# US 12,760,391 B1 · Systems and methods for on/off leaching of a heap

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,760,391 B1
- Document ID: US12760391B1
- Status: Granted
- Kind: B1
- Application number: 19/333,143
- Filed: 2025-09-18
- Granted: 2026-10-13
- Earliest claimed: 2025-09-18
- Assignees: Freeport Minerals Corporation
- Applicants: Freeport Minerals Corporation
- Inventors: Cristian Alejandro Caro; Adam John Leonard; Vladimir Antonio Ancasi Huisa
- Web page: https://patentgrep.com/patent/US12760391B1

## CPC

- C22B 15/0065: {Leaching or slurrying (with organic compounds C22B3/16)}
- C22B 3/04: by leaching (C22B3/18 takes precedence)
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

Methods for recovering a metal value from a metal-bearing material are provided. The method comprises intermittent application of a heated leaching solution to a plurality of regions of the metal bearing material followed by a period of time where no additional heating leaching solution is applied. This method results in a cyclical heating pattern that improves recovery of the metal value with reduced energy and reagent expenditure.

## Claims

### Claim 1

A method for enhanced recovery of a metal value from a metal-bearing material, comprising:
defining a plurality of regions within the metal-bearing material;
applying a first amount of a heated leaching solution to a first region of the metal-bearing material comprising the metal value,
wherein the first amount of the heated leaching solution is heated using an external heat source to a temperature above an ambient temperature of the first region of the metal-bearing material,
wherein application of the first amount of the heated leaching solution elevates the temperature of the metal-bearing material in an area that comprises the first region to a temperature that is greater than the sum of the ambient temperature of the area that comprises the first region of the metal-bearing material and an anticipated amount of heat generated from a chemical reaction between the first amount of the heated leaching solution and the first region of the metal-bearing material;
waiting for a first period of time,
wherein, during the first period of time at least a portion of the metal value in the first region of the metal-bearing material is leached into the first amount of the heated leaching solution to create a first amount of a pregnant leaching solution,
wherein during the first period of time heated leaching solution is applied to at least one other region of the metal-bearing material,
wherein no additional heated leaching solution is applied to the first region of the metal-bearing material during the first period of time;
and wherein the total amount of metal value contained in collected portions of the pregnant leaching solution is greater than that collected from a first region of metal-bearing material comprising an equivalent metal value that is exposed to a leaching solution that is not heated to the temperature of the first amount of heated leaching solution, thereby enhancing recovery of the metal value.

### Claim 2 (depends on 1)

The method of claim 1, wherein a metal of the metal-bearing material is copper.

### Claim 3 (depends on 1)

The method of claim 1, further comprising measuring an amount of the metal value within the pregnant leaching solution.

### Claim 4 (depends on 3)

The method of claim 3, further comprising applying an additional amount of heated leaching solution to the first region of the metal-bearing material when a concentration of less than 1 gram per liter of the metal value within the pregnant leaching solution is measured.

### Claim 5 (depends on 1)

The method of claim 1, further comprising applying a second amount of a heated leaching solution to a second region of the metal-bearing material comprising the metal value,
wherein the second amount of the heated leaching solution is heated using an external heat source to a temperature above an ambient temperature of the second region of the metal-bearing material,
wherein application of the second amount of the heated leaching solution elevates the temperature of the metal-bearing material in an area that comprises the second region to a temperature that is greater than the sum of the ambient temperature of the area that comprises the second region of the metal-bearing material and an anticipated amount of heat generated from a chemical reaction between the second amount of the heated leaching solution and the second region of the metal-bearing material;
waiting for a second period of time,
wherein during the second period of time heated leaching solution is applied to at least one other region of the metal-bearing material,
wherein, during the second period of time at least a portion of the metal value in the second region of the metal-bearing material is leached into the second amount of the heated leaching solution to create a second amount of pregnant leaching solution,
wherein no additional heated leaching solution is applied to the second region of the metal-bearing material during the second period of time;
collecting at least a portion of the first amount of pregnant leaching solution and the second amount of pregnant leaching solution and optionally combining the first amount and the second amount collected; and
wherein the total amount of metal value contained in collected portions of the first and second pregnant leaching solutions is greater than that collected from a first and second region of metal-bearing material comprising an equivalent metal value that is exposed to a leaching solution that is not heated to the temperature of the first or the second amounts of heated leaching solution, thereby enhancing recovery of the metal value.

### Claim 6 (depends on 1)

The method of claim 1, wherein the first amount of heated leaching solution is applied to the first region of the metal-bearing material for a plurality of days.

### Claim 7 (depends on 1)

The method of claim 1, wherein the first period of time is 30 days.

### Claim 8 (depends on 1)

The method of claim 1, wherein the first amount of heated leaching solution is heated to a temperature between 40° C. and 50° C. via an external heating source.

