# US 2001/0017387 A1 · Method of fabricating buried source to shrink chip size in memory array

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0017387 A1
- Document ID: US20010017387A1
- Status: Published application
- Kind: A1
- Application number: 09/784,824
- Filed: 2001-02-20
- Published: 2001-08-30
- Earliest claimed: 1998-05-27
- Assignees: Taiwan Semiconductor Manufacturing Company, Ltd.
- Inventors: Chia-Ta Hsieh; Jenn Tsao; Di-Son Kuo; Yai-Fen Lin; Hung-cheng Sung
- Web page: https://patentgrep.com/patent/US20010017387A1

## CPC

- H10D 62/151: {of IGFETs (of IGFETs having LDD or DDD structure H10D30/601; of thin film transistors H10D30/6713)}
- H10B 20/00: Read-only memory [ROM] devices
- H10D 62/021: {Forming source or drain recesses by etching e.g. recessing by etching and then refilling}
- H10D 62/115: {Dielectric isolations, e.g. air gaps}
- H10W 20/0698: {Local interconnections}
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10B: ELECTRONIC MEMORY DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method is provided for forming buried source line in semiconductor devices. It is known in the art to form buried contacts on the surface of a semiconductor substrate. The present invention discloses a method of fabricating a semiconductor device, particularly a memory cell, having both the source region and the source line buried within the substrate. The source line is formed in a trench in the substrate over the source region. The trench walls are augmented with voltage anti-punch-through protection. The trench also provides the attendant advantages of extended sidewall area, smaller sheet resistance, and yet smaller cell area, therefore, smaller chip size, and faster access time as claimed in the embodiments of this invention. The buried source disclosed here is integrated with source line which is also buried within the substrate.

## Claims

### Claim 1

A method of forming buried source in a memory array comprising the steps of:
providing a silicon substrate having a plurality of active and field areas defined;
forming a pad oxide layer over said substrate;
depositing a layer of nitride over said pad oxide layer;
forming a patterned photoresist mask over said layer of nitride, wherein said patterns correspond to source regions formed in said active areas of said silicon substrate;
etching said underlying layer of nitride and said pad oxide through openings in said patterned photoresist mask;
etching further to form a trench with internal surfaces in said silicon substrate;
removing said photoresist mask;
growing surface oxide on said internal surfaces of said trench;
etching portions of said surface oxide on portions of said internal surfaces of said trench;
performing selective epitaxial growth (SEG) in said trench;
forming an integrated source line in said SEG in said trench over said active regions;
removing said layer of nitride and pad oxide layer; and
using conventional techniques for forming and completing a semiconductor device.

### Claim 2 (depends on 1)

The method of claim 1, wherein said forming a pad oxide layer is accomplished by thermal growth at a temperature between about 850 to 950° C.

### Claim 3 (depends on 2)

The method of claim 2, wherein said pad oxide layer has a thickness between about 250 to 400 angstroms (Å).

### Claim 4 (depends on 1)

The method of claim 1, wherein said depositing a layer of nitride is accomplished with LPCVD.

### Claim 5 (depends on 4)

The method of claim 4, wherein the thickness of said layer of nitride is between about 1500 to 2500 Å.

### Claim 6 (depends on 1)

The method of claim 1, wherein said photoresist mask has a thickness between about 1 to 1.2 micrometers (μm).

### Claim 7 (depends on 1)

The method of claim 1, wherein said etching said layer of nitride and pad oxide is accomplished with dry etch.

### Claim 8 (depends on 1)

The method of claim 1, wherein said etching further to form a trench in said silicon substrate is accomplished with dry etch.

### Claim 9 (depends on 1)

The method of claim 1, wherein said trench with internal surfaces has a depth between about 1500 to 4000 Å, and a width between about 2000 to 5000 Å.

### Claim 10 (depends on 1)

The method of claim 1, wherein said internal surfaces of said trench comprise sidewalls and a bottom surface.

### Claim 11 (depends on 1)

The method of claim 1, wherein said growing surface oxide on said internal surfaces of said trench is accomplished by thermal growth at a temperature between about 900 to 1000° C.

### Claim 12 (depends on 10)

The method of claim 10, wherein said surface oxide formed on said sidewalls in said trench form anti-punch-through walls with a thickness between about 80 to 200 Å.

### Claim 13 (depends on 10)

The method of claim 10, wherein said etching portions of said surface oxide is accomplished by etching said surface oxide on said bottom surface and upper portions of said sidewalls of said trench.

### Claim 14 (depends on 1)

The method of claim 1, wherein said etching portions of said surface oxide is accomplished with dry etch.

### Claim 15 (depends on 1)

The method of claim 1, wherein said performing selective epitaxial growth (SEG) in said trench is accomplished by chemical vapor deposition.

### Claim 16 (depends on 1)

The method of claim 1, wherein said forming an integrated source is accomplished by implanting As ions in the upper portions of said with a dosage between about 4×1015 to 8×1015 atoms/cm2 and at an energy between about 30 to 50 KEV.

### Claim 17 (depends on 17)

The method of claim 17, wherein said integrated source line is formed in said SEG to a depth between about 1500 to 4000 Å.

### Claim 18

An integrated buried source line in a memory array comprising:
a substrate having active and field regions defined;
a buried trench formed in active region of said substrate;
said buried trench having anti-punch-through sidewalls; and
said buried trench having a buried source line integrated with the source region of said substrate.

### Claim 19 (depends on 18)

The integrated source of claim 18, wherein said buried trench is formed with selective epitaxial growth (SEG) layer.

### Claim 20 (depends on 18)

The integrated source of claim 18, wherein said buried trench has a depth between about 1500 to 4000 Å

### Claim 21 (depends on 13)

The integrated source of claim 13, wherein said anti-punch-through sidewalls have a thickness between about 80 to 200 Å.