Microwave-processed, ultra-rapid quenched lithium-rich lithium manganese nickel oxide and methods of making the same
AssigneeStratus Materials Inc.
InventorsJay F. Whitacre, Wei Wu, Sven Burke
Life of this patent
Estimating the term…
Abstract
A method includes sintering a lithium-rich metal oxide (LRMO) material at a sintering temperature to form a sintered LRMO material and quenching the sintered LRMO material from the sintering temperature to room temperature in less than 500 milliseconds to form a quenched LRMO material represented by a chemical formula Lix(MnyNi1-y)2-xO2, where x is greater than 1.05 and less than 1.25, and y ranges from 0.95 to 0.1.
Claims16
A method, comprising:
- sintering a lithium-rich metal oxide (LRMO) material at a sintering temperature to form a sintered LRMO material;
- and
- quenching the sintered LRMO material from the sintering temperature to room temperature in less than 500 milliseconds to form a quenched LRMO material represented by a chemical formula:
- wherein x is greater than 1.05 and less than 1.25, and y ranges from 0.95 to 0.1.
1 more element
A method, comprising:
- thermally decomposing a precursor material using microwave radiation to form a thermally decomposed lithium-rich metal oxide (LRMO) material;
- sintering the thermally decomposed LRMO material to form a sintered LRMO material;
- and
- quenching the sintered LRMO material to form a quenched LRMO material represented by a chemical formula:
- wherein x is greater than 1.05 and less than 1.25, and y ranges from 0.95 to 0.1.
2 more elements