# US 2001/0022207 A1 · Method for fabricating a sealed-cavity microstructure

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0022207 A1
- Document ID: US20010022207A1
- Status: Published application
- Kind: A1
- Application number: 09/836,785
- Filed: 2001-04-17
- Published: 2001-09-20
- Earliest claimed: 1998-07-10
- Assignees: DRS Sensors & Targeting Systems, Inc.
- Inventors: Kenneth Maxwell Hays; Alan Glenn Bisignano; Eugene Timothy Fitzgibbons
- Web page: https://patentgrep.com/patent/US20010022207A1

## CPC

- B81C 1/00269: {Bonding of solid lids or wafers to the substrate}
- G01J 5/04: Casings
- G01J 5/045: {Sealings; Vacuum enclosures; Encapsulated packages; Wafer bonding structures; Getter arrangements (getter arrangements per se H10W76/48, H10P36/03)}
- G01J 5/20: using resistors, thermistors or semiconductors sensitive to radiation, e.g. photoconductive devices
- Y10T 156/1054: and simultaneously bonding [e.g., cut-seaming]
- B81C: PROCESSES OR APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OR TREATMENT OF MICROSTRUCTURAL DEVICES OR SYSTEMS (making microcapsules or microballoons B01J13/02; processes or apparatus specially adapted for the manufacture or treatment of piezoelectric, electrostrictive or magnetostrictive elements per se H10N30/01)
- G01J: MEASUREMENT OF INTENSITY, VELOCITY, SPECTRAL CONTENT, POLARISATION, PHASE OR PULSE CHARACTERISTICS OF INFRARED, VISIBLE OR ULTRAVIOLET LIGHT; COLORIMETRY; RADIATION PYROMETRY (light sources F21, H01J, H01K, H05B; investigating properties of materials by optical means G01N)
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

A sealed cavity microstructure and an associated fabrication method are provided that incorporate both a tight pressure seal and a rugged structural bond. A rugged microstructure device incorporating a pressure-maintained cavity may thereby be fabricated. A vacuum cavity microbolometer is also provided that is fabricated using the associated method. The sealed cavity microstructure and the vacuum cavity microbolometer are thereby adapted to low-cost wafer-scale batch processing.

## Claims

### Claim 1

A method of fabricating a microstructure with at least one pressure-maintained cavity, the method comprising steps of:
providing first and second wafers, wherein at least one wafer defines a recessed portion;
joining said first and second wafers such that the recessed portion of at least one of the wafers forms a cavity therebetween;
forming a pressure seal between said first and second wafers to maintain a pre-determined pressure within said cavity; and
forming a structural bond between said first and second wafers to structurally integrate at least a portion of said first and second wafers.

### Claim 2 (depends on 1)

The method of claim 1 wherein said pressure seal forming step comprises depositing a deformable metal peripherally about the cavity on at least one of said first and second wafers.

### Claim 3 (depends on 2)

The method of claim 2 wherein said depositing step comprises depositing at least one deformable metal selected from the group consisting of gold, tin, lead and indium.

### Claim 4 (depends on 2)

The method of claim 2 wherein said depositing step comprises sputtering at least one deformable metal peripherally about the cavity.

### Claim 5 (depends on 1)

The method of claim 1 further comprising the step of forming a seal ring on at least one of said first and second wafers so as to surround the cavity, wherein said step of forming a pressure seal comprises forming a seal on said seal ring.

### Claim 6 (depends on 1)

The method of claim 1 wherein said structural bond forming step is selected from the group consisting of anodic bonding the first and second wafers, direct bonding the first and second wafers, micro-velcro bonding the first and second wafers, and soldering the first and second wafers.

### Claim 7 (depends on 1)

The method of claim 1 wherein a plurality of cavities are defined by the first and second wafers, and wherein the method further comprises the step of dividing the first and second wafers into a plurality of microstructures that each have at least one cavity.

### Claim 8 (depends on 1)

The method of claim 1 wherein a plurality of cavities are defined by the first and second wafers, wherein the method further comprises the step of forming seal rings on at least one of said first and second wafers so as to surround respective ones of the cavities, wherein said pressure seal forming step comprises depositing a deformable metal on each seal ring, wherein said structural bond forming step comprises forming a structural bond outside of and peripherally about at least a portion of each seal ring, and wherein the method further comprises the step of dividing the first and second wafers into a plurality of microstructures that each have at least one cavity.

### Claim 9

A microstructure with at least one pressure-maintained cavity, said microstructure comprising:
first and second wafers defining a cavity therebetween;
a pressure seal between said first and second wafers that extends peripherally about the cavity to maintain a pre-determined pressure within said cavity; and
a structural bond between said first and second wafers to structurally integrate at least a portion of said first and second wafers.

### Claim 10 (depends on 9)

The microstructure of claim 9 wherein said pressure seal comprises a deformable metal deposited on at least one of said first and second wafers.

### Claim 11 (depends on 10)

The microstructure of claim 10 wherein said deformable metal comprises at least one metal selected from the group consisting of gold, tin, lead and indium.

### Claim 12 (depends on 9)

The microstructure of claim 9 wherein at least one of said first and second wafers defines a seal ring extending peripherally about the cavity.

### Claim 13 (depends on 12)

The microstructure of claim 12 wherein said seal ring comprises a dielectric material.

### Claim 14 (depends on 9)

The microstructure of claim 9 wherein said structural bond is selected from the group consisting of an anodic bond, a direct bond, a micro-velcro bond, and a soldered bond.

### Claim 15 (depends on 9)

The microstructure of claim 9 further comprising a MEMS device disposed within the cavity defined by said first and second wafers.

### Claim 16 (depends on 9)

The microstructure of claim 9 further comprising a microbolometer including an array of radiation detectors within the cavity.

### Claim 17 (depends on 9)

The microstructure of claim 9 wherein at least one of said first and second wafers defines a seal ring that extends peripherally about the cavity, wherein the pressure seal comprises a deformable metal deposited on the seal ring, and wherein the structural bond comprises a structural bond formed outside of and peripherally about at least a portion of the seal ring.

### Claim 18

A microbolometer comprising:
first and second wafers defining a cavity therebetween;
at least one radiation detector suspended within the cavity;
a vacuum seal between said first and second wafers that extends peripherally about the cavity to maintain a vacuum within said cavity; and
a structural bond between said first and second wafers to structurally integrate at least a portion of said first and second wafers.

### Claim 19 (depends on 18)

The microbolometer of claim 18 wherein at least one of said first and second wafers further comprises an electrical circuit adapted to sense the temperature of said at least one radiation detector.

### Claim 20 (depends on 18)

The microbolometer of claim 18 wherein at least one of said first and second wafers further comprises an antireflective coating.