# US 2001/0022271 A1 · Method for the production of substrates, magnetron source and sputter-coating chamber

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0022271 A1
- Document ID: US20010022271A1
- Status: Published application
- Kind: A1
- Application number: 09/775,527
- Filed: 2001-02-01
- Published: 2001-09-20
- Earliest claimed: 2000-02-04
- Assignees: Unaxis Deutschland GmbH
- Inventors: Bernhard Cord; Gerd Deppich; Karl-Heinz Schuller; Oliver Keitel
- Web page: https://patentgrep.com/patent/US20010022271A1

## CPC

- H01J 37/3429: {Plural materials}
- C23C 14/3407: {Cathode assembly for sputtering apparatus, e.g. Target}
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- H01J 37/3405: {Magnetron sputtering}
- H01J 37/3408: {Planar magnetron sputtering}
- H01J 37/3455: {Movable magnets}
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A target of an alloy of metals having different specific weights is used in a method for producing substrates that are coated with a layer comprising the same two metals by magnetron sputtering of the target. When sputtering such a target material, the metals of the alloy will sputter off with different sputtering characteristics with regard to a static angle a at which the sputtered off material leaves the target. For this reason, at the substrate to be sputter-coated, there occurs a demixing effect of these metals which will be deposited with a varying local ratio of the metals, that differs form the ratio of the metals in the alloy of the target. To counter-act this demixing phenomenon, the location of an electron trap formed by the magnetron field of the sputter source at the target with respect to the location of the substrate, is selected. By proving this electron trap and the resulting erosion profile on the target, the amount of deposited heavier metal to the amount of lighter metal is increased along the surface of the substrate.

## Claims

### Claim 1

A method for producing substrates that are coated with a layer comprising at least two distinct heavy elements (L, S) by magnetron sputtering of a target (6) of a compound of the two elements, where d is an interfacial distance between a substrate surface (5) of the substrate and a new target surface (6o), r is the radius of the substrate, RE is the radius of a site of maximum erosion (Emax) at an erosion profile (9) on the target of an electron trap forming the magnetron magnetic field (H) and substrate, RH is the radius of a site of maximum field strength (H) of the electron trap, parallel to the new target surface of a magnetron tunnel field (11) bringing about the erosion profile (9), the method comprising: selecting a mutual geometric disposition for RE, RH, r and d of the electron trap to approximate a local distribution of a ratio (V) of the target alloy elements in the layer.

### Claim 2 (depends on 1)

A method as claimed in claim 1, wherein the at least two elements are metals and the compound is an alloy.

### Claim 3 (depends on 1)

A method as claimed in claim 1, including increasing the ratio (V) of heavy element (S) to light element (L) in a region of the substrate respect to a surface normal (N, A) on this region, where the field strength (H) and the erosion profile (9) produced thereby on the target (6) is laterally shifted.

### Claim 4 (depends on 1)

A method as claimed in claim 1, wherein the ratio (V) of heavy element to light element is lowered in a region of the substrate that, with respect to a surface normal (N, A) on this region, the field strength (H) and the thereby produced erosion profile (9′) on target (6) is shifted toward the region in which the normal (A) penetrates the new sputter surface (6o) of the target (6).

### Claim 5 (depends on 4)

A method as claimed in claim 4, including providing a first magnetic field (H9) in a first substrate region to raise the ratio (V) and providing a second magnetic field (H9′) in a further substrate region to lower the ratio (V).

### Claim 6 (depends on 1)

A method as claimed in claim 1, wherein the substrate is one of essentially planar, circularly or annularly in shape with an annularly or circular-disk shaped magnetron target that is coaxial with the substrate, including providing a magnetron magnetic field annularly over a sputter surface of the target, which has a maximal field component (Hmax) parallel to the new target surface essentially along a coaxial circle, and the circle radius RH is greater than the substrate radius r.

### Claim 7 (depends on 1)

A method as claimed in claim 1, wherein the substrate is one of essentially planar, circularly or annularly in shape with an annularly or circular-disk shaped magnetron target that is coaxial with the substrate, wherein, on the target, a coaxially encircling erosion excavation is produced as part of the erosion profile, whose greatest depth is essentially on a coaxial circular path, and whose radius RE is greater than the substrate radius r.

### Claim 8 (depends on 6)

A method as claimed in claim 6, wherein for RE and/or RH:
1.2r≦(RE, RH)≦5r.

### Claim 9 (depends on 7)

A method as claimed in claim 7, wherein for RE and/or RH:
1.2r≦(RE, RH)≦5r.

### Claim 10 (depends on 1)

A method as claimed in claim 1, wherein, on a planar, circularly or annularly shaped substrate with a circular disk-form magnetron target coaxial with the substrate, a collisional region of substrate and target axis (A) on the target (6) the erosion profile (9′) is produced which is essentially bell-shaped, and that the distance d between new target surface (6o) and the substrate surface to be coated the radius r of the substrate is selected as follows:
r/2≦d≦3r.

### Claim 11 (depends on 1)

A method as claimed in claim 1, wherein, on a planar, circularly or annularly shaped substrate with an annularly or circular-disk shaped magnetron target coaxial with the substrate, to the distance d of the substrate surface to be coated and the new target surface (6o) as well as an overhang ΔRE of that target region wherein the greatest depth of a coaxially encircling erosion profile (9) is formed, the following is established:
0.33d≦ΔRE≦4d.

