# US 2001/0018224 A1 · Semiconductor device and manufacturing method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0018224 A1
- Document ID: US20010018224A1
- Status: Published application
- Kind: A1
- Application number: 09/778,082
- Filed: 2001-01-07
- Published: 2001-08-30
- Earliest claimed: 1994-10-07
- Assignees: Semiconductor Energy Laboratory Co., Ltd.
- Inventors: Hongyong Zhang
- Web page: https://patentgrep.com/patent/US20010018224A1

## CPC

- H10P 14/3816: {Pulsed laser beam}
- G02F 1/13454: {Drivers integrated on the active matrix substrate (G02F1/136277 takes precedence)}
- H10D 86/0225: {using crystallisation-promoting species, e.g. using a Ni catalyst}
- H10D 86/40: characterised by multiple TFTs
- H10D 86/60: wherein the TFTs are in active matrices
- H10P 14/2922: {being non-crystalline insulating materials, e.g. glass or polymers}
- H10P 14/3238: {being insulating materials}
- H10P 14/3411: {Silicon, silicon germanium or germanium}
- H10P 14/3466: {Crystal orientation}
- H10P 14/3806: {using crystallisation-enhancing elements}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- G02F: OPTICAL DEVICES OR ARRANGEMENTS FOR THE CONTROL OF LIGHT BY MODIFICATION OF THE OPTICAL PROPERTIES OF THE MEDIA OF THE ELEMENTS INVOLVED THEREIN; NON-LINEAR OPTICS; FREQUENCY-CHANGING OF LIGHT; OPTICAL LOGIC ELEMENTS; OPTICAL ANALOGUE/DIGITAL CONVERTERS
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES

## Abstract

TFTs of peripheral logic circuits and TFTs of an active matrix circuit (pixel circuit) are formed on a single substrate by using a crystalline silicon film. The crystalline silicon film is obtained by introducing a catalyst element, such as nickel, for accelerating crystallization into an amorphous silicon film and heating it. In doing so, the catalyst element is introduced into regions for the peripheral logic circuits in a non-selective manner, and is selectively introduced into regions for the active matrix circuit. As a result, vertical crystal growth and lateral crystal growth are effected in the former regions and the latter regions, respectively. Particularly in the latter regions, the off-current and its variation can be reduced.

## Claims

### Claim 1

A method of manufacturing a semiconductor device, said method comprising the steps of:
forming a plurality of thin film transistors being provided on an insulating surface, each of said thin film transistors comprising a semiconductor film having a source region, a drain region and a pair of lightly doped impurity regions,
wherein the semiconductor film comprises (111), (220) and (311) planes,
wherein a ratio of a reflection intensity of the (111) plane to sum of reflection intensities of the (111), (220) and (311) planes amounts to larger than 90%,
wherein the reflection intensities of the (111), (220) and (311) planes are measured by an X-ray diffraction.

### Claim 2 (depends on 1)

A method according to claim 1,
wherein the semiconductor film has a thickness of 300 to 1500 angstrom and comprises silicon.

### Claim 3 (depends on 1)

A method according to claim 1,
wherein the semiconductor device further comprises an interlayer insulating film comprising a silicon nitride film.

### Claim 4 (depends on 1)

A method according to claim 1,
wherein the semiconductor film has a crystal growth direction parallel to the insulating surface.

### Claim 5

A method of manufacturing a semiconductor device, said method comprising the steps of:
forming a plurality of thin film transistors being provided on an insulating surface, each of said thin film transistors comprising a semiconductor film having at least a source region, a drain region and a pair of lightly doped impurity regions,
wherein the semiconductor film comprises (111), (220) and (311) planes,
wherein a first ratio of a reflection intensity of the (111) plane to sum of reflection intensities of the (111), (220) and (311) planes amounts to larger than 80% in one region of the semiconductor film while a second ratio does not amount to larger than 80% in another region of the semiconductor film,
wherein the reflection intensities of the (111), (220) and (311) planes are measured by an X-ray diffraction.

### Claim 6 (depends on 5)

A method according to claim 5,
wherein the semiconductor film has a thickness of 300 to 1500 angstrom and comprises silicon.

### Claim 7 (depends on 5)

A method according to claim 5,
wherein the semiconductor device further comprises an interlayer insulating film comprising a silicon nitride film.

### Claim 8 (depends on 5)

A method according to claim 5,
wherein the one region of the semiconductor film has a crystal growth direction parallel to the insulating surface.

