# US 2001/0018476 A1 · Transparent, low-flammability, UV-resistant film made from a crystallizable thermoplastic, its use and process for its production

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0018476 A1
- Document ID: US20010018476A1
- Status: Published application
- Kind: A1
- Application number: 09/760,169
- Filed: 2001-01-12
- Published: 2001-08-30
- Earliest claimed: 2000-01-20
- Assignees: Mitsubishi Polyester Film GmbH
- Inventors: Ursula Murschall; Ulrich Kern; Guenther Crass; Andreas Stopp
- Web page: https://patentgrep.com/patent/US20010018476A1

## CPC

- C08J 3/226: {using a polymer as a carrier}
- C08J 5/18: Manufacture of films or sheets
- C09K 21/12: containing phosphorus
- C08J 2367/02: Polyesters derived from dicarboxylic acids and dihydroxy compounds; (C08J2367/06 takes precedence)
- C08J 2467/00: Characterised by the use of polyesters obtained by reactions forming a carboxylic ester link in the main chain; Derivatives of such polymers
- Y10S 428/91: Product with molecular orientation
- Y10S 428/921: Fire or flameproofing
- Y10T 428/263: Coating layer not in excess of 5 mils thick or equivalent
- Y10T 428/265: 1 mil or less
- Y10T 428/31786: Of polyester [e.g., alkyd, etc.]
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
- Y10T: TECHNICAL SUBJECTS COVERED BY FORMER US CLASSIFICATION

## Abstract

The present invention relates to a transparent, low-flammability, UV-resistant, oriented film made from a crystallizable thermoplastic and having a thickness of from 5 to 300 μm. The film comprises at least one UV stabilizer and at least one flame retardant, and at least the flame retardant, and preferably also the UV stabilizer, is fed directly as a masterbatch to the crystallizable thermoplastic during production of the film. The film may have one or more layers, and the UV stabilizer may have been selected from the group consisting of the 2-hydroxybenzophenones, the 2-hydroxybenzotriazoles, the organonickel compounds, the salicylic esters, the cinnamic ester derivatives, the resorcinol monobenzoates, the oxanilides, the hydroxybenzoic esters, the sterically hindered amines and triazines, and the flame retardant may be an organic phosphorus compound, in particular an organic phosphorus compound soluble in polyethylene terephthalate.

## Claims

### Claim 1

A transparent, low-flammability, UV-resistant, oriented film made from a crystallizable thermoplastic and having a thickness of from 5 to 300 μm, wherein the film comprises at least one UV stabilizer and at least one flame retardant, where at least the flame retardant, and preferably also the UV stabilizer, is fed directly as a masterbatch to the crystallizable thermoplastic during production of the film.

### Claim 2 (depends on 1)

The film as claimed in claim 1, wherein the crystallizable thermoplastic comprises polyethylene terephthalate, polybutyleneterephthalate or polyethylene naphthalate, preferably polyethylene terephthalate.

### Claim 3 (depends on 1)

The film as claimed in claim 1, which has one or more layers and has additionally been coated with copolyesters or with adhesion promoters.

### Claim 4 (depends on 1)

The film as claimed in claim 1, wherein the amount of flame retardant present is from 0.5 to 30% by weight, based on the weight of the layer of the crystallizable thermoplastic.

### Claim 5 (depends on 1)

The film as claimed in claim 1, wherein the amount of the UV stabilizer present is from 0.01 to 5% by weight, based on the weight of the layer of the crystallizable thermoplastic.

### Claim 6 (depends on 1)

The film as claimed in claim 1, wherein the UV stabilizer present comprises light stabilizers selected from one or more elements of the group consisting of 2-hydroxybenzophenones, 2-hydroxybenzotriazoles, organonickel compounds, salicylic esters, cinnamic ester derivatives, resorcinol monobenzoates, oxanilides, hydroxybenzoic esters, sterically hindered amines and triazines.

