# US 2001/0017198 A1 · Process and device for improving the quality of continuously cast metallic bodies

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0017198 A1
- Document ID: US20010017198A1
- Status: Published application
- Kind: A1
- Application number: 09/771,001
- Filed: 2001-01-25
- Published: 2001-08-30
- Earliest claimed: 2000-01-26
- Inventors: Alfredo Poloni; Milorad Pavlicevic; Anatoly Kolesnichenko; Andrea Codutti
- Web page: https://patentgrep.com/patent/US20010017198A1

## CPC

- B22D 11/0401: {Moulds provided with a feed head}
- B22D 11/07: Lubricating the moulds
- B22D 11/115: by using magnetic fields
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

In a continuous-casting plant which uses a tank made of refractory material set on top of the crystallizer for removing the meniscus and the supernatant layer of covering powders from the solidification area, around the said tank there are electromagnetic means designed to generate variable magnetic fields for slowing down and making uniform the disordered flow of liquid metal inside the said tank, whilst at the joint between the tank and the crystallizer, other electromagnetic means are set which are designed to generate a direct magnetic field so as to remove locally the liquid metal from the walls of the tank and of the crystallizer.

## Claims

### Claim 1

Device for continuous casting of blooms, slabs, or billets, consisting of a cooled crystallizer in the form of an open hollow body and of a tank made of refractory material set on top of the crystallizer, into which liquid metal to be cast is poured, wherein the said tank made of refractory material is equipped with means designed to slow down and render uniform the disordered motion of the liquid metal, and in that means are present, set at the height of the boundary between the crystallizer and the tank, which are designed to cause and to maintain detachment of the molten metal from the walls of the tank-crystallizer ensemble.

### Claim 2 (depends on 1)

Device according to claim 1, wherein the said means for slowing down and rendering uniform the disordered motion of the liquid metal consist of a continuous core set around the tank and equipped with at least four poles and with windings set around each pole, and of means, adapted to interrupt and modify periodically the electrical supply of the said windings, thus creating electromagnetic fields which are periodically interrupted and modified in direction and intensity.

### Claim 3 (depends on 1)

Device according to claim 1, wherein the said means adapted to cause and maintain detachment of the molten metal from the walls of the tank-crystallizer ensemble are made up of an induction coil, supplied by a pulse current, consisting of a plurality of turns inserted in a magnetic core.

### Claim 4 (depends on 3)

Device according to claim 3, wherein the said induction coil is set between the tank and the crystallizer, and is provided with a wall facing towards the inside of the tank-crystallizer ensemble.

### Claim 5 (depends on 3)

Device according to claim 3, wherein the said induction coil is set outside the crystallizer, the contact surface between the tank and the crystallizer consisting of profiles of the end parts of the tank and of the crystallizer which are complementary and generically ogival or parabolic.

### Claim 6 (depends on 5)

Device according to claim 5, wherein the crystallizer has, in its part close to the tank, through slots.

### Claim 7 (depends on 6)

Device according to claim 6, wherein the said slots are at least partially closed by material transparent to electromagnetic fields, in which case one part of the said slots that has remained free serves for passage of a lubricant.

### Claim 8 (depends on 5)

Device according to claim 5, wherein the said induction coil is provided with a plurality of ducts for introducing, into the said compartment, lubricating material, fed in by means of manifolds.

### Claim 9 (depends on 7)

Device according to claim 7, wherein the said crystallizer is provided with ducts for the coolant, which are connected to similar ducts made in the induction coil, for cooling the latter.

### Claim 10 (depends on 4)

Device according to claim 4, wherein the crystallizer, at its initial part set facing towards the tank, has inserts which have high permeability and are provided with an electrically insulating coating on their surfaces that are in contact with the liquid metal.

### Claim 11 (depends on 1)

Device according to claim 1, wherein outside the crystallizer, mechanical exciters are set of an electrodynamic, pneumatic, magnetostrictive, or piezoelectric type, and the like, the frequency of which corresponds to the resonance frequency of the crystallizer-cast body system and is between 100 Hz and 25 000 Hz.

