# US 12,770,961 B2 · Pouch film laminate body and battery case manufactured using same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,770,961 B2
- Document ID: US12770961B2
- Status: Granted
- Kind: B2
- Application number: 18/722,855
- Filed: 2022-12-22
- Published: 2024-12-19
- Granted: 2026-10-20
- Earliest claimed: 2021-12-24
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Soo Ji Hwang; Dae Woong Song; Sang Hun Kim; Hyung Kyun Yu; Min Hyeong Kang; Hun Hee Lim
- Web page: https://patentgrep.com/patent/US12770961B2

## CPC

- H01M 50/129: with two or more layers of only organic material
- H01M 50/105: Pouches or flexible bags
- H01M 50/119: Metals
- H01M 50/121: Organic material
- H01M 50/133: Thickness
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY

## Abstract

Disclose herein is a pouch film laminate body including a gas barrier layer, a base layer disposed on one surface of the gas barrier layer, and a sealant layer disposed on the other surface of the gas barrier layer. A loop stiffness of the pouch film laminate body in machine direction of the pouch film laminate body may be 750 mN to 1300 mN.

## Claims

### Claim 1

A battery case manufactured by drawing molding a pouch film laminate body, the pouch film laminate body comprising:
a gas barrier layer defining a thickness of 60 μm to 100 μm;
a base layer disposed on one surface of the gas barrier layer, the base layer including a laminate structure of a polyethylene terephthalate film and a nylon film; and
a sealant layer disposed on an opposite surface of the gas barrier layer, the sealant layer defining a thickness of 60 μm to 100 μm,
wherein a loop stiffness of the pouch film laminate body in a machine direction (MD) of the pouch film laminate body is 750 mN to 1300 mN, a ratio of a loop stiffness of the pouch film laminate body in a transverse direction of the pouch film laminate body to the loop stiffness in the machine direction is 0.9 to 1.1,
wherein the battery case includes at least one cup portion, wherein the cup portion has a depth of 10 mm or greater, and a curl height of 25 mm or less.

### Claim 2 (depends on 1)

The battery case of claim 1, wherein a loop stiffness of the pouch film laminate body in a transverse direction (TD) of the pouch film laminate body is 750 mN to 1300 mN.

### Claim 3 (depends on 1)

The battery case of claim 1, wherein the base layer has a breakage strength of 10 N/15 mm to 18 N/15 mm in the machine direction.

### Claim 4 (depends on 1)

The battery case of claim 1, wherein the polyethylene terephthalate film has a thickness of 5 μm to 20 μm, and the nylon film has a thickness of 10 μm to 30 μm.

### Claim 5 (depends on 1)

The battery case of claim 1, wherein the gas barrier layer comprises an aluminum alloy thin film.

### Claim 6 (depends on 5)

The battery case of claim 5, wherein the aluminum alloy thin film comprises 1.2 wt % to 1.7 wt % of iron.

### Claim 7 (depends on 5)

The battery case of claim 5, wherein the aluminum alloy thin film has a grain size of 10 μm to 13 μm.

### Claim 8 (depends on 1)

The battery case of claim 1, wherein the sealant layer comprises cast polypropylene, acid-treated polypropylene, a polypropylene-butylene-ethylene copolymer, or a combination thereof.