### Claim 7 (depends on 1)

The film as claimed in claim 1, wherein the flame retardant comprises organic phosphorus compounds.

### Claim 8 (depends on 7)

The film as claimed in claim 7, wherein the flame retardant comprises dimethyl methylphosphonate.

### Claim 9 (depends on 1, 7)

The film as claimed in claim 1 or 7, wherein from 0.1 to 1.0% by weight of a hydrolysis stabilizer selected from the group consisting of alkali metal stearates, alkaline earth metal stearates, alkali metal carbonates and alkaline earth metal carbonates, or from 0.05 to 0.6% by weight, of a hydrolysis stabilizer selected from one or more elements of the group consisting of phenolic stabilizers having a molar mass above 500 g/mol is additionally present in the film.

### Claim 10 (depends on 9)

The film as claimed in claim 9, wherein the phenolic stabilizers is pentaerythrityl tetrakis-3-(3,5-di-tert-butyl-4-hydroxyphenyl)propionate or 1,3,5-trimethyl-2,4,6-tris(3,5-di-tert-butyl-4-hydroxybenzyl)benzene.

### Claim 11 (depends on 9)

The film as claimed in claim 9, wherein the organic phosphorus compounds comprise long-chain, encapsulated ammonium polyphosphates or carboxyphosphinic acids or anhydrides of these and wherein, besides the hydrolysis stabilizer, from 0.01 to 5.0% by weight of 2-(4,6-diphenyl-1,3,5-triazin-2-yl)-5-hexyloxyphenol or from 0.01 to 5.0% by weight of 2,2-methylenebis(6-(2H-benzotriazol-2-yl)-4-(1,1,2,2-tetramethylpropyl)phenol or mixtures of these UV stabilizers or mixtures of at least one of these two UV stabilizers with other UV stabilizers are present in the film, where the total amount of UV stabilizer is from 0.01 to 5.0% by weight, based on the weight of crystallizable polyethylene terephthalate.

### Claim 12 (depends on 1)

The film as claimed in claim 1, wherein the surface gloss of the film, measured according to DIN 67530 (measurement angle: 20°), is above 100, and wherein its luminous transmittance L, measured according to ASTM D 1003, is above 80%, and wherein its haze, measured according to ASTM S 1003, is below 20%.

### Claim 13 (depends on 1)

A process for producing a transparent, low-flammability, UV-resistant film as claimed in claim 1 by extrusion on an extrusion line, which comprises adding the flame retardant, to the crystallizable thermoplastic, by way of masterbatch technology, where the flame retardant has been fully dispersed in a solid carrier material, in polyethylene terephthalate or in another polymer compatible with the thermoplastic.

### Claim 14 (depends on 13)

The process as claimed in claim 13, wherein the UV stabilizer, too, is added by way of masterbatch technology, where the UV stabilizer has been fully dispersed in a solid carrier material, in polyethylene terephthalate or in another polymer sufficiently compatible with the thermoplastic.

### Claim 15 (depends on 13, 14)

The process as claimed in claim 13 or 14 wherein the flame retardant continues a hydrolysis stabilizer.

### Claim 16 (depends on 13, 14, 15)

The process as claimed in claim 13, 14 or 15, wherein the particle size and the bulk density of the masterbatch are set to be similar to the particle size and the bulk density of the thermoplastic.

### Claim 17 (depends on 15)

The process as claimed in claim 15, wherein the masterbatch in which the flame retardant and the hydrolysis stabilizer are present is precrystallized or predried, by taking the masterbatch at room temperature from a metering vessel in the desired blend together with the thermoplastic batchwise into a vacuum dryer which then operates, in particular from 0.1 to 0.3% by weight, at a temperature in range of from 20 to 130° C. during a time of from 2 to 4 while stirring at from 10 to 70 rpm.

### Claim 18 (depends on 17)

The process as claimed in claim 17, wherein the precrystallized or predried masterbatch is post-dried in a downstream vessel, which is evacuated, and operates at a temperature of from 100 to 170° C.