### Claim 12

Process for improving the quality of metallic bodies obtained from continuous casting, in which a tank made of refractory material is used, which is set on top of a crystallizer having the shape of an open hollow body, and into which, by means of a special discharging device, liquid metal is continuously poured which advances with a disordered motion towards the crystallizer and in the latter starts to solidify at a joining area (referred to as “triple point”) between the tank and the crystallizer, thus forming a so-called “skin” of the cast body extracted continuously from the crystallizer, the said tank having the purpose of removing, from the region of start of solidification, the free surface of the metal, the supernatant scale, and the area of molten metal with a flow that is perturbed as a result of the continuous addition of metal, wherein, in the said tank, a first action is carried out of slowing down and rendering uniform the disordered motion of liquid metal in the tank, which is combined with a second action of detachment of the liquid metal from the walls of the tank and of the crystallizer at the said joining point.

### Claim 13 (depends on 12)

Process according to claim 12, wherein the said first action of slowing down and rendering uniform the motion of the liquid metal is obtained by means of electromagnetic fields that are periodically interrupted and modified in direction and intensity.

### Claim 14 (depends on 13)

Process according to claim 13, wherein the said electromagnetic fields are generated by means of an induction system consisting of a first continuous core, set around the tank, provided with at least four poles and with windings set around each pole, the said poles being energized in a pre-set order for a given period of time Δt, and with a time interval, between two successive energizings, of 0.1-0.2 Δt.

### Claim 15 (depends on 14)

Process according to claim 14, wherein the said time period Δt is between 1 and 15 seconds.

### Claim 16 (depends on 15)

Process according to claim 15, wherein the said time period Δt is between 4 and 10 seconds.

### Claim 17 (depends on 14)

Process according to claim 14, wherein the current used for generating the said electromagnetic fields is between 1 kA and 200 kA.

### Claim 18 (depends on 12)

Process according to claim 12, wherein the second action of detachment of the liquid metal from the triple point is obtained by means of a pulsating magnetic field generated by a second induction coil consisting of a plurality of turns inserted into a second magnetic core which completely surrounds the crystallizer and is electrically insulated from the external environment.

### Claim 19 (depends on 18)

Process according to claim 18, wherein the said second induction coil is activated by means of a pulse current, having an intensity of between 5 kA and 200 kA, with a pulse duration of between 50 μs and 500 μs, and a frequency of between 2 Hz and 150 Hz.

### Claim 20 (depends on 19)

Process according to claim 19, wherein said current intensity is between 30 kA and 200 kA.

### Claim 21 (depends on 19)

Process according to claim 19, wherein the duration of said current pulses is between 100 μs and 200 μs.

### Claim 22 (depends on 19)

Process according to claim 19, wherein the frequency of the said pulse current is between 100 Hz and 200 Hz.

### Claim 23 (depends on 12)

Process according to claim 12, wherein, in an area corresponding to the said triple point, lubricant is injected in order to favour sliding of the forming skin against the walls of the crystallizer.

### Claim 24 (depends on 12)

Process according to claim 12, wherein, in addition to the detachment of the liquid metal, also detachment of the solidifying skin from the walls of the crystallizer is obtained, which is favoured by subjecting the crystallizer to vibrations both in the transverse and in the longitudinal directions with respect to the axis of the crystallizer, by means of mechanical exciters of an electrodynamic, pneumatic, magnetostrictive, or piezoelectric type, or the like, applied outside the crystallizer, with at least one per wall.

### Claim 25 (depends on 23)

Process according to claim 23, wherein the said lubricant has ferromagnetic properties.

### Claim 26 (depends on 25)

Process according to claim 25, wherein the said lubricant comprises a mixture of ferromagnetic particles having a size smaller than 100 μm, in a quantity of between 5 wt % and 25 wt % of the total lubricant.