# US 2001/0018036 A1 · Method of producing cubic boron nitride

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0018036 A1
- Document ID: US20010018036A1
- Status: Published application
- Kind: A1
- Application number: 09/777,657
- Filed: 2001-02-07
- Published: 2001-08-30
- Earliest claimed: 1997-11-25
- Assignees: Showa Denko K.K.
- Inventors: Kousuke Shioi; Eiji Ihara
- Web page: https://patentgrep.com/patent/US20010018036A1

## CPC

- C04B 35/5831: based on cubic boron nitrides {or Wurtzitic boron nitrides, including crystal structure transformation of powder}
- B01J 3/062: {characterised by the composition of the materials to be processed}
- B01J 2203/0645: Boronitrides
- B01J 2203/066: Boronitrides
- B01J 2203/068: Crystal growth
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS

## Abstract

hBN is converted to cBN by keeping it under temperature and pressure conditions within the range of stability of cubic boron nitride, in the presence of at least one compound selected from amides, imides and carbides of alkali metals and alkaline earth metals, as well as a silicon source and/or a boron source.

## Claims

### Claim 1

A method for producing cubic boron nitride which is characterized by keeping hexagonal boron nitride under temperature and pressure conditions within the range of stability of cubic boron nitride, (1) in the presence of (i) at least one compound selected from the group consisting of amides, imides and carbides of alkali metals and alkaline earth metals and (ii) a silicon source, or (2) in the presence of (i) at least one compound selected from the group consisting of amides and imides of alkali metals and alkaline earth metals, (ii) at least one compound selected from the group consisting of carbides of alkali metals and alkaline earth metals and (iii) a boron source; or (3) in the presence of (i) at least one compound selected from the group consisting of amides, imides and carbides of alkali metals and alkaline earth metals, (ii) a silicon source and (iii) a boron source, to convert the hexagonal boron nitride to cubic boron nitride.

### Claim 2 (depends on 1)

The method according to claim 1, wherein said conversion is conducted in the presence of (1) at least one compound selected from the group consisting of amides, imides and carbides of alkali metals and alkaline earth metals, and (ii) a silicon source.

### Claim 3 (depends on 1)

The method according to claim 1, wherein said conversion is conducted in the presence of (i) at least one compound selected from the group consisting of amides and imides of alkali metals and alkaline earth metals, (ii) at least one compound selected from the group consisting of carbides of alkali metals and alkaline earth metals and (iii) a boron source.

### Claim 4 (depends on 1)

The method according to claim 1, wherein said conversion is conducted in the presence of (i) at least one compound selected from the group consisting of amides, imides and carbides of alkali metals and alkaline earth metals, (ii) a silicon source and (iii) a boron source.

### Claim 5 (depends on 1)

The method according to claim 1, wherein said at least one compound selected from the group consisting of the amides, imides and carbides is used such that the total number of metal atoms making up said at least one compound is in a range of 0.1 - 30 parts to 100 parts by the number of molecules of the hexagonal boron nitride.

### Claim 6 (depends on 5)

The method according to claim 5, wherein said at least one compound selected from the group consisting of the amides, imides and carbides is used such that the total number of the metal atoms making up said at least one compound is in a range of 0.5 to 20 parts to 100 parts by the number of molecules of the hexagonal boron nitride.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the ratio of said at least one carbides to said at least one amides and/or imides is from 70:30 to 5:95, based on the total numbers of the metal atoms making up the compounds.

### Claim 8 (depends on 7)

The method according to claim 7, wherein the ratio of said at least one carbide to said at least one amides and/or imides is from 50:50 to 5:95, based on the total numbers of the metal atoms making up the compounds.

### Claim 9 (depends on 1)

The method according to claim 1, wherein said silicon source is used such that the total number of silicon atoms making up the silicon source is in a range of 0.01 to 0.8 part to 100 parts by the number of molecule of the hexagonal boron nitride.

### Claim 10 (depends on 9)

The method according to claim 9, wherein said silicon source is used such that the total number of silicon atoms making up the silicon source is in a range of 0.025 to 0.3 part to 100 parts by the number of molecule of the hexagonal boron nitride.

### Claim 11 (depends on 1)

The method according to claim 1, wherein said boron source is used such that the total number of silicon atoms making up the boron source is in a range of 0.05 to 15 parts to 100 parts by the number of molecule of the hexagonal boron nitride.

### Claim 12 (depends on 11)

The method according to claim 11, wherein said boron source is used such that the total number of boron atoms making up the boron source is in a range of 0.1 to 5 parts by the number of molecule of the hexagonal boron nitride.

### Claim 13 (depends on 1)

A method according to claim 1, wherein said region of stability of cubic boron nitride is selected to have a temperature of 1100° C. or higher and a pressure of 3.8 GPa or higher.

### Claim 14 (depends on 1)

A method according to claim 1, wherein a lump comprising the converted cubic boron nitride and the unconverted hexagonal boron nitride is obtained and the lump is crushed, after which sodium hydroxide and water are added thereto and heating is effected to selectively dissolve the hexagonal boron nitride, and then cooling, acid cleaning and filtration are conducted, so as to isolate the cubic boron nitride.

### Claim 15 (depends on 1)

A method according to claim 1, wherein said at least one compound of amides, imides and carbides is at least one of amides, imides and carbides of lithium, magnesium and calcium.

### Claim 16 (depends on 1)

A method according to claim 1, wherein a combination of LiNH2 and CaC2 is used, optionally with a silicon source and/or a boron source.