 to 35 mol % as main components, the method comprising the steps of:
employing a media agitating mill of wet internal circulation type for grinding materials having passed through mixture and grind of raw materials and pre-sintering, using partially stabilized zirconia beads as media beads;
containing Y2O3 whose amount for the total amount is 0.007 to 0.028 wt % and ZrO2 whose amount therefor is 0.12 to 0.55 wt %;
separately adding Bi2O3 to be 0.03 to 10.12 wt % for the total amount in the oxide magnetic material;
carrying out dispersion by means of the media agitating mill of wet internal circulation type.

### Claim 7 (depends on 5, 6)

A method of producing oxide magnetic material as set forth in claim 5 or 6, wherein agitation speed of the media beads is in a range of 4.0 to 10.0 m/s.

### Claim 8

A method of producing laminated coil components characterized by forming and sintering at 880 to 910° C. internal conductors in an oxide magnetic material comprising: Fe2O3 of 35 to 51 mol %, ZnO less than 35 mol %, NiO more than 5 mol % and CuO of 1 to 35 mol % as main components, and Y2O3, ZrO2 and Bi2O3 are contained with respect to these main components, where an amount of Y2O3 is 0.007 to 0.028 wt %, an amount of ZrO2 is 0.12 to 0.55 wt % and an amount of Bi2O3 is 0.03 to 10.12 wt % for the total amount.

### Claim 9 (depends on 8)

A method of producing laminated coil components as set forth in claim 8, wherein the internal conductors are Ag or Ag.Pd alloy being a main component.