# US 2001/0018257 A1 · Interconnect structure having improved resist adhesion

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0018257 A1
- Document ID: US20010018257A1
- Status: Published application
- Kind: A1
- Application number: 09/775,178
- Filed: 2001-02-01
- Published: 2001-08-30
- Earliest claimed: 1997-08-18
- Assignees: Micron Technology, Inc.
- Inventors: Viju K. Mathews
- Web page: https://patentgrep.com/patent/US20010018257A1

## CPC

- H10P 50/71: {using masks for conductive or resistive materials}
- Y10S 438/902: Capping layer
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- Y10S: TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS

## Abstract

A method for use in patterning a conductive layer of an integrated circuit includes providing a conductive layer to be patterned and then forming a titanium nitride layer on the conductive layer. An oxide region is formed on the titanium nitride layer. A photoresist layer is formed on the oxide region for use in patterning the conductive layer. The oxide region may be formed by oxidation of the titanium nitride layer or by depositing an oxide layer on the titanium nitride layer.

## Claims

### Claim 1

A method for use in patterning a conductive layer of an integrated circuit, the method comprising the steps of:
providing a conductive layer;
forminng a titanium nitride layer on the conductive layer;
oxidizing the titanium nitride layer resulting in an oxide region having a thickness in the range of about 5 nanometers to about 30 nanometers; and
forming a photoresist layer on the oxide region.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the thickness is in the range of about 5 nanometers to about 20 nanometers.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the step of oxidizing the titanium nitride layer includes oxidizing the titanium nitride layer at a temperature less than about 400° C.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the step of oxidizing the titanium nitride layer includes oxidizing the titanium nitride layer at a pressure in the range of about 10 to about 50 atmospheres.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the step of oxidizing the titanium nitride layer includes oxidizing the titanium nitride layer at a pressure in the range of about 10 to about 50 atmospheres.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the step of oxidizing the titanium nitride layer includes oxidizing the titanium nitride layer us in g ozone.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the step of oxidizing the titanium nitride layer includes reacting the titanium nitride layer with a solution.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the step of oxidizing the titanium nitride layer includes subjecting the titanium nitride layer to an oxygen ash.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the photoresist is a non-chernically amplified photoresist.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the step of providing a conductive layer includes providing a layer of aluminum.

### Claim 11

A method for use in patterning a conductive layer of an integrated circuit, the method comprising the steps of:
providing a conductive layer;
forming a titanium nitride layer on the conductive layer;
forming an oxide layer on the titanium nitride layer, the oxide layer having a thickness in the range of about 5 nanometers to about 30 nanometers; and
forming a photoresist layer on the oxide layer.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the step of forming an oxide layer includes depositing an oxide layer on the titanium nitride layer.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the oxide layer is a silicon dioxide layer.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the step of forming the oxide layer includes forming an oxidizable layer on the titanium nitride layer and thereafter oxidizing the oxidizable layer.

### Claim 15 (depends on 11)

The method according to claim 11, wherein the thickness is in the range of about 5 nanometers to about 20 nanometers.

### Claim 16 (depends on 11)

The method according to claim 11, wherein the step of forming the oxide layer includes depositing the oxide layer at a temperature less than about 400° C.

### Claim 17 (depends on 11)

The method according to claim 11, wherein the photoresist is a nonchemically amplified photoresist.

### Claim 18 (depends on 11)

The method according to claim 11, wherein the step of providing a conductive layer includes providing a layer of aluminum.

### Claim 19

A method for forming a patterned conductive layer, the method comprising the steps of:
providing a conductive layer;
forming a titanium nitride layer on the conductive layer;
forming an oxide layer having a thickness in the range of about 5 nanometers to about 30 nanometers on the titanium nitride layer at a temperature less than about 400° C.; and
forming a photoresist layer on the oxide layer to define features in the conductive layer having a pitch of less than or equal to about 0.6 microns.

### Claim 20 (depends on 19)

The method according to claim 19, wherein the thickness is in the range of about 5 nanometers to about 20 nanometers.

### Claim 21 (depends on 19)

The method according to claim 19, wherein the step of forming an oxide layer includes depositing an oxide layer on the titanium nitride layer.

### Claim 22 (depends on 21)

The method according to claim 21, wherein the oxide layer is a silicon dioxide layer.

### Claim 23 (depends on 21)

The method according to claim 21, wherein the oxygen concentration in the oxide layer is at least about 60 percent.

### Claim 23 (depends on 19)

The method of claim 19, wherein the step of forming an oxide layer includes incorporating oxygen into a portion of the titanium nitride layer.

### Claim 24 (depends on 23)

The method according to claim 23, wherein the oxygen concentration in the oxide layer is at least about 20 percent.

### Claim 25 (depends on 19)

The method of claim 19, wherein the step of forming an oxide layer includes thermally oxidizing the titanium nitride layer at a pressure in the range of about 10 atmospheres to about 50 atmospheres.

### Claim 26 (depends on 19)

The method of claim 19, wherein the photoresist includes a non-chemically amplified photoresist.

### Claim 27

A method for forming a patterned conductive layer, the method comprising the steps of:
providing a conductive layer;
forming a titanium nitride layer on the conductive layer;
forming an oxide layer having a thickness in the range of about 5 nanometers to about 30 nanometers on the titanium nitride layer;
forming a photoresist layer on the oxide layer;
patterning the photoresist layer resulting in exposed portions of the oxide layer; and
removing the exposed portions of the oxide layer, and portions of the titanium nitride layer and portions of conductive layer underlying the exposed portions.