### Claim 12 (depends on 1)

A method as claimed in claim 1, wherein, on a planar, circularly or annularly shaped substrate with an annularly or circular-disk shaped magnetron target coaxial with the substrate, characterized in that with respect to the distance d of the substrate surface to be coated and the new target surface, on the one hand, and the overhang ΔRH of a circular coaxial site of maximum new target surface-parallel magnetic field strength (Hmax) the following is established:
0.33d≦ΔRH≦4d.

### Claim 13 (depends on 1)

A method as claimed in claim 1, wherein, on the target, at least two coaxial erosion profiles are produced, with a radial distance ΔρE of their sites of greatest erosion depth, with respect to the distance d between the substrate surface to be coated and the new target surface, is adjusted according to be:
ΔρE≦2d.

### Claim 14 (depends on 1)

A method as claimed in claim 1, wherein, on the target at least two coaxial magnetron tunnel fields are generated with a radial distance ΔρH of the sites of maximum new target surface-parallel field strength (Hmax), wherein this, with respect to distance d between substrate surface to be coated and new target surface is adjusted according to:
ΔρH≦2d.

### Claim 15

A method for producing an essentially centric erosion profile (9′) on a magnetron target, wherein, in a center of the target (A) a tunnel-shaped magnetic field (H9′) over the target sputter surface is generated, whereon the magnetic field lines, exit or penetrate along a target surface zone encircling the center (A) and directly in the region of center A, however with respect to an offset to the center, the field lines enter or exit the sputter surface, and the magnetic field with respect to the target sputter surface is rotated (ω) about the center (A).

### Claim 16

A magnetron source with a target (6) and a movable magnet configuration driven about an axis (A) perpendicular to the new target surface, characterized in that the magnet configuration comprises at least one magnet collar (14, 14″) extending at least in a sector about the axis, as well as in the region of the axis of rotation (A), radially offset with respect to it, a magnet (M, 12″).

### Claim 17 (depends on 15)

A magnetron source as claimed in claim 15, wherein the magnet collar (14) extends in the form of a kidney about the axis of rotation (A), but not encompassing it, and with respect to this magnet collar (14) disposed radially outwardly, at least one further magnet collar (12) is provided, which encompasses the axis of rotation (A), wherein the magnet (M, 12″) is formed by a terminal magnet (M) of a spoke-like magnet configuration (16) projecting from the further magnet collar (12) radially into the kidney-shaped indentation of the first listed magnet collar (14).

### Claim 18

A sputter-coating chamber with a magnetron source with circular-disk or annularly shaped planar target (6) as well as a substrate mounting for receiving an annularly or circular-disk shaped substrate (7) coaxial (A) with the target (6) and spaced apart with respect to it, wherein the magnetron source generates at least one coaxial magnetron field (H9) revolving about the axis, characterized in that for the radial distance RH of the essentially circular site of maximum new target surface-parallel field strength (Hmax) and the substrate radius r:
1.2r≦RH≦5r.

### Claim 19 (depends on 18)

A sputter-coating chamber according to the claim 18, wherein, for the radius RE of a site of maximum erosion depth (Emax) of an essentially coaxial erosion excavation (9) and the radius r of the substrate:
1.2r≦RE≦5r.

### Claim 20 (depends on 18)

A sputter-coating chamber as claimed in claim 18, wherein, with respect to the substrate radius r and the distance d between the substrate surface to be coated and new target surface:
r/2≦d≦3r.

### Claim 21 (depends on 18)

A sputter-coating source as claimed in claim 18, wherein, the overhang ΔRE of the radius RE of a site of greatest erosion depth (Emax) revolving coaxially about axis (A) on the target over the substrate radius r and with respect to distance d from the new target surface to the substrate surface to be coated:
0.33d≦ΔRE≦4d.

### Claim 22 (depends on 18)

A sputter-coating chamber as claimed in claim 18, wherein, for the overhang ΔRH of radius RH of a site of maximum new target surface-parallel magnetic field strength (Hmax) revolving coaxially about axis (A) over the substrate radius r with respect to distance d between the substrate surface to be coated and the new target surface:
0.33d≦ΔRH≦4d.

### Claim 23 (depends on 18)

A sputter-coating chamber as claimed in claim 18, wherein coaxially with the axis on the target at least two erosion zones (9, 9a, 9′) are provided, and for the radial distance ΔρE of the sites of maximum erosion (Emax), with respect to the distance d between the substrate surface to be coated and the new target surface:
ΔQE≦2d.

### Claim 24 (depends on 18)

A sputter-coating chamber as claimed in claim 18, wherein, the magnetron source over the target generates at least two coaxial tunnel field radially spaced apart, and that for the sites of maximum field strength parallel to the new target surface and the distance d between the substrate surface to be coated and the new target surface:
ΔρH23 2d.

### Claim 25 (depends on 18)

A sputter-coating chamber as claimed in claim 18, wherein the substrate coating is an alloy layer comprising at least PtCo, TbFeCo or GdFeCo.

### Claim 26 (depends on 1)

A method as claimed in claim 1, wherein the substrate coating is an alloy layer comprising at least PtCo, TbFeCo or GdFeCo.