- H10W 10/014: {using trench refilling with dielectric materials, e.g. shallow trench isolations}
- H10W 10/17: formed using trench refilling with dielectric materials, e.g. shallow trench isolations
- H10P 14/6308: {of Group IV semiconductors}
- H10P 14/6309: {of silicon in uncombined form, i.e. pure silicon}
- H10P 14/69215: {the material being a silicon oxide, e.g. SiO2}
- H10P 95/062: {involving a dielectric removal step}
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention proposes a method for fabricating shallow trench regions for isolation. A masking oxide layer is patterning on a semiconductor substrate, and the active areas are defined by recessing the semiconductor substrate to form trench regions. Silicon spacers are then formed on the sidewalls of the trench regions by LPCVD of amorphous silicon followed by an anisotropic etching. Sub-trench regions are thus constructed with the silicon spacers as its sidewalls. An ion implantation is performed to form channel stop regions. A thermal oxidation is carried out to grow a thermal oxide layer on the sidewalls and bottoms of the trench regions. A thick CVD oxide layer is deposited on the semiconductor substrate, and the oxide film outside the trench regions is removed by using a CMP process.

## Claims

### Claim 1

A method for forming trench isolation regions in a semiconductor substrate, said method comprises:
opening trench regions in said semiconductor substrate;
forming silicon spacers on the sidewall of said trench regions in said semiconductor substrate;
performing an oxidation to form a first oxide layer on the sidewalls and bottoms of said trench regions;
forming a second oxide layer on said first oxide layer, thereby filling said trench regions with said second oxide layer; and
removing portions of said first and second oxide layers which exceed said trench regions.

### Claim 2 (depends on 1)

The method according to claim 1, further comprising the following steps to form said trench regions:
forming a pad oxide layer on said semiconductor substrate;
patterning said pad oxide layer to expose a portion of said semiconductor substrate which defines said trench regions of said semiconductor substrate; and
etching said semiconductor substrate using said patterned pad oxide layer as an etching mask to form trench regions in said semiconductor substrate.

### Claim 3 (depends on 2)

The method according to claim 2, wherein said pad oxide layer has a thickness of about 300 to 2000 angstroms.

### Claim 4 (depends on 2)

The method according to claim 2, wherein said trench regions are recessed by an anisotropic etching using a plasma source selected from the group consisting of Cl2, BCl3, HBr, SF6 and SiCl4.

### Claim 5 (depends on 1)

The method according to claim 1, wherein said silicon spacers is formed of amorphous silicon.

### Claim 6 (depends on 1)

The method according to claim 1, wherein said silicon spacers is formed by the following steps:
forming a silicon layer on said semiconductor substrate;
etching back said silicon layer by a dry etching process.

### Claim 7 (depends on 6)

The method according to claim 6, wherein portions of said semiconductor substrate on said bottoms of said trench regions are over etched by said dry etching process.

### Claim 8 (depends on 1)

The method according to claim 1, further comprising an channel stopping implantation step to implant impurity ions into said semiconductor substrate after said silicon spacers are formed.

### Claim 9 (depends on 1)

The method according to claim 1, wherein said oxidation is performed in an oxygen containing ambient at a temperature of about 800 to 1100° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein said second oxide layer is formed of a material selected from the group consisting of tetra-ethyl-ortho-silicate-oxide (TEOS-oxide), boro-phospho silicate glass (BPSG), phospho silicate glass (PSG), boro silicate glass, (BSG), and undoped silicate glass (USG).

### Claim 11 (depends on 1)

The method according to claim 1, wherein said exceeded portions of said first and second oxide layers are removed by a chemical mechanical polishing (CMP) process.

### Claim 12

A method for forming trench isolation regions in a semiconductor substrate, said method comprises:
forming a pad oxide layer on said semiconductor substrate;
patterning said pad oxide layer to expose a portion of said semiconductor substrate which defines said trench regions of said semiconductor substrate;
etching said semiconductor substrate using said patterned pad oxide layer as an etching mask to form trench regions in said semiconductor substrate;
forming a silicon layer on said semiconductor substrate;
etching back said silicon layer by a dry etching process, thereby forming silicon spacers on the sidewall of said trench regions in said semiconductor substrate;
performing an oxidation to form a first oxide layer on the sidewalls and bottoms of said trench regions;
forming a second oxide layer on said first oxide layer, thereby filling said trench regions with said second oxide layer; and
removing said patterned pad oxide layer and portions of said first and second thermal oxide layers which exceed said trench regions.

### Claim 13 (depends on 12)

The method according to claim 12, wherein said pad oxide layer has a thickness of about 300 to 2000 angstroms.

### Claim 14 (depends on 12)

The method according to claim 12, wherein said trench regions are recessed by an anisotropic etching using the plasma source selected from the group consisting of Cl2, BCl3, HBr, SF6 and SiCl4.

### Claim 15 (depends on 12)

The method according to claim 12, wherein said silicon film is formed of amorphous silicon.

### Claim 16 (depends on 12)

The method according to claim 12, wherein portions of said semiconductor substrate on said bottoms of said trench regions are over etched by said dry etching process.

### Claim 17 (depends on 12)

The method according to claim 12, further comprising an channel stopping implantation step to implant impurity ions into said semiconductor substrate after said silicon spacers are formed.

### Claim 18 (depends on 12)

The method according to claim 12, wherein said oxidation is performed in an oxygen containing ambient at a temperature of about 800 to 1100° C.

### Claim 19 (depends on 12)

The method according to claim 12, wherein said third oxide layer is formed of a material selected from the group consisting of tetra-ethyl-ortho-silicate-oxide (TEOS-oxide), boro-phospho silicate glass (BPSG), phospho silicate glass (PSG), boro silicate glass, (BSG), and undoped silicate glass (USG).

### Claim 20 (depends on 12)

The method according to claim 12, wherein said patterned pad oxide layer and said exceeded portions of said first and second oxide layers are removed by a chemical mechanical polishing (CMP) process.