### Claim 28

A method for forming a patterned conductive layer, the method comprising the steps of:
providing a conductive layer;
forming a titanium nitride layer on the conductive layer, the titanium nitride layer having a thickness of less than about 600Å;
depositing an oxide layer on the titanium nitride layer, the oxide layer having a thickness in a range of about 5 nanometers to about 30 nanometers;
forming a photoresist layer on the oxide layer; and
defining at least one feature in the conductive layer, the at least one feature having a critical dimension less than or equal to about 0.6 microns.

### Claim 29 (depends on 28)

The method according to claim 28, wherein the defining step includes patterning the photoresist layer to expose portions of the underlying titanium nitride layer and conductive layer.

### Claim 30 (depends on 29)

The method according to claim 29, wherein the titanium nitride layer has a thickness of less than about 300Å.

### Claim 31

An intermediate structure formed during a semiconductor wafer fabrication process, the structure comprising:
a conductive layer on a substrate;
a titanium nitride layer on the conductive layer;
an oxide region having a thickness in the range of about 5 nanometers to about 30 nanometers on the titanium nitride layer; and
a photoresist layer on the oxide region.

### Claim 32 (depends on 31)

The intermediate structure according to claim 31, wherein the thickness of the oxide region is in a range of 5 nanometers to about 20 nanometers.

### Claim 33 (depends on 31)

The intermediate structure according to claim 31, wherein the oxide region includes one of titanium oxide, TixNyOz, and silicon dioxide.

### Claim 34 (depends on 31)

The intermediate structure according to claim 31, wherein the photoresist is a non-chemically amplified photoresist.

### Claim 35 (depends on 31)

The intermediate structure according to claim 31, wherein the conductive layer is a layer of aluminum.

### Claim 36

An intermediate structure formed during a semiconductor wafer fabrication process, the structure comprising:
a conductive layer on a substrate surface;
a titanium nitride layer on the conductive layer;
an oxide layer having a thickness in the range of about 5 nanometers to about 20 nanometers on the titanium nitride layer; and
a photoresist layer on the oxide layer, wherein at least portions of the oxide layer, titanium nitride layer, and conductive layer are removed to the substrate surface.

### Claim 37 (depends on 36)

The intermediate structure according to claim 36, wherein at least one feature is defined in the conductive layer, the at least one feature having a pitch of less than or equal to about 0.6 microns.

### Claim 38 (depends on 36)

The intermediate structure according to claim 36, wherein the oxide region comprises titanium oxide.

### Claim 39 (depends on 36)

The intermediate structure according to claim 36, wherein the oxide region comprises TixNyOz.

### Claim 40 (depends on 36)

The intermediate structure according to claim 36, wherein the oxide region comprises silicon dioxide.

### Claim 41 (depends on 36)

The intermediate structure according to claim 36, wherein the photoresist layer comprises non-chemically amplified photoresist.

### Claim 42 (depends on 36)

The intermediate structure according to claim 36, wherein the conductive layer comprises aluminum.

### Claim 43

An intermediate interconnect structure for med during a semiconductor wafer fabrication process, the structure comprising:
a conductive material on at least a portion of a substrate surface, wherein the conductive material comprises aluminum;
a patterned stack on at least a portion of the conductive material, the patterned stack comprising:
at least one titanium nitride region on the conductive material,
at least one oxide region having a thickness in the range of about 5 nanometers to about 20 nanometers on the at least one titanium nitride region, and
at least one photoresist region on the at least one oxide region, wherein conductive material has been removed to define features in the conductive material having a pitch of less than or equal to about 0.6 microns.

### Claim 44 (depends on 43)

The intermediate interconnect structure according to claim 43, wherein the at least one oxide region comprises titanium oxide.

### Claim 45 (depends on 43)

The intermediate interconnect structure according to claim 43, wherein the at least one oxide region comprises TixNyOz.

### Claim 46 (depends on 43)

The intermediate interconnect structure according to claim 43, wherein the at least one oxide region comprises silicon dioxide.

### Claim 47 (depends on 43)

The intermediate interconnect structure according to claim 43, wherein the at least one photoresist region comprises non-chemically amplified photoresist.

### Claim 48

An intermediate patterned aluminum containing interconnect structure, comprising a patterned stack, wherein the patterned stack comprises:
a conductive material on at least a portion of a substrate surface, wherein the conductive material comprises aluminum;
at least one titanium nitride region on at least a portion of the conductive material;
at least one oxide region having a thickness in the range of about 5 nanometers to about 20 nanometers on the at least one titanium nitride region; and
at least one photoresist region on the at least one oxide region, wherein features in the conductive material have a pitch of less than or equal to about 0.6 microns.

### Claim 49 (depends on 48)

The intermediate interconnect structure according to claim 48, wherein the oxide region comprises titanium oxide.

### Claim 50 (depends on 48)

The intermediate interconnect structure according to claim 48, wherein the oxide region comprises TixNyOz.

### Claim 51 (depends on 48)

The intermediate interconnect structure according to claim 48, wherein the oxide region comprises silicon dioxide.

### Claim 52 (depends on 48)

The intermediate interconnect structure according to claim 48, wherein the photoresist region comprises non-chemically amplified photoresist.