### Claim 9

A method of manufacturing an active matrix device, said method comprising the steps of:
forming a plurality of thin film transistors arranged in a direction over a substrate for constituting at least a part of an active matrix region,
each of said thin film transistors comprising:
a semiconductor film comprising crystalline silicon having at least a source region, a drain region, a channel region and a pair of lightly doped impurity regions; and
a gate electrode adjacent to the channel region with an insulating film interposed between the gate electrode and the channel region,
wherein the semiconductor film comprises (111), (220) and (311) planes,
wherein a ratio of a reflection intensity of the (111) plane to sum of reflection intensities of the (111), (220) and (311) planes amounts to larger than 90%,
wherein the reflection intensities of the (111), (220) and (311) planes are measured by an X-ray diffraction.

### Claim 10 (depends on 9)

A method according to claim 9,
wherein the semiconductor film has a thickness of 300 to 1500 angstrom and comprises silicon.

### Claim 11 (depends on 9)

A method according to claim 9,
wherein the active matrix device further comprises an interlayer insulating film comprising a silicon nitride film.

### Claim 12 (depends on 9)

A method according to claim 9,
wherein the semiconductor film has a crystal growth direction parallel to a surface of the substrate.

### Claim 13

A method of manufacturing an active matrix device, said method comprising the steps of:
forming a plurality of thin film transistors arranged in a direction over a substrate for constituting at least a part of an active matrix region;
each of said thin film transistors comprising:
a semiconductor film comprising crystalline silicon having at least a source region, a drain region, a channel region and a pair of lightly doped impurity regions; and
a gate electrode adjacent to the channel region with an insulating film interposed between the gate electrode and the channel region;
forming a gate line extending in the direction over the substrate, said gate line being connected to the gate electrode;
wherein the semiconductor film comprises (111), (220) and (311) planes,
wherein a ratio of a reflection intensity of the (111) plane to sum of reflection intensities of the (111), (220) and (311) planes amounts to larger than 90%,
wherein the reflection intensities of the (111), (220) and (311) planes are measured by an X-ray diffraction.

### Claim 14 (depends on 13)

A method according to claim 13,
wherein the semiconductor film has a thickness of 300 to 1500 angstrom.

### Claim 15 (depends on 13)

A method according to claim 13,
wherein the active matrix device further comprises an interlayer insulating film comprising a silicon nitride film.

### Claim 16 (depends on 13)

A method according to claim 13,
wherein the semiconductor film has a crystal growth direction parallel to a surface of the substrate.

### Claim 17

A method of manufacturing an active matrix device, said method comprising the steps of:
forming a plurality of thin film transistors arranged in a direction over a substrate for constituting at least a part of an active matrix region;
each of said thin film transistors comprising:
a semiconductor film comprising crystalline silicon having at least a source region, a drain region, a channel region and a pair of lightly doped impurity regions; and
a gate electrode adjacent to the channel region with an insulating film interposed between the gate electrode and the channel region;
forming a source line extending in the direction over the substrate,
wherein one of the source region and the drain region is connected to the source line,
wherein the semiconductor film comprises (111), (220) and (311) planes,
wherein a ratio of a reflection intensity of the (111) plane to sum of reflection intensities of the (111), (220) and (311) planes amounts to larger than 90%,
wherein the reflection intensities of the (111), (220) and (311) planes are measured by an X-ray diffraction.

### Claim 18 (depends on 17)

A method according to claim 17,
wherein the semiconductor film has a thickness of 300 to 1500 angstrom.

### Claim 19 (depends on 17)

A method according to claim 17,
wherein the active matrix device further comprises an interlayer insulating film comprising a silicon nitride film.

### Claim 20 (depends on 17)

A method according to claim 17,
wherein the semiconductor film has a crystal growth direction parallel to a surface of the insulating surface.

### Claim 21

A method of manufacturing a semiconductor device, said method comprising:
forming a plurality of thin film transistors provided on an insulating surface, each of said thin film transistors comprising a semiconductor film having at least a source region, a drain region and a pair of lightly doped impurity regions,
wherein the semiconductor film comprises a (220) plane,
wherein a ratio of a reflection intensity of the (220) plane to sum of reflection intensities of (111), (220) and (311) planes amounts to larger than 90%,
wherein the reflection intensities of the (111), (220) and (311) planes are measured by an X-ray diffraction.

### Claim 22 (depends on 21)

A method according to claim 21,
wherein the semiconductor film has a thickness of 300 to 1500 angstrom and comprises silicon.

### Claim 23 (depends on 21)

A method according to claim 21,
wherein the semiconductor device further comprises an interlayer insulating film comprising a silicon nitride film.

### Claim 24 (depends on 21)

A method according to claim 21,
wherein the semiconductor film has a crystal growth direction parallel to the insulating surface.