Bicontinuous separating layers for solid-state batteries and methods of forming the same
AssigneeGM Global Technology Operations LLC
InventorsThomas A. Yersak, Ion C. Halalay, Yubin Zhang
Life of this patent
Estimating the term…
Loading patent…
AssigneeGM Global Technology Operations LLC
InventorsThomas A. Yersak, Ion C. Halalay, Yubin Zhang
Estimating the term…
A bicontinuous separating layer includes a separating matrix having pores and a solid-state electrolyte disposed in the pores of the separating matrix. In certain variations, the bicontinuous separating layer is prepared by contacting a solid-state electrolyte liquid-state precursor with the separating matrix and heating the infiltrated separating matrix to a temperature between about 25° C. and about 300° C. The solid-state electrolyte liquid-state precursor includes a solvent and a solid-state electrolyte powder or a solid-state electrolyte precursor. In other variations, the bicontinuous separating layer may be prepared by contacting a solid-state electrolyte powder with a separating matrix to form a physical mixture and heating the physical mixture to a temperature between about 240° C. and about 500° C., where the separating matrix is defined by a polymer having a melting temperature greater than about 215° C., and the solid-state electrolyte has a melting temperature greater than about 300° C.
A bicontinuous separating layer for an electrochemical cell, the bicontinuous separating layer comprising:
Dependencies are inferred from the claim text.