Abstract
Provided is a gas barrier laminate including: a paper substrate; a layer including a polyvinyl alcohol-based resin; a vapor-deposited layer; and a layer including a polyolefin having a polar group, in order.
Claims19
A gas barrier laminate consisting of, in following order:
- a paper substrate;
- a first resin layer including a polyvinyl alcohol-based resin;
- a vapor-deposited layer including at least one material from among aluminum, aluminum oxide (AlOx), and silicon oxide (SiOx);
- and
- a second resin layer in direct contact with the vapor-deposited layer, the second resin layer including 90% or more by mass of a polyolefin having a polar group, the polyolefin including at least one functional group selected from a carboxyl group, a salt of a carboxyl group, a carboxylic acid anhydride group, and a carboxylic acid ester, wherein
- a thickness of the first resin layer is 1 μm to 5 μm, and
- the first resin layer is a directly applied coat on a surface of the paper substrate.
4 more elements
A gas barrier laminate consisting of, in following order:
- a paper substrate;
- a first resin layer including a polyvinyl alcohol-based resin;
- a vapor-deposited layer including at least one material from among aluminum, aluminum oxide (AlOx), and silicon oxide (SiOx);
- and
- a second resin layer in direct contact with the vapor-deposited layer, the second resin layer including a polyolefin having a polar group, wherein
- a thickness of the second resin layer is 2 μm to 10 μm,
- a thickness of the paper substrate is 30 μm to 100 μm,
- a thickness of the paper substrate is 80% or more of a thickness of an entirety of the gas barrier laminate,
- the polyolefin having the polar group is a copolymer of ethylene and an unsaturated carboxylic acid,
- a content of the polyolefin in the second resin layer is 90% by mass or more,
- a thickness of the first resin layer is 1 μm to 5 μm, and
- the first resin layer is a directly applied coat on a surface of the paper substrate.