### Claim 9 (depends on 1)

The method of claim 1, wherein the heated leaching solution comprises a leaching beneficial reagent.

### Claim 10 (depends on 5)

The method of claim 5, wherein the second amount of heated leaching solution is applied to the second region of the metal-bearing material for a plurality of days.

### Claim 11 (depends on 5)

The method of claim 5, wherein the second period of time is 30 days.

### Claim 12 (depends on 5)

The method of claim 5, wherein the second amount of heated leaching solution is heated to a temperature between 40° C. and 50° C. via an external heating source.

### Claim 13 (depends on 5)

The method of claim 5, wherein the first region of the metal-bearing material and the second region of the metal-bearing material are contained within a heap comprising the metal-bearing material.

### Claim 14 (depends on 5)

The method of claim 5, wherein the first region of the metal-bearing material and the second region of the metal-bearing material overlap within a heap comprising the metal-bearing material.

### Claim 15 (depends on 5)

The method of claim 5, wherein the first region of the metal-bearing material and the second region of the metal-bearing material are separated within a heap comprising the metal-bearing material.

### Claim 16 (depends on 5)

The method of claim 5, wherein the first region of the metal-bearing material and the second region of the metal-bearing material are adjacent within a heap comprising the metal-bearing material.

### Claim 17 (depends on 16)

The method of claim 16, wherein the first region of the metal-bearing material and the second region of the metal-bearing material are longitudinally arranged along a length or a width of the heap.

### Claim 18 (depends on 17)

The method of claim 17, wherein heated leaching solution is successively applied to the longitudinally arranged first region of the metal-bearing material and then to the second region of the metal-bearing material.

### Claim 19

A method for enhanced recovery of a metal value from a metal-bearing material, comprising:
defining a plurality of regions within the metal-bearing material;
applying a first amount of a heated leaching solution to a first region of the metal-bearing material comprising the metal value,
wherein the first amount of the heated leaching solution is heated using an external heat source to a temperature above an ambient temperature of the first region of the metal-bearing material,
wherein application of the first amount of the heated leaching solution elevates the temperature of the metal-bearing material in an area that comprises the first region to a temperature that is greater than the sum of the ambient temperature of the area that comprises the first region of the metal-bearing material and an anticipated amount of heat generated from a chemical reaction between the first amount of the heated leaching solution and the first region of the metal-bearing material;
waiting for a period of time between about 30 and about 60 days,
wherein, during the period of time at least a portion of the metal value in the first region of the metal-bearing material is leached into the first amount of the heated leaching solution to create a first amount of a pregnant leaching solution,
wherein during the period of time heated leaching solution is applied to at least one other region of the metal-bearing material,
wherein no additional heated leaching solution is applied to the first region of the metal-bearing material during the period of time; and
wherein the total amount of metal value contained in collected portions of the pregnant leaching solution is greater than that collected from a first region of metal-bearing material comprising an equivalent metal value that is exposed to a leaching solution that is not heated to the temperature of the first amount of heated leaching solution, thereby enhancing recovery of the metal value.

### Claim 20

A method for enhanced recovery of a metal value from a metal-bearing material, comprising:
defining a plurality of regions within the metal-bearing material;
applying a first amount of a heated leaching solution to a first region of the metal-bearing material comprising the metal value,
wherein the first amount of the heated leaching solution is heated using an external heat source to a temperature between about 40° C. and about 50° C.,
wherein the first amount of heated leaching solution is applied over a period time of about 30 to about 60 days at a rate of between about 5 liters per hour per square meter and about 10 liters per hour per square meter,
wherein application of the first amount of the heated leaching solution elevates the temperature of the metal-bearing material in an area that comprises the first region to a temperature that is greater than the sum of an ambient temperature of the area that comprises the first region of the metal-bearing material and an anticipated amount of heat generated from a chemical reaction between the first amount of the heated leaching solution and the first region of the metal-bearing material;
terminating application of the heated leaching solution to the first region of the metal-bearing material;
waiting for a period of time between about 30 and about 60 days,
wherein no additional heated leaching solution is applied to the first region of the metal-bearing material during the period of time;
wherein during the period of time heated leaching solution is applied to at least one other region of the metal-bearing material,
wherein, during the application and waiting periods, at least a portion of the metal value in the first region of the metal-bearing material is leached into the first amount of the heated leaching solution to create a pregnant leaching solution,
optionally repeating the application, termination, and waiting steps a plurality of times; and
collecting the pregnant leaching solution,
wherein the total amount of metal value contained in collected portions of the pregnant leaching solution is greater than that collected from a first region of metal-bearing material comprising an equivalent metal value that is exposed to a leaching solution that is not heated to the temperature of the first amount of heated leaching solution, thereby enhancing recovery of the metal value and/or wherein energy and reagent expenditure is less than energy and reagent expenditure realized when heated leaching solution is constantly applied to the metal-bearing material for an equivalent period of time.