# US 12,735,596 B2 · Manufacturing method of conductive layer

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 12,735,596 B2
- Document ID: US12735596B2
- Status: Granted
- Kind: B2
- Application number: 18/824,925
- Filed: 2024-09-05
- Published: 2024-12-26
- Granted: 2026-09-15
- Earliest claimed: 2022-03-30
- Assignees: FUJIFILM Corporation
- Applicants: FUJIFILM Corporation
- Inventors: Yusuke Fujii; Norihide Shimohara; Masaharu Kawai
- Web page: https://patentgrep.com/patent/US12735596B2

## CPC

- C09D 11/52: Electrically conductive inks
- B41J 2/01: Ink jet
- B41M 5/00: Duplicating or marking methods; Sheet materials for use therein (by using light-sensitive materials G03; electrography, magnetography G03G {; repeatedly usable boards or tablets for writing or drawing B43L1/00})
- B41M 5/0047: {by ink-jet printing}
- B41M 7/0081: {using electromagnetic radiation or waves, e.g. ultraviolet radiation, electron beams}
- B41M 7/009: {using thermal means, e.g. infrared radiation, heat}
- C09D 7/80: Processes for incorporating ingredients
- C09D 11/037: characterised by the pigment
- C09D 11/30: Inkjet printing inks
- C09D 11/322: Pigment inks
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- B41J: TYPEWRITERS; SELECTIVE PRINTING MECHANISMS, i.e. MECHANISMS PRINTING OTHERWISE THAN FROM A FORME; CORRECTION OF TYPOGRAPHICAL ERRORS
- B41M: PRINTING, DUPLICATING, MARKING, OR COPYING PROCESSES; COLOUR PRINTING, (correction of typographical errors B41J; processes for applying transfer pictures or the like B44C1/16; fluid media for correction of typographical errors by coating C09D10/00; printing textiles D06P)

## Abstract

An object of the present invention is to provide a manufacturing method of a conductive layer, in which storage stability and jetting stability of an ink are excellent and a conductive layer having excellent conductivity can be formed. The manufacturing method of a conductive layer of the present invention includes a deaeration step of deaerating a conductive ink accommodated in an ink container and a conductive layer forming step of, with an ink jet recording method, applying the deaerated conductive ink onto a substrate by jetting the deaerated conductive ink from a nozzle to form a conductive layer, in which the conductive ink contains at least one material selected from the group consisting of a metal salt, a metal complex, and metal particles, and in a case where a dissolved oxygen amount in the conductive ink before the deaeration step is denoted as a dissolved oxygen amount A and a dissolved oxygen amount in the deaerated conductive ink after the deaeration step is denoted as a dissolved oxygen amount B, a value obtained by subtracting the dissolved oxygen amount B from the dissolved oxygen amount A is larger than 15 mg/L.

## Claims

### Claim 1

A manufacturing method of a conductive layer, comprising:
a deaeration step of deaerating a conductive ink accommodated in an ink container; and
a conductive layer forming step of, with an ink jet recording method, applying the deaerated conductive ink onto a substrate by jetting the deaerated conductive ink from a nozzle to form a conductive layer,
wherein the conductive ink contains at least one material selected from the group consisting of a metal salt, a metal complex, and metal particles, and
in a case where a dissolved oxygen amount in the conductive ink before the deaeration step is denoted as a dissolved oxygen amount A and a dissolved oxygen amount in the deaerated conductive ink after the deaeration step is denoted as a dissolved oxygen amount B, a value obtained by subtracting the dissolved oxygen amount B from the dissolved oxygen amount A is larger than 15 mg/L.

### Claim 2 (depends on 1)

The manufacturing method of a conductive layer according to claim 1,
wherein the dissolved oxygen amount B is 10 mg/L or less.

### Claim 3 (depends on 1)

The manufacturing method of a conductive layer according to claim 1,
wherein a metal constituting the metal salt, the metal complex, and the metal particles includes at least one of silver or copper.

### Claim 4 (depends on 1)

The manufacturing method of a conductive layer according to claim 1,
wherein the conductive ink contains at least one of the metal salt or the metal complex.

### Claim 5 (depends on 1)

The manufacturing method of a conductive layer according to claim 1,
wherein, in a case where a molar concentration of metals in the conductive ink is denoted as Mm and a molar concentration of dissolved oxygen in the deaerated conductive ink after the deaeration step is denoted as Mb, a value of Mm/Mb is 1,700 to 100,000,
provided that units of Mm and Mb are both mmol/L.

