# US 2001/0011732 A1 · Semiconductor laser apparatus and method of producing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2001/0011732 A1
- Document ID: US20010011732A1
- Status: Published application
- Kind: A1
- Application number: 09/777,922
- Filed: 2001-02-07
- Published: 2001-08-09
- Earliest claimed: 2000-02-07
- Assignees: Sharp Kabushiki Kaisha
- Inventors: Ikuo Kohashi
- Web page: https://patentgrep.com/patent/US20010011732A1

## CPC

- H01S 5/0236: using an adhesive
- H01S 5/023: Mount members, e.g. sub-mount members
- H01S 5/0233: Mounting configuration of laser chips
- H01S 5/0235: Method for mounting laser chips
- H10W 72/073: {of die-attach connectors}
- H01S: DEVICES USING THE PROCESS OF LIGHT AMPLIFICATION BY STIMULATED EMISSION OF RADIATION [LASER] TO AMPLIFY OR GENERATE LIGHT; DEVICES USING STIMULATED EMISSION OF ELECTROMAGNETIC RADIATION IN WAVE RANGES OTHER THAN OPTICAL
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

In a method of producing a semiconductor laser apparatus, a conductive die-bonding paste is applied to a bonding surface in a predetermined position thereof and then preheated at a temperature equal to or higher than a temperature at which a diluent of the conductive die-bonding paste starts to transpire, but lower than a temperature at which the conductive die-bonding paste starts a thermosetting reaction. Then, with a semiconductor laser chip placed on the preheated conductive die-bonding paste, the latter is heated to be hardened. In the thus produced semiconductor laser apparatus, a highest position at which the conductive die-bonding paste adheres to end surfaces of the semiconductor laser chip is at a height of more than 0.01 mm from the bonding surface, but is below light-emitting points of the semiconductor laser chip.

## Claims

### Claim 1

A semiconductor laser apparatus having a semiconductor laser chip die-bonded to a bonding surface with a conductive die-bonding paste, said semiconductor laser chip having a light-emitting point at each of opposed end surfaces thereof,
wherein a highest position at which the conductive die-bonding paste adheres to the end surfaces of the semiconductor laser chip is at a height of more than 0.01 mm from the bonding surface, but is below the light-emitting point of the semiconductor laser chip.

### Claim 2 (depends on 1)

A semiconductor laser apparatus according to claim 1, wherein said conductive die-bonding paste contains an epoxy resin as a base material.

### Claim 3 (depends on 1)

A semiconductor laser apparatus according to claim 1, wherein said conductive die-bonding paste contains silver flakes as a conductive filler.

### Claim 4

A method of producing a semiconductor laser apparatus, comprising the steps of:
applying a conductive die-bonding paste to a bonding surface in a predetermined position thereof;
preheating the applied conductive die-bonding paste and then placing a semiconductor laser chip on the preheated conductive die-bonding paste; and
heating the preheated conductive die-bonding paste to a temperature higher than a temperature at which the conductive die-bonding paste starts a thermosetting reaction to thereby harden the conductive die-bonding paste.

### Claim 5 (depends on 4)

A method according to claim 4, wherein a temperature at which the conductive die-bonding paste is preheated is equal to or higher than a temperature at which a diluent of the conductive die-bonding paste starts to transpire, but lower than a temperature at which the conductive die-bonding paste starts a thermosetting reaction.

### Claim 6 (depends on 4)

A method according to claim 4, wherein said conductive die-bonding paste contains an epoxy resin as a base material and is preheated at a temperature of 60° C. or more but lower than 100° C.

### Claim 7 (depends on 6)

A method according to claim 6, wherein said conductive die-bonding paste is preheated at a temperature of 60° C. to 80° C. inclusive.

### Claim 8 (depends on 4)

A method according to claim 4, wherein the preheating is performed until the conductive die-bonding paste becomes as thin as about 0.02 mm.

### Claim 9 (depends on 4)

A method according to claim 4, wherein the preheating is performed for two seconds or more.