### Claim 6 (depends on 1)

The manufacturing method of a conductive layer according to claim 1,
wherein the conductive layer forming step includes a curing treatment of performing at least one of heating or light irradiation on the deaerated conductive ink applied onto the substrate to cure the deaerated ink applied onto the substrate, and
a time from a point in time at which the deaerated ink is landed on the substrate until the heating or the light irradiation is started is within 1 second.

### Claim 7 (depends on 1)

The manufacturing method of a conductive layer according to claim 1,
wherein a temperature of the conductive ink in a case of performing the deaeration step is 30° C. or higher.

### Claim 8 (depends on 2)

The manufacturing method of a conductive layer according to claim 2,
wherein a metal constituting the metal salt, the metal complex, and the metal particles includes at least one of silver or copper.

### Claim 9 (depends on 2)

The manufacturing method of a conductive layer according to claim 2,
wherein the conductive ink contains at least one of the metal salt or the metal complex.

### Claim 10 (depends on 2)

The manufacturing method of a conductive layer according to claim 2,
wherein, in a case where a molar concentration of metals in the conductive ink is denoted as Mm and a molar concentration of dissolved oxygen in the deaerated conductive ink after the deaeration step is denoted as Mb, a value of Mm/Mb is 1,700 to 100,000,
provided that units of Mm and Mb are both mmol/L.

### Claim 11 (depends on 2)

The manufacturing method of a conductive layer according to claim 2,
wherein the conductive layer forming step includes a curing treatment of performing at least one of heating or light irradiation on the deaerated conductive ink applied onto the substrate to cure the deaerated ink applied onto the substrate, and
a time from a point in time at which the deaerated ink is landed on the substrate until the heating or the light irradiation is started is within 1 second.

### Claim 12 (depends on 2)

The manufacturing method of a conductive layer according to claim 2,
wherein a temperature of the conductive ink in a case of performing the deaeration step is 30° C. or higher.

### Claim 13 (depends on 3)

The manufacturing method of a conductive layer according to claim 3,
wherein the conductive ink contains at least one of the metal salt or the metal complex.

### Claim 14 (depends on 3)

The manufacturing method of a conductive layer according to claim 3,
wherein, in a case where a molar concentration of metals in the conductive ink is denoted as Mm and a molar concentration of dissolved oxygen in the deaerated conductive ink after the deaeration step is denoted as Mb, a value of Mm/Mb is 1,700 to 100,000,
provided that units of Mm and Mb are both mmol/L.

### Claim 15 (depends on 3)

The manufacturing method of a conductive layer according to claim 3,
wherein the conductive layer forming step includes a curing treatment of performing at least one of heating or light irradiation on the deaerated conductive ink applied onto the substrate to cure the deaerated ink applied onto the substrate, and
a time from a point in time at which the deaerated ink is landed on the substrate until the heating or the light irradiation is started is within 1 second.

### Claim 16 (depends on 3)

The manufacturing method of a conductive layer according to claim 3,
wherein a temperature of the conductive ink in a case of performing the deaeration step is 30° C. or higher.

### Claim 17 (depends on 4)

The manufacturing method of a conductive layer according to claim 4,
wherein, in a case where a molar concentration of metals in the conductive ink is denoted as Mm and a molar concentration of dissolved oxygen in the deaerated conductive ink after the deaeration step is denoted as Mb, a value of Mm/Mb is 1,700 to 100,000,
provided that units of Mm and Mb are both mmol/L.

### Claim 18 (depends on 4)

The manufacturing method of a conductive layer according to claim 4,
wherein the conductive layer forming step includes a curing treatment of performing at least one of heating or light irradiation on the deaerated conductive ink applied onto the substrate to cure the deaerated ink applied onto the substrate, and
a time from a point in time at which the deaerated ink is landed on the substrate until the heating or the light irradiation is started is within 1 second.

### Claim 19 (depends on 4)

The manufacturing method of a conductive layer according to claim 4,
wherein a temperature of the conductive ink in a case of performing the deaeration step is 30° C. or higher.

### Claim 20 (depends on 5)

The manufacturing method of a conductive layer according to claim 5,
wherein the conductive layer forming step includes a curing treatment of performing at least one of heating or light irradiation on the deaerated conductive ink applied onto the substrate to cure the deaerated ink applied onto the substrate, and
a time from a point in time at which the deaerated ink is landed on the substrate until the heating or the light irradiation is started is within 1 second.